Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 1
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

High-temperature solar-selective coatings based on Cr(Al)N. Part 2: Design, spectral properties and thermal stability of multilayer stacks

  • Rojas, T. Cristina
  • Caro, A.
  • Escobar-Galindo, Ramón
  • Sánchez-López, J.C.
Two multilayer solar selective absorber coatings [Al/CrN0.95/Cr0.96Al0.04N1.08/Cr0.53Al0.47N1.12/Al2O3 (stack #1) and Cr0.96Al0.04N0.89/Cr0.62Al0.38N1.00/Cr0.53Al0.47N1.12/Al2O3 (stack #2)] were deposited on 316L steel by combining direct current (DC) and high power impulse magnetron sputtering (HiPIMS) technologies with the aim of increasing the working limit temperature. The composition and thickness of the constituent layers were optimized using CODE software to achieve a high solar absorptance (α) and low values of thermal emittance (ɛ) in the infrared region. The deposited multilayered stacks were heated during 2 hours in air at 600, 700 and 800 ºC to study their thermal stability and optical performance. Compositional, structural and optical characterization of the stacks (as-prepared and after thermal treatment) was performed. Both stacks presented a good solar selectivity with  > 95% and 25 ºC < 15%, were stable up to 600 ºC and fulfilled the performance criterion PC < 5% after 600 and 700 ºC treatments. Despite the stacks suffered chemical transformations above 600 ºC, partial oxidation (stack #1) and Cr2N formation (stack #1 and #2), the optical properties were optimum up to 700 ºC for stack #1 (α = 94%, ε(25 ºC) =12%) and 600 ºC for stack #2 (α = 93%, ε25 ºC =13%).The solar-to-mechanical energy conversion efficiencies () of the as-deposited and annealed (600 and 700 ºC) samples were up to 20 percentage points higher than the absorber paint commercially used (Pyromark). At 800 ºC, they underwent a further structural transformation, provoked by the oxidation of the inner layers, and they consequently lost their solar selectivity., Peer reviewed