Pasar al contenido principal

NUEVOS SUPERCONDENSADORES HIBRIDOS BASADOS EN ELECTRODOS DE NANOCOMPOSITES DE CARBONO/GRAFENO DERIVADOS DE (OXI)CARBUROS

MAT2016-78700-R

•
Nombre agencia financiadora Agencia Estatal de Investigación
Acrónimo agencia financiadora AEI
Programa Programa Estatal de I+D+i Orientado a los Retos de la Sociedad
Convocatoria Proyectos I+D+i Retos de Investigación
Año convocatoria 2016
Plan Estatal 2013-2016 Plan Estatal de Investigación Científica y Técnica y de Innovación
Centro beneficiario AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 1
Encontrada(s) 1 página(s)

RUA. Repositorio Institucional de la Universidad de Alicante
Publicación Otros (Other)

Formation of carbon nanofibers with Ni catalyst supported on a micro-mesoporous glass

  • Mazo, M. Alejandra
  • Sanguino, Javier
  • Martin-Gullon, Ignacio
  • Rubio, Juan
  • Martin-Gullon, Ignacio|||/items/04aa2bce-ad55-4c4a-ba48-66e07d390b63
The Ni/SiO2 system is one of the most interesting to produce COx-free H2 and valuable carbon nanofibers (CNFs) by the catalytic decomposition of CH4. SiO2 is one of the most effective support while Ni catalyst displays long life and high activity. We studied the catalytic chemical vapor deposition (CCVD) process of CH4 within Ni/glass system at relatively low temperature (600 °C) during long times (3 h), varying the amount of the catalyst (2.3–17.8% Ni(%)) and the carbon source (100:200 to 100:0, CH4:N2). As the amount of Ni and CH4 increases, the formation of CNFs is enhanced giving as a result CNFs/glass materials with more amount, longer and thicker CNFs. The initial microstructure of the glass support and the way of Ni catalyst is deposited play a decisive role. Pristine porous glass displays a microstructe of interconnected mesopores which are progressively filled with Ni, producing ink-bottle pores with open ends. After the CCVD process as the amount of Ni or CH4 increases, the porosity of the Ni-doped glass is reduced due to the progressively filling of the mesopores (4 nm) with CNFs. Furthermore, due to the formation of large entanglements of CNFs new pores appear (20–70 nm) depending on the processing conditions. Fish-bone with hollow core and bamboo-like CNFs are found over the surface and also inside the porous glass support. It is observed a base-growth mechanism due to the strong interaction between the catalyst and the support, which prevents the Ni deactivation enhancing its activity for long times.