Biointegration of corneal macroporous membranes based on poly(ethyl acrylate) copolymers in an experimental animal model

  • Alió del Barrio, Jorge L.
  • Chiesa, Massimo
  • Garagorri, Nerea
  • Briz, Nerea
  • Fernández Delgado, Jorge
  • Sancho-Tello Valls, María
  • Carda Botella, Carmen
  • García-Tuñón, Ignacio
  • Bataille, Laurent
  • Rodríguez, Alejandra
  • Arnalich Montiel, Francisco
  • Antolinos Turpín, Carmen María
  • Gallego-Ferrer, Gloria|||0000-0002-2428-0903
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
  • Gómez-Tejedor, José-Antonio|||0000-0001-6854-0829
Currently available keratoprosthesis models (nonbiological corneal substitutes) have a less than 75% graft survival rate at 2 years. We aimed at developing a model for keratoprosthesis based on the use of poly(ethyl acrylate) (PEA)-based copolymers, extracellular matrix-protein coating and colonization with adipose-derived mesenchymal stem cells. Human adipose tissue derived mesenchymal stem cells (h-ADASC) colonization efficiency of seven PEA-based copolymers in combination with four extracellular matrix coatings were evaluated in vitro. Then, macroporous membranes composed of the optimal PEA subtypes and coating proteins were implanted inside rabbit cornea. After a 3-month follow-up, the animals were euthanized, and the clinical and histological biointegration of the implanted material were assessed. h-ADASC adhered and survived when cultured in all PEA-based macroporous membranes. The addition of high hydrophilicity to PEA membranes decreased h-ADASC colonization in vitro. PEA-based copolymer containing 10% hydroxyethyl acrylate (PEA-HEA10) or 10% acrylic acid (PEA-AAc10) monomeric units showed the best cellular colonization rates. Collagen plus keratan sulfate-coated polymers demonstrated enhanced cellular colonization respect to fibronectin, collagen, or uncoated PEAs. In vivo implantation of membranes resulted in an extrusion rate of 72% for PEA, 50% for PEA-AAc10, but remarkably of 0% for PEA-HEA10. h-ADASC survival was demonstrated in all the membranes after 3 months follow-up. A slight reduction in the extrusion rate of h-ADASC colonized materials was observed. No significant differences between the groups with and without h-ADASC were detected respect to transparency or neovascularization. We propose PEA with low hydroxylation as a scaffold for the anchoring ring of future keratoprosthesis., Contract grant sponsor: Fundacio Marato de TV3, Spain
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Assessment of Parameters Influencing fiber characteristics of chitosan nanofiber membrane to optimize fiber mat productioi

  • Areias, A.C.
  • Gómez-Tejedor, José Antonio
  • Sencadas, V.
  • Alio, J.
  • Lanceros-Mendez, S.
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
Electrospun chitosan nanofiber mats have been obtained using chitosan solutions in a mixture of trifluoroacetic acid and dichloromethane. The relationship between processing parameters (solvent composition, polymer concentration in the solution, feeding rate, applied voltage, traveling distance between the needle, and the collector) and fiber morphology was studied. Taguchi's methodology was followed to determine which parameters have the strongest influence on mean fiber diameter and fiber homogeneity. Chitosan nanofibers obtained with this procedure were water soluble due to the protonation of amine side groups but were successfully neutralized by immersion in calcium carbonate solutions. It was established that fiber diameter is mainly determined by the solution concentration and the distance from the needle to the collector while other parameters have less influence. The set of parameters that produce the thinnest fibers were a concentration of 8 wt%, a TFA/DCM ratio of 80:20 (v/v%), a voltage of 30 kV, a flow rate of 6.0 mL/h, a gap distance of 10 cm, using a needle diameter of 0.5, allowing to produce randomly oriented mats with a mean fiber thickness of 66 nm. © 2012 Society of Plastics Engineers., Contract grant sponsor: Portuguese Foundation for Science and Technology (FCT); contract grant number: NANO/NMed-SD/0156/2007; Contract grant sponsor: FCT; contract grant number: SFRH/BPD/63148/2009; Contract grant sponsor: Spanish Ministry of Science and Innovation; contract grant number: MAT2010-21611-C03-01; Contract grant sponsor: Programa Nacional de Internacionalizacion de la I+D; contract grant number: EUI2008-00126; Contract grant sponsors: Regenerative Medicine collaboration agreement from the Conselleria de Sanidad (Generalitat Valenciana), and the Instituto de Salud Carlos III (Ministry of Science and Innovation); Contract grant sponsors: Spanish Ministry of Science and Innovation, Centro para el Desarrollo Tecnologico Industrial (CDTI), CENIT: "Customized Eye Care'' and CeyeC; contract grant number: CEN-20091021; Contract grant sponsor: The translation of this paper was funded by the Universitat Politecnica de Valencia, Spain.