Data for Novel Ir1–xCoxO2 thin films: growth and characterization

  • Laguna-Marco, M. A.
  • Herrero-Albillos, Julia
  • Aguirre, Myriam H.
  • Rueda-Jiménez, Marcos
  • Mikulska, Iuliia
  • Proyecto: PID2020-115159GB-I00
[Ir1–xCoxO2 thin films were prepared by reactive magnetron co–sputtering deposition on Si substrates at room temperature (RT) from metallic Ir and Co targets. Crystal structures were characterized by powder X-ray diffraction (XRD) at room temperature in a Rigaku D-Max system using Cu Kalpha wavelength. The resistivity measurements were carried out in a PPMS-9T. The magnetic measurements were carried out in a SQUID magnetometer MPMS–XL (both from Quantum Design). Transmission electron microscopy images, HRTEM (High resolution transmission electron microscopy) and STEM-HAADF (scanning TEM with high angular annular dark field detector), were performed by Tecnai F30 and Titan G2 80-300 keV (with aberration corrected probe), respectively, operated at 300 keV. The compositional analysis profile was performed by energy dispersive spectroscopy (EDS) in an Oxford Aztec equipment in situ STEM-HAADF analysis. The lamellae for TEM analysis were prepared by focused ion beam in a commertial Helios 650 N dual beam equipment. X–ray absorption spectroscopy (XAS) measurements were carried out at the B18 beamline of the Diamond Light Source. Co K-edge and Ir L2,3-edge XAS spectra of the films were measured in fluorescence mode using Quick-EXAFS technique. A Si (111) double crystal monochromator was used to select the incident X-ray energy. Co K-edge (Ir L3-edge) measurements have been performed using collimating mirror with Pt (Cr) coating. The fluorescence measurements have been performed using Canberra 36-pixel Monolithic Segmented Hyper Pure Germanium Detector with the STFC Xspress4 Digital Pulse Processor.], Spanish MICINN Project No. PID2020-115159GBI00/AEI/10.13039/501100011033; Regional Government of Aragon (Grant No. E12-23R RASMIA); European Commission under the H2020-MSCA-RISE-2020 MELON project Nº 872631 and H2020-MSCA-RISE-2021 ULTIMATE-I project Nº 101007825., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

High-quality epitaxial five-layer Aurivillius films with in-plane ferroelectricity for electrocaloric cooling [Dataset]

  • Lafuerza, Sara
  • Blasco, Javier
  • Evangelisti, Marco
  • Subías, Gloria
  • Gracia, David
  • Pardo, José A.
  • Barriuso, Eduardo
  • Torrelles, Xavier
  • Padilla-Pantoja, Jessica
  • Caicedo, José Manuel
  • Santiso, José
[Description of methods used for collection/generation of data]: The structural characterization of the films was performed by X-ray diffraction (XRD) 2θ/ω wide scans, X-ray reflectivity (XRR) and reciprocal space maps (RSMs) of selected asymmetric reflections, by using a four-circle X-ray diffractometer (Malvern-Panalytical X'pert Pro MRD) and standard Cu Kα1,2 X-ray source with a parabolic mirror (for reciprocal space maps, a 2xGe(220) monochromator was added to the incident optics). A 2D array PIXcel detector was used. The topography of selected films was studied using atomic force microscopy (AFM) in contact mode (Keysight 5100) over different areas. The structure of the films was also analyzed by high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) on a Fisher Spectra microscope operated at 200 kV. Cross-section lamellas were prepared by focused ion beam (FIB) on a SBTO5 film deposited under optimized conditions, with the cut oriented to show STO [100] zone axis., [Ferroelectric and Electrocaloric Properties]: These properties were investigated by measuring the in-plane polarization using the IDEs with a 500 V-built-in ferroelectric tester (Precision Premier II model, Radiant Technologies). Hysteresis measurements were carried out based on a bipolar triangular wave excitation, and also remanent hysteresis measurements based on half triangular waves following the principle of the positive-up negative-down (PUND) method. The frequency of the triangular wave excitation was set to 2 kHz for both measurement protocols. Temperature (T)-dependent polarization versus E field, P(E, T) curves, were measured on heating in a dedicated homemade cell allowing a maximum temperature of 140 °C. Samples were immersed in a silicon oil bath during the polarization measurements to avoid electric discharges., High-quality purely c-axis oriented epitaxial thin films of the Aurivillius phase Sr2Bi4Ti5O18 with n = 5 (Sr,Bi)TiO3 perovskite-like layers, are grown on SrTiO3 substrates by pulsed laser deposition. The highest crystalline quality is obtained with a 20 wt.% Bi-excess target and average stacking order values in the proximity of the ideal value n = 5 are attained for an optimum deposition temperature of 650 °C. Scanning transmission electron microscopy reveals regions with n ranging from 4 to 6 around an average thickness of n = 5, in agreement with the X-ray diffraction analysis. Interdigital electrodes are used to probe the in-plane polarization and survey the electrocaloric properties. A maximum adiabatic temperature change of ΔT ∼ 0.95 °C for an electric field of 150 kV cm−1 is observed at ≈135 °C. Larger values are expected at higher temperatures around the ferroelectric Curie temperature, TC. Since TC of Sr2Bi4Ti5O18 can be tuned by codoping, the findings pave the way toward a large electrocaloric effect at ambient temperature., S.L. acknowledges funding from the European Union's Horizon 2020 research and innovation program under the Marie Skłodowska-Curie grant agreement No. 101029019. This work was also supported by Ministerio de Ciencia, Innovación y Universidades (PID2021-124734OB-C21), “Severo Ochoa” Programme for Centres of Excellence in R&D (CEX2023-001286-S, CEX2023-001263-S and CEX2021-001214-S) and Diputación General de Aragón (E11-23R, E12-23R). D. G. acknowledges financial support from the Gobierno de Aragón through a doctoral fellowship. Authors would like to acknowledge C. Cosculluela from Unidad Técnica en Ingeniería de Microdispositivos (INMA) and R. Valero for the IDEs fabrication at the National Facility ELECMI ICTS, node “Laboratorio de Microscopías Avanzadas”, through Servicio General de Apoyo a la Investigación from Universidad de Zaragoza. The authors also acknowledge the use of instrumentation as well as the technical advice provided by the Joint Electron Microscopy Center at ALBA (JEMCA) and funding from Grant IU16-014206 (METCAM-FIB) to ICN2 funded by the European Union through the European Regional Development Fund (ERDF), with the support of the Ministry of Research and Universities, Generalitat de Catalunya. J. S. acknowledges B. Mundet, F. Belarre and M. Rosado for the STEM images and FIB fabrication of the lamellas, as well as the financial support of the European Commission through the Horizon H2020 funding by H2020-MSCA-RISE-ID:101007825 –ULTIMATE-I. X. T. acknowledges financial support by Ministerio de Ciencia, Innovación y Universidades (PID2021-123276OB-I00)., With funding from the Spanish government through the "Severo Ochoa Centre of Excellence" accreditation (CEX2023-001286-S)., With funding from the Spanish government through the "Severo Ochoa Centre of Excellence" accreditation (CEX2023-001263-S)., With funding from the Spanish government through the "Severo Ochoa Centre of Excellence" accreditation (CEX2021-001214-S)., Peer reviewed