Supplementary Information for Valorization of carbonaceous co-product obtained from iron ore-catalyzed methane cracking as support for Pd catalysts in toluene hydrogenation reaction [Dataset]

  • López de los Ríos, Jaime
  • Torres Gamarra, Daniel
  • Di Stasi, Christian
  • Ayala Cortés, Alejandro
  • Suelves Laiglesia, Isabel
  • Pinilla Ibarz, José Luis
11 figures, 7 tables.-- Under a Creative Commons BY-NC-ND 4.0 license, https://creativecommons.org/licenses/by-nc-nd/4.0/, Appendix A. Materials analysis: The XRD analysis of the iron from the ore used as a precursor to generated carbon nanomaterial shows that this iron is conformed only by hematite as shown in Figure S.1. XRD analysis also showed the presence of other metallic oxides such as MgO, SiO2 and CaO. A posterior analysis to the iron ore with N2 physisorption showed that the isotherm of the ore shown in Figure S2 corresponds to a solid with no porosity. XPS results of the catalyst’s surface analyses generated through the synthesis ways are shown in Figure S3. Analysis of the catalysts with N2 physisorption shown in Figure S4 revealed that the catalysts could be fitted to type IV isotherms, characteristic of mesoporous solids and the BJH pore size distribution. Oxidized catalysts have achieved high Pd dispersions with Pd nanoparticle sizes of a few nanometers as can be seen in the STEM images of high resolution in Figure S5. Table S1 shows the conversion and the hydrogenation capacity of the hybrid materials used as supports without Pd. As it can be seen supports did not possess activity in these reaction conditions., This research was funded by MCIN/AEI/10.13039/501100011033 and EU “NextGenerationEU”/PRTR” through project TED2021- 131416B-I00. The authors also acknowledge Gobierno de Aragón (DGA) for the financial support to Grupo de Conversión de Combustibles (T06_20R). J L-d.l.R. acknowledges Diputación General de Aragón (DGA) for the predoctoral fellowship. DT is grateful for the Juan de la Cierva Incorporación (JdC-I) fellowship (Grant Number: IJC2020-045553-I) funded by MCIN/AEI/ 10.13039/501100011033 and by “European Union NextGenerationEU/PRTR. C.D.S is grateful for the Juan de la Cierva (JdC) fellowship (Grant Number: JDC2022-048765-I) funded by MICIU/AEI /10.13039/501100011033 and by FSE+., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

Supplementary information for High-energy milling of iron ore into an efficient catalyst for cracking of methane and biogas [Dataset]

  • López de los Ríos, Jaime
  • Torres Gamarra, Daniel
  • Di Stasi, Christian
  • Ayala Cortés, Alejandro
  • Suelves Laiglesia, Isabel
  • Pinilla Ibarz, José Luis
Under a Creative Commons BY-NC-ND 4.0 license., Fig. A.1 Diffractograms of iron ores obtained after reduction in thermobalance in H2 at 900 ºC. Fig. A.2. Evolution of the acummulated carbon thourghout the CCM, a) WHSV = 2 NL gcat -1 h-1 and 900 ºC, b) WHSV = 2 NL gcat -1 h-1.Fig. A.3 N2 adsorption isotherm of the hybrid materials produced at the CCM at 900 ºC and a) 2 NL h-1 gcat -1, b) 4 NL h-1 gcat -1. Fig. A.4 SEM images with direct electrons (top) and backscattered electrons (bottom) of the hybrid materials produced at the CCM at 900 ºC and 2 NL h-1 gcat -1. Fig. A.5 TEM images of the hybrid materials produced at the CCM at 900 ºC and 2 NL h-1 gcat -1. Fig. A.6 TEM images of the hybrid materials produced at the CCM at 900 ºC and 4 NL h-1 gcat -1. Fig. A.7 TEM images of the hybrid materials produced at the CCM at 800, 850 and 900 ºC and 2 NL h-1 gcat -1. Fig. A.8. Evolution of the concentrations of the outlet gases in the CCB at 900 ºC and 2 NL h-1 gcat -1 with a) WT-ore, b) SM-ore, c) MM-ore and d) LM-ore. Fig. A.9. TEM images of the solid product at the CCB at 900 ºC and 2 NL h-1 gcat., This research was funded by MCIN/AEI/10.13039/501100011033 and EU “NextGenerationEU”/PRTR” through project TED2021-131416B-I00 and by MCIN/AEI/10.13039/501100011033 and FEDER, UE through project PID2023-147514OB-I00. The authors also acknowledge Gobierno de Aragón (DGA) for the financial support to Grupo de Conversión de Combustibles (T06_20R). Jaime López-De Los Ríos acknowledges Diputación General de Aragón (DGA) for the predoctoral fellowship (CPT_01_23). C.D.S is grateful for the Juan de la Cierva (JdC) fellowship (Grant Number: JDC2022-048765-I) funded by MICIU/AEI/10.13039/501100011033 and by FSE+. DT is grateful for the Juan de la Cierva Incorporación (JdC-I) fellowship (Grant Number: IJC2020–045553-I) funded by MCIN/AEI/10.13039/501100011033 and by “European Union NextGenerationEU/PRTR., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

Supplementary material for Tuning hydroconversion performance of n-hexadecane over Ni/silica-alumina catalysts: Role of Si/Al ratio and nickel loading [Dataset]

  • Andrades García, María
  • Di Stasi, Christian
  • Ayala Cortés, Alejandro
  • Torres Gamarra, Daniel
  • Suelves Laiglesia, Isabel
  • Pinilla Ibarz, José Luis
Under a Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International license., Table S1. Composition and textural properties of Siral series (hydrated silica-alumina) prior and after calcination at 550 °C. Information obtained from the official Sasol website. Figure S1. TPR pattern of calcined Ni10/Siral40. Figure S2. N2 adsorption-desorption isotherms for NiX/SiralY catalysts. Figure S3. SEM images (top panel) and EDX elemental mappings (bottom panel) for Siral40, Ni10/Siral40 and Ni25/Siral40. Figure S4. Particle size distributions for NiX/SiralY catalysts calculated from TEM images. Figure S5 Liquid (a) and gaseous in H2-free basis (b) products distribution obtained with Ni10/Siral40 at 300 °C and 30, 60, 90 bar of H2. Figure S6. Liquid (a) and gaseous in H2-free basis (b) products distribution obtained with Ni10/Siral40 at 60 bar of H2 and 300, 350 and 400 °C. Figure S7. Liquid (a) and gaseous in H2-free basis (b) products distribution obtained with different supports and with a Ni loading of 10 wt.% at 350 °C and 60 bar of H2. Figure S8. Liquid (a) and gaseous in H2-free basis (b) products distribution obtained with Siral40 as support and different Ni loadings at 350 °C and 60 bar of H2., Research Agency MCIN/AEI/10.13039/501100011033 and EU “NextGenerationEU”/PRTR” through project TED2021- 131416B-I00, and by the MCIN with “NextGenerationEU” funds from the European Union (PRTR-C17-I1) within the Energy and Green Hydrogen-CSIC program, as part of the Interdisciplinary Thematic Platform of the CSIC (PTI+) Sustainable Energy Transition+ (PTI-TRANSENER+). Authors acknowledge the Government of Aragon for the grant awarded to the Fuel Conversion Group (T06_23R). C.D.S is grateful for the Juan de la Cierva (JdC) fellowship (Grant Number: JDC2022-048765-I) funded by MICIU/AEI/10.13039/501100011033 and by the European Union NextGenerationEU/PRTR., Peer reviewed