DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Plasma electrolytic oxidation of AZ31 magnesium stents for degradation rate control

  • Muñoz, Marta
  • Fernández, Juan Pablo
  • Torres, Belén
  • Pulido, Nuria
  • Zhang, Guangqi
  • Shanov, Vesselin
  • Moreno, Lara
  • Matykina, Endzhe
  • Rams, Joaquín
Cardiovascular disease caused by the accumulation of atheroma plaques in the coronary arteries and the subsequent decrease in the blood flow through the affected vessel, known as atherosclerosis, is responsible for a high percentage of deaths worldwide. Angioplasty is practiced to treat atherosclerosis which involves inserting a stent inside the occluded vessel to expand it and restore normal blood flow. In this work, temporary biodegradable stents made of AZ31 magnesium alloy have been fabricated using photo-chemical etching. The stents were coated via plasma electrolytic oxidation (PEO) technique. The radial strength of the stents was evaluated by cyclic compression, and the corrosion protection provided by the PEO coatings was studied by electrochemical and in vitro corrosion tests respectively. The stents showed an optimal maximum radial force of 0.147 N/mm and revealed elastic recuperation lower than 7 % of the total deformation after expansion. The applied PEO coating helped to control the corrosion of the magnesium alloy, delaying its initiation and, once it has started, decreased the degradation rate compared with the bare AZ31 samples. Thus, the stents treated with the PEO coatings developed in this research present promising results for their use as temporary medical devices used in angioplasty., The authors gratefully acknowledge the support of PID2021- 124341OB-C21 and PID2021-124341OB-C22 (MICINN/AEI/FEDER, UE) and ADITIMAT-CM (S2018/NMT-4411, Regional Government of Madrid and EU Structural Funds). The UC team would like to acknowledge the support by NSF through grant EEC-0812348., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Study of the effect of magnetic fields on static degradation of Fe and Fe-12Mn-1.2C in balanced salts modified Hanks’ solution

  • Limón, Irene
  • Multigner, Marta
  • Paternoster, Carlo
  • Lieblich, Marcela
  • Torres, Belén
  • Mantovani, Diego
  • Rams, Joaquín
Iron and its alloys are attractive as biodegradable materials because of their low toxicity and suitable mechanical properties; however, they generally have a slow degradation rate. Given that corrosion is an electrochemical phenomenon where an exchange of electrons takes place, the application of magnetic fields from outside the body may accelerate the degradation of a ferrous temporary implant. In the present study, we have investigated the effect of alternating and direct low magnetic field (H = 6.5 kA/m) on the corrosion process of pure iron (Fe) and an iron-manganese alloy (FeMnC) in modified Hanks' solution. A 14-day static immersion test was performed on the materials. The corrosion rate was assessed by mass and cross-sectional loss measurements, scanning electron microscopy, X-ray diffractometry, Fourier-transform infrared spectroscopy and X-ray photoelectron spectroscopy before and after degradation. The results show that the presence of magnetic fields significantly accelerates the degradation rate of both materials, with the corrosion rate being twice as high in the case of Fe and almost three times as high for FeMnC. In addition, a homogenous degradation layer is formed over the entire surface and the chemical composition of the degradation products is the same regardless of the presence of a magnetic field., Financial support of Ministry of Science and Innovation of Spain (MICINN) PID2021-123891OB-I00. PID2021-124341OB-C21 and PID2022-139323NB-I00 funded by MCIN/AEI/10.13039/ 501100011033. Rey Juan Carlos University, Móstoles (Madrid) Spain has funded the C1PREDOC2020 grant of Irene Limon. This work was partially supported by the Natural Science and Engineering Research Council of Canada, the Fonds de la Recherche du Québec sur les Natures et les Technologies, and the Canada Foundation for Innovation, Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Hardness and biocorrosion behaviour of a biodegradable Mg-3.0Zn-0.4Ca alloy after different processing routes

  • Hernández, M.
  • Fajardo, Santiago
  • Torres, B.
  • Rams, J.
  • Hidalgo-Manrique, P.
Biodegradable Mg alloys emerge as promising alternatives for biomedical applications, which requires a suitable combination of properties. In this work, a cast biocompatible Mg-3 wt% Zn-0.4 wt% Ca alloy, showing dendrites with large (α-Mg + CaMgZn) particles at the boundaries, was homogenised at 400 °C for 24 h. Afterwards, the alloy was subjected to either rolling or heat treatment or rolling followed by heat treatment. Microstructural characterisation revealed that (1) homogenisation causes the partial dissolution of particles, (2) rolling leads to deformed dendrites with basal orientation and (3) heat treatment results in a fully recrystallised microstructure with a grain size dependent on whether the alloy was previously rolled or not and promotes both the redistribution of the particles at the grain boundaries into a more connected configuration and the formation of a fine distribution of CaMgZn-rich particles within the grains. Hardness and corrosion tests in Hanks’ solution revealed that compared with the as-cast alloy homogenisation leads to higher corrosion resistance but slightly lower hardness, rolling to much higher hardness but the same corrosion rate and heat treatment to higher hardness and lower corrosion rate. The mechanical and biocorrosion behaviour was mainly ascribed to particle distribution and dislocation density, grain size and texture showing a negligible effect., The authors are grateful to the Spanish State Research Agency (AEI) ADIMAG project (PID2021-124341OB-C21) for funding. The research leading to these results has also received funding from the Community of Madrid and Rey Juan Carlos University under the Young Researchers R&D DISEMAG project (M2741), which is also gratefully acknowledged. The authors also thank Manuel Avella (IMDEA Materials Institute) and Ignacio Carabias (UDRX UCM) for assistance with EBSD and macrotexture measurements, respectively. Finally, one of the authors (M.´A. Hern´andez) also thanks the Spanish Ministry of Universities and Rey Juan Carlos University for a Margarita Salas postdoctoral contract.