Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 18
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

The effect of environmental conditions on the mechanical and thermoelectric properties of Bi2Ca2Co1.7Ox textured rods

  • Kahraman, F.
  • Diez, J. C.
  • Rasekh, Sh.
  • Madre, M. A.
  • Torres, M. A.
  • Sotelo, Andres
The effect of environmental conditions on the microstructural, mechanical and thermoelectric properties of highly textured Bi2Ca2Co1.7Ox thermoelectric materials was investigated by powder X-ray diffraction, scanning electron microscopy, three point bending test, electrical resistivity, and thermopower measurements. Textured thin rods were directionally grown from the melt through a laser floating zone melting technique. The mechanical and thermoelectric properties of Bi2Ca2Co1.7Ox were determined as a function of two different environmental conditions, air and water. Flexural strength data showed that these oxide materials possess an unsuspected degradation resistance. These good results have been related to the presence of a very thin (~250 µm) low porosity region and relatively small grain sizes, which avoids the internal degradation by water infiltration through the porosity. Moreover, thermoelectric performances, evaluated through the power factor are maintained practically unchanged, independently of the environmental conditions., The authors acknowledge financial support from the Gobierno de Aragón and the Fondo Social Europeo (Consolidated Research Groups T12 and T87) and MINECO-FEDER (Project MAT2013-46505-C3-1-R). F. Kahraman acknowledges a financial grant from the Council of Higher Education (YÖK) in Turkey for international mobility. Authors would like to acknowledge the use of Servicio General de Apoyo a la Investigación-SAI, Universidad de Zaragoza., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Use of laser technology to produce high thermoelectric performances in Bi2Sr2Co1.8Ox

  • Rasekh, Sh.
  • Costa, F. M.
  • Ferreira, Nuno M.
  • Torres, M. A.
  • Madre, M. A.
  • Diez, J. C.
  • Sotelo, Andres
Bi2Sr2Co1.8Ox bulk polycrystalline ceramics were prepared by conventional sintering of powders, obtained by polymer solution method and by directional growth using the laser floating zone technique. Microstructural analysis showed randomly oriented grains in the classical sintered materials, while in the laser-textured samples well oriented crystals with the c-axis nearly perpendicular to the growth direction were observed. A significant reduction on electrical resistivity, compared with the sintered materials, was observed due to the decrease on the secondary phases content. As a consequence, a raise on the power factor of about 2 and 5 times, compared with the classically sintered samples, was obtained for the as-grown and annealed laser-textured samples, respectively. The maximum power factor obtained at 650 °C in the annealed laser-textured samples (∼0.20 mW/K2 m) is much higher than the best value obtained in sinter–forged textured materials at the same temperature., The authors wish to thank the MINECO-FEDER (Project MAT2013--46505-C3-1-R) and the Gobierno de Aragón and Fondo Social Europeo (Research Groups T12 and T87) for financial support. F.M. Costa and N.M. Ferreira gratefully acknowledge the support from UID/CTM/50025/2013 project., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Mechanical and thermoelectric environmental evolution properties of Bi2 Sr2 Co1.8 Ox ceramics textured by laser floating zone technique

  • Kahraman, F.
  • Sotelo, Andres
  • Madre, M. A.
  • Rasekh, Sh.
  • Torres, M. A.
  • Diez, J. C.
Bi2Sr2Co1.8Ox ceramics have been synthesized through solid-state reaction methods and directionally grown from the melt by laser floating zone technique. Mechanical and thermoelectric characteristics of this material were determined by three point bending tests and the four probe technique, respectively. The mechanical and thermoelectric properties of Bi2Sr2Co1.8Ox were determined as a function of the environmental conditions, air and water. Flexural strength data show that textured materials possess a high degradation resistance due to the low porosity of the external part of the rods (~65 µm), which avoids water infiltration and, as a consequence, the internal degradation. Moreover, power factor values are maintained practically unchanged for the samples immersed in water for 24 h., The authors acknowledge financial support from the Gobierno de Aragón and the Fondo Social Europeo (Consolidated Research Groups T12 and T87) and MINECO-FEDER (Project MAT2013-46505-C3-1-R). F. Kahraman acknowledges a financial grant from the Council of Higher Education (YÖK) in Turkey for international mobility., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of synthesis methods on the Ca3Co4O9 thermoelectric ceramic performances

  • Sotelo, Andres
  • Rasekh, Sh.
  • Torres, M. A.
  • Bosque, P.
  • Madre, M. A.
  • Diez, J. C.
Three different synthesis methods producing nanometric grain sizes, coprecipitation with ammonium carbonate, oxalic acid, and by attrition milling have been studied to produce Ca3Co4O9 ceramics and compared with the classical solid state route. These three processes have produced high reactive precursors and all the organic material and CaCO3·have been decomposed in a single thermal treatment. Coprecipitation leads to pure Ca3Co4O9 phase, while attrition milling and classical solid state produce small amounts of Ca3Co2O6 secondary phase. Power factor values are similar for all three samples, being slightly lower for the ones produced by attrition milling. These values are much higher than the obtained in samples prepared by the classical solid state method, used as reference. The maximum power factor values determined at 800 °C (~0.43 mW/K2 m) are slightly higher than the best reported values obtained in textured ones which also show much higher density values., The authors wish to thank the Gobierno de Aragón (Grupos de Investigacion Consolidados T12 and T87) and MINECO-FEDER (MAT2013-46505-C3-1-R) for financial support. Authors would like to acknowledge the use of Servicio General de Apoyo a la Investigación-SAI, Universidad de Zaragoza. Sh. Rasekh acknowledges a JAEPreDoc2010 grant from the CSIC., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Decrease of Ca3Co4O9+δ thermal conductivity by Yb-doping

  • Klirat, G.
  • Aksan, M. A.
  • Rasekh, Sh.
  • Madre, M. A.
  • Diez, J. C.
  • Sotelo, Andres
In this study, the effect of Yb-substitution on the structural, electrical and thermal transport properties of the CaCoO system has been investigated in the low temperature region (between 10 and 300 K). The resistivity of samples increases with raising the Yb-concentration in the system. All the samples show a metal-semiconductor transition below 85 K. In the analysis based on Strongly Correlated Fermi Liquid Model, an increased bandwidth and a reduced electronic correlation are found. It has also been found that the energy gap, E , value also decreases with Yb-substitution. The samples show positive thermoelectric power, indicating that dominant charge carriers are holes in all the samples. The thermoelectric power value decreases with Yb-substitution. From Mott equation, it is determined that the Fermi energy and hole concentration decrease in the Yb-susbtituted samples, compared to the undoped ones. Thermal conductivity, κ, is decreased in about 50% of the measured in undoped samples for the 0.01 and 0.03 Yb-doped samples at 300 K. Highest figure of merit, ZT, value is found to be 5.4 10 at 300 K for the unsubstituted sample and the ZT value decreases by the substitution., The authors wish to thank the MINECO-FEDER (Project MAT2013-46505-C3-1-R) and the Gobierno de Aragón and Fondo Social Europeo (Research Groups T12 and T87) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of secondary annealing process on critical current density in highly textured Bi-2212 superconducting system

  • Aksan, M. A.
  • Madre, M. A.
  • Rasekh, Sh.
  • Constantinescu, G.
  • Torres, M. A.
  • Diez, J. C.
  • Sotelo, Andres
  • Yakinci, M. E.
Bi-2212 samples prepared by a solid-state reaction technique have been grown from the melt using the laser floating zone method. After annealing the as-grown bars, the samples showed a good grain alignment and a high transport critical current density. Secondary annealing processes were performed on the annealed samples with the aim of producing Bi-2212 phase controlled decomposition. Hence, the Bi-2201 phase and the secondary phases, which act as effective pinning centers, were obtained with the secondary annealing process. After these thermal treatments, the transport critical current densities of samples significantly increased, when compared to the annealed ones. The maximum critical current density was achieved when the samples were subjected to secondary annealing at 680°C for 168 h with an improvement of ~80%, compared to the annealed ones. Moreover, it was found that magnetization of the secondarily annealed samples was also increased. The magnetic critical current densities in these secondary annealed samples were about 3 times higher than the values obtained for the annealed ones. These results clearly indicate that the secondary annealing processes lead to the formation of effective pinning centers in the bulk material., The authors acknowledge financial support from the Gobierno de Aragón (Grupos de Investigacion Consolidados T12 and T87) and the Spanish MINECO-FEDER (Project MAT2013-46505-C3-1-R)., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of Na doping on the Ca3Co4O9 thermoelectric performance

  • Constantinescu, G.
  • Rasekh, Sh.
  • Torres, M. A.
  • Bosque, P.
  • Diez, J. C.
  • Madre, M. A.
  • Sotelo, Andres
Ca3-xNaxCo4O9 polycrystalline thermoelectric ceramics with small amounts of Na (x=0, 0.01, 0.03, 0.05, 0.07, and 0.10) have been prepared using the classical solid state method. Microstructural characterization has shown that Na has been incorporated into the Ca3Co4O9 phase and that no Na-based secondary phases have been produced. It has also been found that Na addition promotes grain growth and favours sintering due to the formation of a small amount of liquid phase. Electrical resistivity decreases when Na content increases until 0.07Na addition while Seebeck coefficient is maintained practically unchanged. The improvement in electrical resistivity leads to higher power factor values than the usually obtained in samples prepared by more complex and expensive techniques., This research has been supported by the Spanish MINECO-FEDER (MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón-Fondo Social Europeo (Consolidate research group T12 and consolidated research group T87) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of Yb substitution in Bi-2212 ceramics prepared by laser floating zone technique

  • Özkurt, B.
  • Özçelik, Bekir
  • Madre, M. A.
  • Sotelo, Andres
  • Diez, J. C.
In the present work, the influence of Yb substitution for Bi on the structural, electrical and magnetic properties of textured Bi-2212 ceramics has been investigated. X-ray diffraction studies indicated that the major peaks correspond to the Bi-2212 phase. The SEM images clearly show that there is an increase in the number of secondary phases with raising Yb content while all samples maintain similar grain morphology. Magnetic analysis of all samples has been done by magnetic hysteresis measurements, indicating that an enhancement in the M-H loops is obtained by a low Yb doping. The critical current density of samples was calculated from the M-H curves by using Bean’s critical state model, indicating that sample with 0.05 Yb substitution possesses the highest Jc values., The authors wish to thank the Gobierno de Aragón and Fondo Social Europeo (Grupos de Investigacion Consolidados T12 and T87) and MINECO-FEDER (MAT2013-46505-C3-1-R) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Enhancement of mechanical and thermoelectric properties of Ca3Co4O9 by Ag addition

  • Kahraman, F.
  • Madre, M. A.
  • Rasekh, Sh.
  • Salvador, C.
  • Bosque, P.
  • Torres, M. A.
  • Diez, J. C.
  • Sotelo, Andres
Ca3Co4O9 + x wt.% Ag (x = 0, 1, 3, 5, and 10) polycrystalline thermoelectric ceramics have been prepared by a sol–gel route via nitrates followed by high temperature treatment before sintering. Out-of-plane XRD data have shown that major phase is the Ca3Co4O9 one, accompanied by metallic Ag. SEM observations have agreed with the XRD data. Apparent density measurements have revealed that all samples possess densities ranging between 80% and 90% when Ag content is raised. Mechanical properties have shown a drastic increase of bending stress when Ag is added to the samples. Electrical resistivity decreases with the Ag content, compared with the pure ones, while Seebeck coefficient slightly decreases. Maximum power factor values around 0.43 mW/K2 m at 800 °C have been achieved for the 10 wt.% Ag samples which is much higher than the measured in the pure Ca3Co4O9 samples., This research has been supported by MINECO-FEDER (MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón-Fondo Social Europeo (Consolidated Research Groups T12 and T87) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Thermoelectric properties in Ca3Co4-xMnxOy ceramics

  • Constantinescu, G.
  • Torres, M. A.
  • Rasekh, Sh.
  • Bosque, P.
  • Madre, M. A.
  • Diez, J. C.
Ca3Co4-xMnxOy polycrystalline thermoelectric ceramics with small amounts of Mn have been prepared by the classical solid state method. X-ray diffraction data have shown that Ca3Co4O9 is the major phase, with small amounts of the Ca3Co2O6 one. Moreover, they show that the Mn has been incorporated into these two phases. Electrical resistivity decreases, compared with the values for undoped samples, with Mn content until a minimum for the 0·03 doped ones, increasing for higher Mn substitution. Seebeck coefficient does not change in all the measured temperature range, independently of Mn content. The improvement in electrical resistivity leads ∼30% higher power factor values for the 0·03 Mn doped samples than that obtained in the undoped ones. The maximum power factor at 800°C, ∼0·28 mW K-2 m-1, is close to that obtained in much higher density samples, clearly indicating the good thermoelectric properties of these samples., The authors wish to thank the Gobierno de Aragón (Research Groups T12 and T87) and the MINECO-FEDER (MAT2013-46505-C3-1-R) for financial support. Authors would also like to acknowledge the use of Servicio General de Apoyo a la Investigación-SAI, Universidad de Zaragoza. The technical contributions of C. Estepa and C. Gallego are also acknowledged. Sh. Rasekh acknowledges a JAE-PreDoc 2010 grant from CSIC., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Role of Ag in textured-annealed Bi2Ca2Co1.7Ox thermoelectric ceramic

  • Flahaut, D.
  • Allouche, J.
  • Sotelo, Andres
  • Rasekh, Sh.
  • Torres, M. A.
  • Madre, M. A.
  • Diez, J. C.
Bi2Ca2Co1.7Ox thermoelectric ceramics with small Ag additions (0, 1, 2, 3, 4, and 5 wt.%) have been successfully grown from the melt, using the laser floating zone method and subsequently annealed at 800 °C for 24 h. The microstructure has shown a reduction of the amount of secondary phases for Ag contents up to 4 wt.%. This microstructural evolution leads to a decrease of the electrical resistivity values until an Ag content of 4 wt.%, whereas Seebeck coefficient has been maintained unchanged. This is in agreement with the presence of metallic Ag in all samples, confirmed not only by Energy Dispersive Spectrometry but also by X-ray photoelectron and Auger spectroscopy. These electrical properties lead to maximum power factor values of about 0.30 mW/K2.m at 650 °C for the 4 wt.% Ag containing samples, which is among the best results obtained for this type of materials., This research has been supported by the Spanish MINECO-FEDER (MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón-FEDER (Consolidated Research Groups T87 and T12) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Tailoring Ca3Co4O9 microstructure and performances using a transient liquid phase sintering additive

  • Sotelo, Andres
  • Costa, F. M.
  • Ferreira, Nuno M.
  • Amaral, Vitor S.
  • Amaral, J.S.
  • Rasekh, Sh.
  • Torres, M. A.
  • Madre, M. A.
  • Diez, J. C.
et al., A flexible, adaptable, economical and easily scalable processing route, allowing microstructural control, is presented. It involves classical solid state sintering method and addition of liquid promoting compound. Controlled porosity and high thermoelectric performance have been attained in CaCoO by KCO additions, drastically improving the sintering procedure. KCO behaves as transient liquid phase, providing microstructural benefits, vanishing during sintering. Electrical resistivity was improved by enhanced grains connectivity and growth. Significant increase in Seebeck coefficient at high temperatures has been produced while lattice thermal conductivity was unaffected. The best ZT value, estimated at 800°C, assuming the thermal conductivity value at 140°C, is 0.35 for 5wt.% KCO samples. These values are significantly higher than that obtained in highly-dense textured materials at the same temperature. The results suggest that this approach is very effective for preparing highly-performing CaCoO-based thermoelectric materials with relatively high porosity to control thermal conductivity., The authors wish to thank the MINECO-FEDER (MAT2013-46505-C3-1-R) and Gobierno de Aragón-Fondo Social Europeo (Research Groups T12 and T87) for financial support. This research was also partially supported by FCT, Portugal (IF/00302/2012 and PEst-C), project RECI/CTM-CER/0336/2012 co-financed by FEDER, QREN reference COMPETE: FCOMP-01-0124-FEDER-027465, and the projects financed by national funds through the FCT/MEC: UID/CTM/50025/2013, UID/CTM/50011/2013., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Thermoelectric properties of directionally grown Bi2Ba2Co2Oδ/Ag composites: effect of annealing

  • Rasekh, Sh.
  • Sotelo, Andres
  • Torres, M. A.
  • Bosque, P.
  • Madre, M. A.
  • Diez, J. C.
Bi2Ba2Co2Oδ thermoelectric ceramics with Ag additions (0, 1, 3, and 5 wt%) have been successfully textured using the laser floating zone method. Microstructure has shown that samples are composed by thermoelectric grains, together with a high amount of secondary phases, and that 3 wt% Ag addition leads to the best grain orientation. These microstructural benefits have been reflected in the highest thermoelectric performances determined in these samples. It has also been found that annealing procedure leads to a drastic decrease of secondary phases amount and raises the oxygen content in the thermoelectric phase. These modifications are reflected in an important decrease of electrical resistivity, ρ (compared to the as-grown samples) without drastic modification of Seebeck coefficient, S. As a consequence, the highest thermoelectric performances, determined through the power factor, have been reached in the 3 wt% Ag textured and annealed samples in the whole measured temperature range. The maximum PF (=S/ρ) values at 650 °C determined in these samples are very close to the highest reported in single crystals or very low rate LFZ grown Bi2Ba2Co2Oδ compounds, making them very attractive for practical applications., This research has been supported by the Spanish MINECO-FEDER (MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón and Fondo Social Europeo (Consolidated Research Groups T87 and T12) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Improved thermoelectric performances in textured Bi1.6Pb0.4Ba2Co2Oy/Ag composites

  • Sotelo, Andres
  • Rasekh, Sh.
  • Torres, M. A.
  • Bosque, P.
  • Madre, M. A.
  • Diez, J. C.
BiPbBaCoO thermoelectric ceramics with small Ag additions (0, 1, 3, and 5 wt%) have been textured using the laser floating zone method. Microstructure has shown a slight decrease on the secondary phases content and a better grain alignment in Ag added samples. These microstructural features are reflected in the thermoelectric properties, which have shown a significant decrease of electrical resistivity, when the Ag content is raised. In spite of a corresponding decrease of Seebeck coefficient, all the Ag-containing samples possess higher Power Factor values than the BiPbBaCoO ones. Moreover, the maximum Power Factor values (about 0.36 mW/K.m at 650 °C) have been measured in BiPbBaCoO+3 wt% Ag samples, which are the best results reported in this family of materials., This research has been supported by the MINECO-FEDER (Project MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón (Consolidated Research Groups T87 and T12) for financial support., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Improvement of structural and superconducting properties of Bi-2212 textured rods by substituting sodium

  • Nane, O.
  • Özçelik, Bekir
  • Sotelo, Andres
  • Madre, M. A.
In this paper, the physical and superconducting properties of BiSrCaNaCuO with x=0.0, 0.05, 0.075, 0.1, and 0.20 textured superconducting fiber rods prepared by a laser floating zone (LFZ) technique were studied. The effects of Na substitution for Ca have been investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX), transport measurements, dc-magnetization, magnetic hysteresis and magnetic critical current density. The powder XRD patterns of samples have indicated that Bi-2212 phase is the major one, independently of Na content. The best critical temperature, T, has been found as 93.3 K from M-T data for the sample with 0.075 Na substitution. The maximum magnetic J value has been calculated as 1.35×10 A/cm at 10 K for the 0.10 Na sample. The maximum transport critical current density has directly been measured as 1.3×10 A/cm at 77 K for the 0.05Na sample., This work is supported by Research Fund of Çukurova University, Adana, Turkey, under Grant contracts no: FBA-2015-3934. M. A. Madre and A. Sotelo wish to thank the Gobierno de Aragón and Fondo Social Europeo (Grupo de Investigacion Consolidado T12) and MINECO-FEDER (project MAT2013-46505-C3-1-R) for financial support. M. A. Madre also acknowledges funding from MINECO-FEDER (Project ENE2014-52105-R)., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

High thermoelectric performance in Bi2-xPbxBa2Co2Oy promoted by directional growth and annealing

  • Madre, M. A.
  • Costa, F. M.
  • Ferreira, Nuno M.
  • Rasekh, Sh.
  • Torres, M. A.
  • Diez, J. C.
  • Amaral, Vitor S.
  • Amaral, J.S.
  • Sotelo, Andres
Bi2-xPbxBa2Co2Oy (x=0.0, 0.2, 0.4, and 0.6) misfit compounds were grown by the laser floating zone technique. Microstructural analysis has shown the formation of thermoelectric grains together with high amount of secondary phases. Thermoelectric grains orientation is increased until 0.4Pb, while further substitution drastically destroys the preferential grain orientation. Electrical resistivity is very low compared with the values obtained in sintered materials, spectacularly increasing power factor. Moreover, the performance of these materials was further improved subjecting the as-grown samples to a postannealing step due to the rise of thermoelectric phase content. These microstructural modifications led to a high decrease of electrical resistivity, improving power factor in around a factor two at room temperature, compared with the as-grown samples. Moreover, the low thermal conductivity of the textured annealed samples leads to a maximum estimated ZT value of 0.53 for the 0.2 Pb-doped samples, much higher than the reported in literature., This research has been supported by the Spanish MINECO-FEDER (MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón-Fondo Social Europeo (Consolidated Research Groups T12 and T87) for financial support and to C. Gallego, C. Estepa and J. A. Gomez for their technical assistance. The authors also acknowledge the PEst-C/CTM/LA 25/2013-14, RECI/CTM-CER/0336/2012 co-financed by FEDER, QREN reference COMPETE: FCOMP-01-0124-FEDER-027465, “Facing the challenges of characterizing novel thermal materials and processes (Heat@UA)” and CICECO-Aveiro Institute of Materials (Ref. FCT UID /CTM /50011/2013) funding., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of Na substitution on superconducting properties of Bi-2212 ceramics prepared by Sinter-Forged process

  • Nane, O.
  • Özçelik, Bekir
  • Sotelo, Andres
  • Madre, M. A.
Bulk textured BiSrCaNaCuO (x = 0.0, 0.05, 0.075 0.1, 0.15, and 0.20) ceramics have been prepared by a polymer solution method followed by sinter-forging process. The microstructure and superconducting properties of textured samples were affected by Na substitution. According to XRD data, all samples show that Bi-2212 phase is the major one, and main peaks corresponded to the (00ℓ) diffractions confirming that the crystallographic c-axis is perpendicular to the surface. SEM micrographs showed that samples are composed of well-stacked and oriented grains. The best critical temperature, T, was measured as 85.6 K for x = 0.075. The critical current density Jc, values decrease gradually with the increase of applied magnetic field. The maximum calculated Jc was 1.38 × 10 A/cm at 10 K for 0.075 Na sample which is about four times higher than the 0.34 × 10 A/cm value determined for the pure sample. The anisotropic properties of these textured materials have been investigated using magnetic measurements., This work is supported by Research Fund of Çukurova University, Adana, Turkey, under grant contracts no: FBA-2014-3500. A. Sotelo and M.A. Madre acknowledge the Gobierno de Aragón and Fondo Social Europeo (Grupo de Investigacion Consolidado T12) and MINECO-FEDER (MAT2013-46505-C3-1-R) for financial support. M.A. Madre also acknowledges MINECO-FEDER (Project ENE2014-52105-R) for funding. Authors would like to acknowledge the use of Servicio General de Apoyo a la Investigación-SAI, Universidad de Zaragoza. This work is also supported by Research Fund of Hakkari University, Turkey, under grant contracts no: MF2014BAP1., Peer Reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Enhanced electrical and thermoelectric properties from textured Bi1.6Pb0.4Ba2Co2Oy/Ag composites

  • Madre, M. A.
  • Rasekh, Sh.
  • Torres, M. A.
  • Bosque, P.
  • Diez, J. C.
  • Sotelo, Andres
Bi1.6Pb0.4Ba2Co2Oy/3 wt% Ag composites have been textured using the laser floating zone technique. Microstructural observations have shown the formation of relatively high amounts of secondary phases and cracks along the plate-like grains in the as-grown materials. In spite of these microstructural features, electrical properties have not been drastically decreased. Annealing of these as-grown rods has enhanced the grains connectivity, decreased the contents of the secondary phases, and healed the cracks, thereby increasing their electrical performances. It has been deduced that oxygen content in the thermoelectric phase has not been significantly modified through annealing, as demonstrated by the very similar Seebeck values at room temperature in the as-grown and annealed samples. As a consequence of the low electrical resistivity values in the annealed materials, they reached higher power factor values than the as-grown ones. The highest power factor at room temperature is in the range of those reported for single crystals, while at 650 °C, it is the highest reported in Bi–Ba–Co–O polycrystalline family so far., This research has been supported by the MINECO-FEDER (Project MAT2013-46505-C3-1-R). The authors wish to thank the Gobierno de Aragón-FEDER (Consolidated Research Groups T87 and T12) for their financial support., Peer Reviewed