Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 2
Encontrada(s) 1 página(s)

Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

Iron oxide ores as carriers for the production of high purity hydrogen from biogas by steam–iron process

  • Lachén, J.
  • Plou, J.
  • Durán, P.
  • Herguido, J.
  • Peña, J.A.
Production of high purity hydrogen (<50 ppm CO) by steam–iron process (SIP) from a synthetic sweetened biogas has been investigated making use of a natural iron ore containing up to 81 wt% of hematite (Fe2O3) as oxygen carrier. The presence of a lab-made catalyst (NiAl2O4 with NiO excess above its stoichiometric composition) was required to carry out the significant transformation of mixtures of methane and carbon dioxide in hydrogen and carbon monoxide by methane dry reforming reaction. Three consecutive sub-stages have been identified along the reduction stage that comprise A) the combustion of CH4 by lattice oxygen of NiO and Fe2O3, B) catalyzed methane dry reforming and C) G–G equilibrium described by the Water-Gas-Shift reaction. Oxidation stages were carried out with steam completing the cycle. Oxidation temperature was always kept constant at 500 °C regardless of the temperature used in the previous reduction to minimize the gasification of eventual carbon deposits formed along the previous reduction stage. The presence of other oxides different from hematite in minor proportions (SiO2, Al2O3, CaO and MgO to name the most significant) confers it an increased thermal resistance against sintering respecting pure hematite at the expense of slowing down the reduction and oxidation rates. A “tailor made” hematite with additives (Al2O3 and CeO2) in minor proportions (2 wt%) has been used to stablish comparisons in performance between natural and synthetic iron oxides. It has been investigated the effect of the reduction temperature, the proportion of methane to carbon dioxide in the feed (CH4:CO2 ratio) and the number of repetitive redox cycles.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

High purity hydrogen from biogas via steam iron process: Preventing reactor clogging by interspersed coke combustions

  • Lachén, J.
  • Herguido, J.
  • Peña, J.A.
Production of high purity hydrogen from biogas by combined dry reforming of methane and steam iron process (SIP), outlines a serious drawback with the possible formation of coke deposits along reduction steps of the iron oxide. Steam used along reoxidations, which regenerates the iron oxide and force the release of high purity hydrogen, could also be responsible of the gasification of such coke deposits and the consequent contamination of hydrogen with carbonaceous species such as CO or CO2. Oxidations at low enough temperature can inhibit coke gasification, but paradoxically, increasing amounts of coke upon repeated cycles will provoke reactor clogging sooner or later. To circumvent this issue, a strategy consisting of interspersing coke combustion stages with diluted oxygen within the regular cycles of reduction with biogas and reoxidation with steam releasing hydrogen, has been analyzed with three solids based on iron oxide. It has been verified that including coke combustion stages within the regular scheme of redox cycles, not only counteracts both bed clogging and catalyst deactivation by coking, but also breaks down the trend to lose (by sintering) active material for the redox process, thus allowing the extension of the useful life of the solid.