DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación
Artículo científico (JournalArticle)
Optical second harmonic generation from LaAlO3/SrTiO3 interfaces with different in-plane anisotropies
Oxide growth with semiconductor-like accuracy allows the fabrication of atomically precise
thin films and interfaces displaying a wide range of phases and functionalities that are
absent in the corresponding oxide bulk materials. Among the other properties it was found
that a two-dimensional electronic gas is formed under some circumstances at the LaAlO3/
SrTiO3(0 0 1) interface separating two typical insulating perovskite crystals. The origin of this
conducting state has been discussed at length, since different doping mechanisms can act in
these material systems. Many experimental results point to the so-called polar catastrophe
scenario as the principal mechanism driving the formation of the two-dimensional electronic
gas. According to this mechanism, the existence of an interfacial polar discontinuity is the key
ingredient to drive an electronic reconstruction at the LaAlO3/SrTiO3(0 0 1) interface and the
consequent formation of a two-dimensional electron gas. This simple picture has been often
questioned by the existence of material systems whose interface are predicted being non-polar
according to the simplistic ‘ionic’ limit but that display an electrical behavior analogous to
that of LaAlO3/SrTiO3(0 0 1) interfaces. This is the case of the LaAlO3/SrTiO3(1 1 0), i. e., a
LaAlO3/SrTiO3 interface with a different in-plane orientation. It is evident that to solve such
kind of controversies a detailed investigation of the polar or non-polar state of these interfaces
is needed, although this is not simple for the lack of experimental tools that are specifically
sensitive to interfacial polarity. Here we apply Optical Second Harmonic Generation to
investigate LaAlO3/SrTiO3 interfaces with different in-plane orientations to bridge this gap.
By comparing our results with recent theoretical findings, we will arrive to the conclusion that
the real LaAlO3/SrTiO3(1 1 0) interface is strongly polar., This work was supported by ‘Ministero Istruzione Università e
Ricerca’ and ‘Consiglio Nazionale delle Ricerche’. It was also
supported by ‘Spanish Ministerio de Ciència, Innovaciòn y
Universidades’ through Grants No. MAT2017-85232-R (AEI/
FEDER, EU), No. MAT2014-56063-298 C2-1-R, and Severo
Ochoa SEV-2015-0496, and the ‘Generalitat de Catalunya’
through Grant No. 2017 301 SGR1377., Peer reviewed
Proyecto:
AEI / Plan Estatal de Investigación Científica y Técnica y de Innovación 2017-2020 MAT2017-85232-R
,
MINECO / Plan Estatal de Investigación Científica y Técnica y de Innovación 2013-2016 MAT2014-56063-298 C2-1-R
,
MINECO / Plan Estatal de Investigación Científica y Técnica y de Innovación 2013-2016 SEV-2015-0496