Recycling Spent Fluorescent Lamp Glass Waste in Calcium Aluminate Cement: Effects on Hydration and Mechanical Performance

  • Reig, Lucia
  • Pitarch, Angel M.
  • Gallardo, Antonio
  • Soriano Martinez, Lourdes|||0000-0002-5749-4609
  • Borrachero Rosado, María Victoria|||0000-0002-7873-0658
  • Paya Bernabeu, Jorge Juan|||0000-0001-7425-5311
  • Monzó Balbuena, José Mª|||0000-0002-3657-3076
[EN] Featured Application; This study presents a novel application of spent fluorescent lamp glass (SFLG) waste as a partial replacement for calcium aluminate cement (CAC), offering a sustainable solution for hazardous waste reuse and reducing CAC's environmental impact. Mortars with 25-50 wt.% SFLG showed enhanced long-term strength due to stratlingite formation, which limited harmful phase conversion. Residual mercury in SFLG was safely encapsulated, ensuring environmentally safe waste management.; Calcium aluminate cement (CAC) offers rapid strength development, chemical durability in harsh environments, and high-temperature resistance, but its long-term performance may be compromised by the conversion of metastable hexagonal hydrates into stable cubic phases. Concurrently, recycling spent fluorescent lamp glass (SFLG) is limited because of its residual mercury content. This study investigates the use of manually (MAN) and mechanically (MEC) processed SFLG as partial CAC replacements (up to 50 wt.%). Both SFLG types had irregular morphologies with mean particle sizes of similar to 20 mu m and mercury concentrations of 3140 +/- 61 ppb (MAN) and 2133 +/- 119 ppb (MEC). Moreover, the addition of SFLG reduced the initial and final setting times, whilst MEC waste notably extended the plastic state duration from 20 min (reference) to 69 min (50 wt.% MEC). Furthermore, strength development was accelerated, with SFLG/CAC mortars reaching peak strengths at 7-10 days versus 28 days as in the CAC reference. CAC and 15 wt.% SFLG mortars showed strength loss over time by reason of their phase conversion, whereas mortars with 25-50 wt.% SFLG experienced significant long-term strength gains, reaching similar to 60 MPa (25 wt.%) and similar to 45 MPa (35 wt.%), respectively, after 365 days, with strength activity indexes (SAI) near 90% and 70%, respectively. These improvements are attributed to the formation of stratlingite (C(2)ASH(8)), which stabilized hexagonal CAH(10) and mitigated conversion to cubic katoite (C(3)AH(6)). Mercury leaching remained below 0.01 mg/kg dry matter for all mixes and curing ages, classifying the mortars as non-hazardous and inert under Spanish Royal Decree 646/2020. The results suggest that SFLG can be safely reused as a sustainable admixture in CAC systems, enhancing long-term mechanical performance while minimizing environmental impact., The authors are grateful to the Universitat Jaume I of Castellon for supporting this study through Project UJI-B2019-21.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Reutilisation of hazardous spent fluorescent lamps glass waste as supplementary cementitious material

  • Pitarch, A.M.
  • Reig, L.
  • Gallardo, A.
  • Rochina, S.
  • Soriano Martinez, Lourdes|||0000-0002-5749-4609
  • Borrachero Rosado, María Victoria|||0000-0002-7873-0658
[EN] Spent fluorescent lamps glass (SFLG) waste, manually and mechanically processed in a lamps waste treatment plant, was used to partially replace up to 50 wt% Portland cement (PC). Both waste types exhibited similar pozzolanic activity. The mortars containing up to 35 wt% SFLG met the specifications for other pozzolanic materials (e.g. fly ash) and, after 90 curing days, their compressive strength values were sim- ilar to or higher than those of the 100% PC sample (58.8 MPa). Our results provide an alternative reutilization process for this hazardous waste to reuse SFLG as-received (no washing to reduce mercury) and contributes to less PC use, This work was supported by the Universitat Jaume I of Castellon [Project UJI-B2019-21], and the Spanish Ministry of Education, Culture and Sport [research collaboration grant, academic year 2015/2016].