Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 3
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

High performance N-doped carbon nanosheet/MnO2 cathode derived from bacterial cellulose for aqueous Zn-ion batteries

  • Wang, Wenhai
  • Black, Ashley P.
  • Liu, Cheng
  • Martin-Diaconescu, Vlad
  • Simonelli, Laura
  • Tonti, Dino
Rechargeable aqueous Zn-ion batteries (ZIBs) have obtained extensive attention owing to their high safety, low-cost, environmental friendliness and high energy density. Nevertheless, developing suitable cathode materials remains challenging due to requirements for appropriate microstructure. We present a porous N-doped carbon nanosheet/MnO2 (NCS/MnO2) derived from bacterial cellulose (BC) by a simple route. BC chunks were soaked in urea solution and then carbonized under Ar flow at 900 °C. N-doped carbon nanosheets were obtained and MnO2 was added by reaction with NaMnO4. Benefiting from both the conductivity and porosity of the NCS support, the NCS/MnO2 composite delivers a high capacity and long cycling stability (114 mA h g−1 at 2 A g−1 after 1800 cycles). The electrode reaction mechanism was further investigated and the MnO2 dissolution/deposition mechanism was confirmed, with a critical role of zinc sulfate hydroxide (ZSH) to assist the deposition of MnO2, This research was funded by the Spanish Agency for Research (AEI) with ERDF cofunding, through the “Severo Ochoa” Programme for Centers of Excellence in R&D (FUNFUTURE, CEX2019-000917-S), the projects RTI2018-096273-B-I00, PID2021-124681OB-I00, and TED2021-132707B-I00. This research has been partially developed within the CSIC Interdisciplinary Thematic Platform (PTI+) Transici´on Energ´etica Sostenible+ (PTI-TRANSENER+) as part of the CSIC program for the Spanish Recovery, Transformation and Resilience Plan funded by the Recovery and Resilience Facility of the European Union, established by the Regulation (EU) 2020/2094. W. W. and C. L. are grateful for the support from the China Scholarship Council (CSC No.: 201808340076 and 202106370079). This work has been performed within the framework of the doctoral program in materials science of UAB (W. W. and C. L.). XAS experiments were performed at CLAESS beamline of ALBA Synchrotron with the collaboration of ALBA staff., With funding from the Spanish government through the ‘Severo Ochoa Centre of Excellence’ accreditation (CEX2019-000917-S)., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Unveiling capacity limitations of MnO2 in rechargeable Zn chemistry

  • Liu, Cheng
  • Martin-Diaconescu, Vlad
  • Black, Ashley P.
  • Khabazian, Siavash
  • Mundet, Bernat
  • Matlak, Krzysztof
  • Stievano, Lorenzo
  • Sorrentino, Andrea
  • Simonelli, Laura
  • Tonti, Dino
Aqueous Zn–MnO2 batteries with mildly acidic electrolytes deliver attractive experimental capacities, however the underlying mechanisms remain elusive, particularly regarding the interactions of Zn2+ and H+ with MnO2, as well as the formation of Mn2+ and Zn4SO4(OH)6·xH2O (ZSH). Although these products are compatible with a two-electron dissolution mechanism, the observed first-discharge capacity is limited to approximately 300 mA h g−1 MnO2, close to that of a one-electron reaction. To address this contradiction, commonly used α-MnO2 nanowires were chosen as cathode material and investigated by a systematic multimodal and multiscale approach under operando or ex situ conditions to analyze the processes that occur during the first discharge. MnO2 dissolution into Mn2+ and ZSH precipitation were confirmed, and the formation of a disordered phase at the nanowire surface with the accumulation of Mn(III) was detected. An in-depth analysis indicates that such Mn(III) species correspond to protonated corner-sharing MnO2 octahedra, which, unlike the edge-sharing ones, are hindered from undergoing disproportion, limiting the MnO2 dissolution and explaining the reduced capacity. This comprehensive mechanistic understanding opens new pathways for the selection of the most appropriate MnO2 phases and the optimization of electrodes to improve the performance of aqueous Zn–MnO2 battery systems., Cheng Liu is very grateful for financial support from the China Scholarship Council (CSC no.: 202106370079). This study was also implemented within the framework of the doctoral program in Materials Science at the Universitat Autònoma de Barcelona (UAB, Spain). This research was funded by the Spanish Agency for Research (AEI) co-funded with ERDF through the “Severo Ochoa” Programme for Centers of Excellence in R&D (CEX2023-001263-S) and the projects PID2021-124681OB-I00 and TED2021-132707B-I00. This research was partially developed within the CSIC Interdisciplinary Thematic Platform PTI-TRANSENER+ as part of the CSIC programme for the Spanish Recovery, Transformation, and Resilience Plan funded by the Recovery and Resilience Facility of the European Union, established by Regulation (EU) 2020/2094. Coding support for Hyperspy, eXSpy, and SpectroChemPy from the respective communities and, in particular, assistance from licouplings@gmail.com and yezhihang@live.com is warmly acknowledged. Material suggestions and synthesis help from Wenhai Wang and Canhuang Li are warmly appreciated. We thank Anna Esther Carrillo, and Judith Oró Solé in the Service at the ICMAB for arrangements of SEM and TEM sessions. Synchrotron-based measurements were performed at CLÆSS and MISTRAL, of ALBA CELLS Synchrotron with the collaboration of ALBA staff. Authors acknowledge the use of instrumentation, as well as the technical advice provided by the Joint Electron Microscopy Center at ALBA (JEMCA) and funding from Grant IU16-014206 (METCAM–FIB) to ICN2 funded by the European Union through the European Regional Development Fund (ERDF), with the support of the Ministry of Research and Universities, Generalitat de Catalunya. This publication was partially developed under the provision of the Polish Ministry of Science and Higher Education project “Support for research and development with the use of research infra-structure of the National Synchrotron Radiation Centre SOLARIS” under contract no 1/SOL/2021/2. Lorenzo Stievano gratefully acknowledges financial support from the French National Research Agency (project Labex STORE-EX, ANR-10-LABX-76-01)., With funding from the Spanish government through the ‘Severo Ochoa Centre of Excellence’ accreditation (CEX2023-001263-S)., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

Dataset for TED2021 AEI Project: Green chemistry for a membrane-free electrolitic flow battery for large scale energy storage (GreenFloBat)

  • Khabazian, Siavash
  • Liu, Cheng
  • Gao, Yan
  • Vallejo, Victor
  • Martin Diaconescu, Vlad
  • Stievano, Lorenzo
  • Tonti, Dino
Fecha de finalización del proyecto: 2025-08-31 This dataset contains the experimental and computational data generated during the TED2021 project TED2021-132707B-I00 Metodología detallada: ¿Cómo se generaron los datos, incluidos los equipos o el software utilizado, el protocolo experimental, etc? For XAS measurements, the synchrotron radiation emitted by a wiggler source was monochromatized using a double-crystal Si(311) monochromator with an appropriate beam size of 1 mm × 1 mm. Higher harmonics were rejected by choosing the proper angles and coatings for the collimating and focusing mirrors. The absorption data of the Mn and Zn references were collected in transmission mode using three ionization chambers for simultaneous measurements of the sample and the Mn foil used as a reference, within an incoming energy resolution below 0.3 eV. For XES experiments, the incoming beam was monochromatized using a double-crystal Si(311) monochromator and the emission data were collected in back scattering geometry with a beam size of 0.2 mm × 0.1 mm, (parallel to the linear polarization vector of the incoming X-ray beam) by means of the CLEAR emission spectrometer. The spectrometer was based on a dynamically bent diced Si(333) crystal analyzer (bending radius R = 1 m) and a 1D position-sensitive Mythen detector. The emission spectra were acquired by exciting the sample well above the Mn K edge and detecting the emitted Mn Kβ1,3 emission lines, with a total energy resolution of approximately 0.6 eV. Repeated X-ray absorption and emission scans were measured to ensure the reproducibility of the spectra and obtain a high signal-to-noise ratio. The measurements were performed at ambient temperature under vacuum conditions. Operando XAS was operated with a similar configuration to the operando cell in Fig. S1, but the cathode was moved from the center to partly expose the separator, as shown in Fig. 2c, where both Zn and Mn K-edge XAS data were acquired synchronously in both the electrolyte and electrode, respectively. The cell was filled with ca. 60 μL 0.5 M ZnSO4 and 0.2 M MnSO4 electrolyte and operated under a C/10 rate and with a low voltage cut-off of 0.9 V vs. Zn/Zn2+, after being maintained for one hour at Open Circle Voltage (OCV) state. The duration of data acquisition was approximately 30 minutes per batch, including a total of 10 spectra (Zn and Mn spectra in both the electrolyte and cathode), along with a short resting time. In situ STXM. 2 μL of a 20 ppm (w/w) suspension of α-MnO2 in H2O was dropped onto a MEMS chip (HUMMINGBIRD). The chip was then mounted on its flow-cell microscope holder, introduced into the STXM chamber, and connected to a BioLogic SP200 potentiostat. The electrolyte (1 M ZnSO4 and 0.2 M MnSO4) was injected from a 1 mL syringe at a speed of 0.2 mL per hour. During cycling, an energy of 1010 eV near the Zn L-edge was selected to acquire the STXM images to provide an optimal image contrast. Galvanostatic cycling tests were conducted using a LANHE M340A cycler. Remaining electrochemical tests were conducted using a BioLogic VSP potentiostat. X-ray Diffraction (XRD) patterns were collected by a Siemens D-5000 diffractometer of Cu K𝛼 radiation. Operando XRD data were acquired by a Bruker D8 Advance A25 diffractometer in a Debye-Scherrer geometry equipped with a Johansson monochromator of the Mo K𝛼 radiation and its standard transmission diffraction collection mode. Scanning Electron Microscopy (SEM) was performed using a FEI Quanta 200 FEG-ESEM equipment (10 – 15 kV). X-Ray Photoelectron Spectroscopy (XPS) data were recorded by a SPECS EA10P hemispherical analyzer with a monochromatic Al K𝛼 radiation. (Scanning) Transmission Electron Microscopy ((S)TEM) and Transmission Electron Microscopy-Energy Dispersive X-Ray (TEM–EDX) and Scanning Transmission Electron Microscopy–Electron Energy Loss Spectroscopy (STEM–EELS) were acquired with a Super-X EDX spectrometer and a Gatan Continuum K3 EELS spectrometer, or a ThermoFisher Scientific Spectra 300. Spectra were collected at a beam energy of 200 keV with an energy step of 0.9 eV. Mn K-edge X-ray Absorption Spectroscopy (XAS) was carried out at the CLÆSS beamline of ALBA CELLS synchrotron, Spain. Ex situ energy-resolved full-field soft X-ray Transmission Microscopy (TXM) was performed at the MISTRAL beamline of ALBA CELLS Synchrotron, Spain.84 In situ Scanning X-ray Transmission Microscopy (STXM) was carried out at the DEMETER beamline of SOLARIS Synchrotron, Poland. The STXM images were obtained at the energy of ca. 1010 eV to optimize the compromise between contrast and radiation damage. XPS fitting was carried out with CasaXPS for Mn 2p3/2, K 2p, and O 1s lines following the procedure described in our previous report.56 For XAS techniques, the Zn and Mn mole evolutions in the electrode and electrolyte of the operando cell were calculated from the X-ray Absorption Near Edge Structure (XANES) edge jumps with a self-built model detailed in the Supporting Information. The EXAFS portion of the operando XAS data was analyzed using ATHENA and ARTEMIS. For the fitting of the pre-edge, the baseline was modeled with the Larch package. The MnO2 and Mn2O3 reference spectra were taken as models of Mn(IV) and Mn(III) components, respectively, using the Hyperspy package. For XES measurements, a linear background was subtracted in SpectroChemPy,93 considering 0.5 – 2 eV of the low- and high-energy tails. Subsequently, each spectrum was normalized to its area. The Integrated Absolute Difference (IAD) with respect to a low-spin reference method was utilized to extract the local magnetic moment quantitatively. The ex situ TXM data were processed following previous work. In situ STXM images and Mn spectra were obtained in aXis2000.99 (S)TEM-related dataset (HRTEM, STEM–HAADF images, TEM–EDX, and STEM–EELS) were treated with eXSpy., Affordable Zn and safe aqueous electrolytes make Zn/MnO₂ batteries promising, but common test conditions hide reversibility issues. Recent work shows Mn(IV) can reduce to Mn(II) in flow cells, and Zn/MnO₂ can be deposited during charging from Zn²⁺/Mn²⁺ solutions, achieving high energy density without ion-selective membranes—cutting cost and risk. The mechanism is complex and poorly understood, involving intercalation, precipitation, and dissolution driven by pH, plus side reactions like corrosion and Zn dendrites. We propose advanced techniques (e.g., X-ray absorption) to identify chemical species and compare main vs. undesired processes under varying electrode designs, additives, and conditions. This will guide development of sustainable, low-cost, scalable Zn-MnO₂ flow batteries., Proyecto TED2021-132707B-I00 financiado por AEI/MCIN, - /data/raw: Original unprocessed data - /data/processed: Derived results - /code: Scripts used for analysis and for simulations - /other: Supplementary files, No