Publicación Artículo científico (JournalArticle)

Optimizing tribocorrosion, corrosion and mechanical performance of Ti Nb Sn shape memory alloys with low elastic modulus for biomedical implants

  • Pérez-González, Clara
  • García-Hernández, Celia
  • Martin-Pedrosa, Fernando
  • Garcia-Cabezón, Cristina
  • Amigó, Vicente|||0000-0002-2107-0273
[EN] Ti and Ti¿6Al¿4V are widely used in biomedical devices because of their strength, corrosion resistance, and biocompatibility. However, Ti alloys suffer from a high elastic modulus that can cause stress-shielding and bone resorption, plus potential cytotoxicity from Al and V ions under tribocorrosion. To address these issues, ß-type Ti alloys stabilized with niobium (Nb) have been proposed. In particular, Ti¿Nb¿Sn alloys are promising because Sn enhances microstructural uniformity, suppresses brittle phases, and stabilizes protective passive films. This work evaluates several Ti¿Nb¿Sn compositions made by powder metallurgy under identical processing and testing conditions to find optimal formulations for orthopedic and dental implant purposes. Four alloys (Ti-30Nb, Ti-30Nb-2Sn, Ti-30Nb-4Sn, and Ti-35Nb-4Sn) were characterized. The Ti-35Nb-4Sn composition exhibited the highest density and lowest porosity. Increasing Sn (and Nb to 35%) reduced the lamellar ¿-phase fraction and increased ß-phase content, as shown by XRD and microscopy. Hardness (macro and micro) decreased with more Sn and Nb, but the elastic modulus dropped dramatically from around 78 GPa in Ti-30Nb to about 42 GPa in Ti-35Nb-4Sn, nearing cortical bone stiffness. In electrochemical tests in artificial saliva, 4Sn alloys had more noble open circuit potentials, lower corrosion currents, and higher polarization resistance. Wear and tribocorrosion tests revealed that Ti-30Nb-4Sn had the lowest wear rate and mass loss, while Ti-35Nb-4Sn suffered greater material loss. Finally, after 60 days of immersion, all alloys developed more stable passive layers, and ion release of Ti, Nb, and Sn remained under 0.10 mg/L, suggesting low toxicity., This work was supported by Junta de Castilla y Leon- FEDER VA117P24 and CLU-2019-04 BIOECOUVA Unit of Excellence and by Ministerio de Ciencia Innovacion y Universidades -FEDER Plan Estatal (PID2021-122365OB-100) .