DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación
Set de datos (Dataset)
Appendix A. Supplementary material for Understanding the structural changes on Fe2O3/Al2O3 oxygen carriers under chemical looping gasification conditions [Dataset]
Under a Creative Commons license CC-BY-NC-ND 4.0, 1- Pictures of the platinum basket with fresh and used oxygen carrier particles at different solid conversion ΔXs, temperature, Fe2O3-content, and number of redox cycles. Figure S1. View of the samples after 300 redox cycles in TGA at different operating conditions. Figure S2. View of the samples as a function of the number of redox cycles. 2. SEM pictures and EDX analyses of Fe presence on different points of Fe20Al particles reacted at three solid conversions ΔXs. Figure S3. Fe content determined by EDX on Fe20Al particles after 300 redox cycles for different ΔXs. T=950 ºC, This work was supported by the CO2SPLIT Project, Grant PID2020-113131RB-I00, funded by MICIN/AEI/10.13039/501100011033. I. Samprón thanks the Spanish Ministerio de Ciencia, Innovación y Universidades (MICIU) for the PRE2018-086217 predoctoral fellowship., Peer reviewed