Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 2
Encontrada(s) 1 página(s)

Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publicación Artículo científico (JournalArticle)

Influence of hydrogen on the hydraulic fracture behavior of a 42CrMo4 steel welds: Effect of the prior austenite grain size

  • Peral, Luis Borja
  • Díaz Portugal, Andrés
  • Arniella, V.
  • Belzunce, J.
  • Alegre Calderón, Jesús Manuel
  • Cuesta Segura, Isidoro Iván
The influence of hydrogen on the mechanical behavior of a quenched and tempered 42CrMo4 steel has been evaluated by means of high internal pressure fracture tests carried out on hydrogen precharged notched cylindrical specimens. The notched cylindrical specimens were precharged in a 1 M H2SO4 + 0.25 g/l As2O3 solution for 3 h with 1.2 mA/cm2. Hydraulic fracture tests were performed at different loading rates. Hydrogen embrittlement resistance increased with grain size refinement although the fine grained specimen had a higher hydrogen content than the coarse grained one. Fractographic analysis showed hydrogen enhanced decohesion fracture was less pronounced with decreasing grain size. Hydrogen embrittlement susceptibility is discussed in terms of the prior austenite grain size (PAGS) and the operative fracture mechanisms., The authors would like to thank the Spanish Government for the financial support received to perform the research projects TED2021-130413B-I00 and PID2021-124768OB-C21. This work was supported by the Regional Government of Castilla y León (Junta de Castilla y León) and by the Ministry of Science and Innovation MICIN and the European Union Next Generation EU/PRTR (MR5W.P3) and PRTR (MR4W.P2). L.B. Peral is grateful for his Margarita Salas Postdoctoral contract (Ref.: MU-21-UP2021-030) funded by the University of Oviedo through the Next Generation European Union.
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publicación Contribución de congreso (ConferenceOutput)

Hydrogen Embrittlement of AISI 316L steel produced by Selective Laser Melting

  • Peral, Luis Borja
  • Díaz Portugal, Andrés
  • Ebrahimzadeh, P.
  • Fernández-Pariente, I.
  • Alegre Calderón, Jesús Manuel
  • Cuesta Segura, Isidoro Iván
Trabajo presentado en: Third European Conference on the Structural Integrity of Additively Manufactures Materials (ESIAM23), Selective laser melting (SLM) is one of the common methods of additive manufacturing and it can be employed to customize components with complex geometry expected to work in hydrogen atmospheres. However, more studies are still needed to characterize the behavior of printed mechanical components intended to work in contact with hydrogen. In this study, smooth and notched tensile samples were precharged in an acid solution with 8 mA/cm2 for 24h time. Hydrogen damage was more marked in the notched samples, especially at 0.005 mm/min, where fracture micromechanism changed from ductile in the absence of hydrogen to quasi-brittle in the presence of internal hydrogen. The role of the strain-induced martensite is also highlighted., The authors would like to thank the Spanish Government for the financial support received to perform the research projects PID2021-124768OB-C21 and TED2021-130413B-I00. This work was also supported by the Regional Government of Castilla y León (Junta de Castilla y León) and by the Ministry of Science and Innovation MICIN and the European Union Next Generation EU/PRTR (MR4W.P2 and MR5W.P3).