Supplementary information for Carbon nanotube film electrodes enabled by nanostructured biopolymers through aqueous processing [Dataset]
Under a Creative Commons Attribution-NonCommercial 3.0 Unported deed license., The optimization of the dispersions of P2-SWCNTs with CNCs (Figure S1) provides key
insights into the influence of the CNC concentration and allomorph type on the SWCNTs’
stabilization in water. The concentration of P2-SWCNTs after centrifugation is the most
immediate parameter of interest, while ζ-potential and hydrodynamic size are crucial
indicators of dispersion quality and stability over time. For type I CNCs, a significant
increase in the stabilized P2-SWCNT concentration occurs between 2 and 2.5 g/L (Figure
S1A), after which a plateau suggests a dispersion limit for this type of nanocrystals.
Regarding the hydrodynamic size (Figure S1B), there is a clear decrease from 2 to 3.5
g/L CNCs, where the size reaches a steady value. The ζ-potential (Figure S1B) remains
close to -30 mV across all dispersions, sufficient for stable dispersions, with a maximum
around -34 mV, observed at 4 g/L CNCs. In contrast, type II CNCs demonstrate a more
efficient stabilization of P2-SWCNTs, with a sharp increase in SWCNT concentration
from 1.5 to 2 g/L of nanocrystals, achieving 0.83 g/L of P2-SWCNTs (Figure S1C).
However, a decline is observed at concentrations beyond 3.5 g/L, particularly at 5 g/L,
suggesting that an excess of CNCs may lead to aggregation. The ζ-potential values across
all dispersions remained between -30 mV and -40 mV (Figure S1D), indicating strong
electrostatic stabilization, and the smaller hydrodynamic sizes reflect better dispersion
homogeneity compared to type I CNCs. Overall, these findings emphasize the need for a
precise tuning of the CNC concentration and allomorph selection to achieve optimal
dispersion efficiency of SWCNTs in water.-- 1. Optimization of the P2-SWCNT/CNC dispersions.............................................S3
2. Optimization of the p-MWCNT/CNC dispersions..............................................S4
3. Colloidal stability of CNT/NB dispersions after long-term storage....................S6
4. Raman spectroscopy of the CNT/NB dispersions ...............................................S6
5. UV-vis-NIR spectroscopy of the SWCNT/NB dispersions ................................S9
6. Characterization of CNTs and NBs materials ...................................................S10
7. TGA results of the lyophilized CNT/NB dispersions after thermal treatment..S10
8. Photographs of the CNT/NB films before and after thermal treatment ............S11
9. Contact angle of the CNT/NB films before and after thermal treatment ..........S12
10. Mechanical characterization of the CNT/NB
films……………………………S13
11. Calculation of the CNT/NB films electrical conductivity.................................S14
12. Cyclic voltammetry measurements ...................................................................S14
13. Electrochemically active surface area estimation .............................................S16
14. Electrochemical impedance spectroscopy measurements……………..……...S18
15. References .........................................................................................................S19, Financial support from the Spanish MCIN/AEI/10.13039/501100011033 and “ERDF A way of making Europe” by the European Union under project grants PID2022-139671OB-I00 and PID2023-147116OB-I00, as well as from the Gobierno de Aragón (DGA), in the R&D&I projects in priority lines and of a multidisciplinary nature (project grant PROY_T41_24), and through the grants to research groups (Grupo Reconocido DGA-T03_23R) is acknowledged. C. M.-B., V. C. and M. Á. Á.-S. thank the DGA for funding their PhD contracts (refs. CUS/621/2023, CUS/581/2020 and IIU/796/2019, respectively)., Peer reviewed