Thermal energy storage-enhanced self-leveling mortars made of pre-placed perlite aggregates filled with bio-based phase change materials

  • Zanjani, Mahdi M.K.
  • Ferreira, Saulo Rocha
  • Lagazzo, Alberto
  • Basbus, Juan F.
  • Fachinotti, Victor D.
  • Caggiano, Antonio
Data will be made available on request., This study investigates the development and performance of self-leveling mortars (SLMs) enhanced with Phase Change Materials (PCMs) and expanded perlite aggregates to provide Thermal Energy Storage (TES) functionality for energy-efficient buildings. A cementitious encapsulation method was used to coat PCM-saturated perlite, forming durable macro-encapsulated aggregates. To preserve the structural integrity of these inclusions during casting, the pre-placed aggregate method was employed in combination with a highly flowable self-consolidating mortar matrix. Three mortar formulations were produced and analyzed: (a) reference SLM, (b) SLM with expanded perlite, and (c) SLM with PCM-filled perlite. Thermal performance was assessed through dynamic “DKK” tests and a custom ASTM C1363-19 Hot-Box apparatus. Tests revealed that PCM-enhanced mortars achieved the highest thermal buffering effect, exhibiting plateaus at 25–30 °C and reduced heat flux values. The apparent thermal conductivity, during the PCM phase change, dropped to 0.28 W/(m·K), demonstrating effective latent heat absorption. The results clearly demonstrate enhanced passive thermal regulation with delayed heat transfer responses, supporting the use of PCM-perlite SLMs as energy-storage building materials. Complementary tests were then performed to verify the material, mechanical, and durability feasibility of the composites. Mechanical tests showed that the reference SLM achieved the highest compressive and flexural strengths, at 60.14 MPa and 5.79 MPa, respectively. The incorporation of expanded perlite reduced the compressive strength to 29.02 MPa, while PCM-enhanced aggregates further reduced it to 17.62 MPa. A slight improvement in flexural strength was observed for the PCM composite (i.e., 3.46 MPa) compared to the uncoated perlite (3.08 MPa), indicating potential reinforcement by the encapsulation shell. Water absorption tests revealed that PCM-enhanced perlite mortars exhibited low absorption within the first 180 min but experienced a sharp increase at 72 h (i.e., 3 days), surpassing all other mixes and suggesting long-term permeability issues. SEM-EDS analyses indicated high Ca/Si ratios (∼7.75) in the shell, and TGA results showed minimal portlandite decomposition, both supporting the hypothesis of calcium hydroxide consumption by silica fume to form additional C–S–H gels. Overall, PCM-perlite SLMs show strong potential for TES-enabled building applications., This work was supported within the framework of the following projects/grants: PRIN 2022 project OPTIMA (OPTImized use of phase change MAterials for energy and seismic retrofitting of buildings). Project Code 2022MP7A4C, funded by the Italian Ministry of University and Research (MUR) under the PRIN 2022 call, in accordance with the Decree of the Secretary General No. 1401 of 18 September 2024, for the period 2025–2027. European Union – Horizon 2020 Marie Skłodowska-Curie Actions: HORIZON-TMA-MSCA-SE-2021 “BEST – Bio-based Energy-efficient Materials and Structures for Tomorrow” (Grant Agreement No. 101086440, DOI: 10.3030/101086440). HORIZON-MSCA-2023-PF-01-01 - MSCA “SMART-NRG – Solutions for constructions and building materials based on Energy Absorption”, Marie Skłodowska-Curie Postdoctoral Fellowship (Grant Agreement No. 101153320, DOI 10.3030/101153320). Work Package WP5 – “Interventi integrati e sostenibili per costruzioni esistenti” (Coordinated by Prof. F. da Porto and Prof. A. Prota), as part of the DPC-ReLUIS 2024–2026 projects funded by the Dipartimento della Protezione Civile. Italian National Recovery and Resilience Plan (PNRR), Mission 4 “Education and Research”, Component 1, Investment 3.4 “Transnational Education (TNE)”, funded by the European Union – NextGenerationEU, under the MUR Directorial Decree prot. no. 167 of 03 October 2023, “Avviso per la concessione di finanziamenti destinati a iniziative educative transnazionali”, within the project TNE23-00074 “Fragility, Marginality, Mobility, Energy Transition – FraMMET”, CUP C96G23000270001., Peer reviewed
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

Thermal energy storage-enhanced self-leveling mortars made of pre-placed perlite aggregates filled with bio-based phase change materials

  • Zanjani, Mahdi M.K.
  • Ferreira, Saulo Rocha
  • Lagazzo, Alberto
  • Basbus, Juan F.
  • Fachinotti, Victor D.
  • Caggiano, Antonio
This study investigates the development and performance of self-leveling mortars (SLMs) enhanced with Phase Change Materials (PCMs) and expanded perlite aggregates to provide Thermal Energy Storage (TES) functionality for energy-efficient buildings. A cementitious encapsulation method was used to coat PCM-saturated perlite, forming durable macro-encapsulated aggregates. To preserve the structural integrity of these inclusions during casting, the pre-placed aggregate method was employed in combination with a highly flowable self-consolidating mortar matrix. Three mortar formulations were produced and analyzed: (a) reference SLM, (b) SLM with expanded perlite, and (c) SLM with PCM-filled perlite. Thermal performance was assessed through dynamic “DKK” tests and a custom ASTM C1363-19 Hot-Box apparatus. Tests revealed that PCM-enhanced mortars achieved the highest thermal buffering effect, exhibiting plateaus at 25–30 °C and reduced heat flux values. The apparent thermal conductivity, during the PCM phase change, dropped to 0.28 W/(m·K), demonstrating effective latent heat absorption. The results clearly demonstrate enhanced passive thermal regulation with delayed heat transfer responses, supporting the use of PCM-perlite SLMs as energy-storage building materials. Complementary tests were then performed to verify the material, mechanical, and durability feasibility of the composites. Mechanical tests showed that the reference SLM achieved the highest compressive and flexural strengths, at 60.14 MPa and 5.79 MPa, respectively. The incorporation of expanded perlite reduced the compressive strength to 29.02 MPa, while PCM-enhanced aggregates further reduced it to 17.62 MPa. A slight improvement in flexural strength was observed for the PCM composite (i.e., 3.46 MPa) compared to the uncoated perlite (3.08 MPa), indicating potential reinforcement by the encapsulation shell. Water absorption tests revealed that PCM-enhanced perlite mortars exhibited low absorption within the first 180 min but experienced a sharp increase at 72 h (i.e., 3 days), surpassing all other mixes and suggesting long-term permeability issues. SEM-EDS analyses indicated high Ca/Si ratios (∼7.75) in the shell, and TGA results showed minimal portlandite decomposition, both supporting the hypothesis of calcium hydroxide consumption by silica fume to form additional C–S–H gels. Overall, PCM-perlite SLMs show strong potential for TES-enabled building applications.