Enhanced hydrothermal resistance of Y-TZP ceramics through colloidal processing

  • E. Rayón|||0000-0002-0653-2046
  • Salvador Moya, Mª Dolores|||0000-0002-4242-478X
  • Manjón, Francisco-Javier|||0000-0002-3926-1705
  • Moreno, R.
  • Alcazar, C.
  • Jimenez-Pique, E.
  • Llanes, L.
Two commercial zirconia powders with 3mol% of yttria (TZ3YE and TZ3YS, labeled as ZE and ZS, respectively) supplied by Tosoh (Japan) were used for this study. Maximum colloidal stability for ZE was achieved by dispersing the powders in a mixture of water/ethanol of 90:10 (wt/wt) using a sonication probe. The rheological behavior of the suspensions was optimized in terms of solids content ranging from 20 to 33vol% and sonication time (06min), the best results being obtained after 2min. ZS samples were prepared to a solids loading of 30vol% in water dispersing with 2min-sonication. Samples obtained by slip casting in plaster molds were used for dynamic sintering studies, and fully dense and nanostructured specimens were obtained at temperatures of 1300 degrees C1350 degrees C (ZE samples) and 1400 degrees C per 2h (ZS samples). The Hardness (H) and Young's Modulus (E) properties of the specimens were studied by nanoindentation technique giving 17 and 250GPa mean values for H and E, respectively. The specimens were then forced to a low-temperature degradation (LTD) treatment at 130 degrees C for 240h in steps of 60h. Raman spectroscopy and nanoindentation results of hydrothermally treated samples showed the absence of transformation from tetragonal to monoclinic phase until 180h whereas the mechanical properties maintained constant even at the sample surface. After 240h of LTD, the monoclinic phase was detected on all specimens by Raman peaks centered at 180, 191, and 383cm1. The nanoindentation study revealed an important loss of mechanical features reaching 10 and 175GPa for H and E, respectively. In the case of the ZS specimens, no monoclinic phase is detected after 240h of LTD treatment and no decay of E or H is detected. The free defect microstructure reached for the ZS specimen revealed a higher hydrothermal resistance so that it is concluded that the excellent behavior against thermal degradation is possible due to the large uniformity obtained by colloidal processing rather than the particle size of the starting powders., This work has been supported by Spanish Ministry of Science and Innovation (Projects MAT2009-14144-C03-02, MAT2009-14369-C02-01, and MAT2008-03398). Authors thank Prof. M. Anglada for helpful comments and discussion. R Moreno thanks the Universidad Politecnica de Valencia for the concession of a grant in the frame of its Program of Support to R+D (PAID-02-11, R-1752). We also wish to acknowledge Rut Benavente for her excellent technical support.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Dense nanostructured zirconia compacts obtained by colloidal filtration of binary mixtures

  • Benavente Martínez, Rut|||0000-0002-4566-9475
  • Salvador Moya, Mª Dolores|||0000-0002-4242-478X
  • Alcázar, M.C.
  • Moreno, R.
As starting materials two commercial nanosized zirconias doped with 3 mol% of Y 2O 3 were used: a powder of about 100 nm (TZ3YE, Tosoh, Japan) and a colloidal suspension of about 15 nm (Mel Chemicals, UK). Colloidal stability in water was studied for both zirconias in terms of zeta potential as a function of deflocculant concentration and pH. Concentrated suspensions were prepared by dispersing the powder in the colloidal suspension to solids loadings ranging from 5 to 30 vol.% using a sonication probe to achieve dispersion. The rheological behavior was optimized in terms of solids content, deflocculant content and sonication time. Optimized suspensions with up to 25 vol.% solids showed a nearly Newtonian behavior and extremely low viscosities and maintain stable for long times (days) which is an important drawback of conventional nanoparticle suspensions. Samples obtained by slip casting in plaster moulds were used for dynamic sintering studies and dense, nanostructured specimens were obtained at temperatures of 1300-1400°C., This work has been supported by Spanish Ministry of Science and Innovation (Projects MAT2009-14144-C03-02 and MAT2009-14369-C02-01). R. Moreno thanks to Universidad Politecnica de Valencia for the concession of a grant in the frame of its Programme of Support to R + D (PAID-02-11, R-1752).