Skip to main content

ENCAPSULACION DE RESIDUOS RADIOACTIVOS EN CEMENTOS DE FOSFATO DE MAGNESIO

PID2020-116738RJ-I00

•
Funding agency name Agencia Estatal de Investigación
Funding agency acronym AEI
Program Programa Estatal de I+D+i Orientado a los Retos de la Sociedad
Call Proyectos de I+D+i (Generación de Conocimiento y Retos Investigación)
Call year 2020
State Plan 2017-2020 Plan Estatal de Investigación Científica y Técnica y de Innovación
Beneficiary centre AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 1
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Acid resistance of alkali-activated binders based on clays from phosphate mining by-products

  • Mabroum, Safaa
  • García-Lodeiro, Inés
  • El Machi, Aiman
  • Chhaiba, Salma
  • Taha, Yassine
  • Benzaazoua, Mostafa
  • Blanco-Varela, María Teresa
  • Hakkou, Rachid
This paper outlines the results of studying the resistance of alkali-activated materials (AAM), based on calcined yellow clay from phosphate mine by-products as a precursor, to an acid attack (with sulfuric and phosphoric acids, 5 %, pH ≈ 0,8–2). Calcined yellow clay (YC850) is used as the source of aluminosilicates, containing montmorillonite, dolomite, and quartz. The alkali-activation of such materials allows the determination of an adequate valorization way and evaluating their durability leads to defining the range of application. The residual compressive strengths were measured after 1, 2, and 4 weeks of immersion in those acids. The deterioration suffered by the paste specimens was examined using different techniques., The degree of deterioration differs from one acid to another; in sulfuric acid, the strengths decrease from 47 MPa to 10.6 MPa presenting 77.4 %. While in phosphoric acid, the decrease was about 36.2 % (30 MPa) after 28 days of attack. This detriment in the strengths is associated with changes not only in the microstructure but also with the alteration of the reaction products, mainly the binding gels C-A-S-H and (C,N)-A-S-H, which undergoes dealumination and decalcification. What is more, the chemical attack involves several reactions; calcium coming from the precursor reacts with the sulfates (in the H2SO4 attack) inducing the precipitation of gypsum, which is responsible for the significant strength loss. In addition, the dissolution of crystalline minerals, such as periclase and gehlenite (present in the precursor) generates higher porosity explaining the obtained results., The authors are acknowledged the concession of the project ICOOP +2020 (ref COOPA20454 funded by the CSIC) and to the Spanish Agency: AGENCIA ESTATAL DE INVESTIGACIÓN (JIN Projects 2021 PID2020-116738RJ-I00/AEI/10.13039/501100011033) and the RYC Excellence Contract (RYC2021-032620-I, MCIN/AEI/10.13039/50110001033). This work was supported by OCP-SA, Morocco, under the specific agreement OCP/UM6P #AS03., Peer reviewed