RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación
Artículo científico (JournalArticle)
Effect of Cross-Linking on the Molecular Motions and Nanodomains Segregation in Polymethacrylates Containing Aliphatic Alcohol Ether Residues
The dielectric relaxation spectra of poly(2-ethoxyethyl methacrylate) in the frequency domain exhibits above Tg and at high frequencies a well-developed secondary  relaxation. This process is followed in decreasing order of frequency for a relatively weak  relaxation and an ostensible glass-rubber relaxation which at high temperatures and low frequencies is dominated by electrode-polymer interfacial processes. By slightly crosslinking the polymer using 1% (mol) of 2-ethoxyethyldimethacrylate as crosslinking agent, the  relaxation disappears, leaving the  relaxation. The activation energy of the  relaxation for the crosslinked and uncrosslinked polymers is ca. 30 kJmol-1, about 10 kJmol-1 below that of the  relaxation. Crosslinking shifts the location of the glass-rubber relaxation nearly 10º C to higher temperatures, without widening the distribution of relaxation times. The X-rays pattern of the crosslinked polymer presents two peaks at q =5.6 nm-1 and 12.76 nm-1 resembling the X-ray patterns of poly(n-alkyl methacrylate)s. The peaks in poly(n-alkyl methacrylate)s were attributed to the formation of nanodomains integrated by side chains flanked by the backbone. However, whereas this heterogeneity produces an PE peak in poly(n-alkyl methacrylate)s with n  2, this microheterogeneity gives rise to a Maxwell-Wagner-Sillars (MWS) relaxation in the crosslinked polymer located at lower frequencies than the glass rubber relaxation. Finally the interfacial-electrode conductive processes of the crosslinked and uncrosslinked polymeric systems are studied in the light of current theories., We thank Dr. J. Guzman for providing us the CEOEMA sample. This work was financially supported by the DGCYT and CAM through the Grant MAT2008-06725-C03.