Supplementary material for Electrochemically-assisted leaching of active cathode materials from spent batteries with minimal pre-treatment using hydroxylated solvents [Dataset]

  • Bastos, Henrique
  • Schaeffer, Nicolas
  • Pringle, Jennifer M.
  • Eftekharnia, Mojtaba
  • Coutinho, João A. P.
  • Pozo Gonzalo, Cristina
Under a Creative Commons license BY 4.0., EXPERIMENTAl: Figure S1. Dismantled Li-metal | NMC622 pouch cells, with the 6 layers of Li-metal anode and 5 layers of NMC622 cathode, intercalated by each other in the top layer, directly after dismantling from right to left. LITERATURE DATA: Table S1. Ecotoxicity, toxicity and cost parameters of the hydroxylated solvents studied in this work. RESULTS: Figure S2. Leaching efficiency (%) obtained through electrochemically-assisted leaching of Co3O4 in 0.5 M HCl in EG, 0.5 M HCl in 25 % (v/v) Gly in water, and EG, for 24 h at 40 °C. Figure S3. UV-Vis spectra after electrochemically-assisted leaching of Co3O4 in 0.5 M HCl in EG for 24 h at 40 °C, at potentials between -0.75 V and 6 V. Figure S4. Resulting leachates after electrochemically-assisted leaching of Co3O4 in 0.5 M HCl in EG for 24 h at 40 °C, at either 5 V or 6 V of constant potential. Figure S5. Raman spectra of 0.5 M HCl in EG electrolyte and resulting leachates after electrochemically-assisted leaching (EL) of Co3O4 in 0.5 M HCl in EG for 24 h at 40 °C at 6 V. Figure S6. 1H-NMR (top) and 13C-NMR (bottom) spectra after chemical leaching (CL) or electrochemically-assisted (EL) leaching of Co3O4 in 0.5 M HCl in EG for 24 h at 40 °C, at either 4 V, 5 V or 6 V of constant potential. Figure S7. Resulting leachates immediately after carrying out the chemical dissolution of NMC622 precursor powder, pristine cathode with NMC622 active material coated with binder on the Al foil current collector and the resulting spent cathode after dismantling the cycled pouch cell. Table S2. Extraction efficiency of Li (%) determined by ICP-MS after electrochemically-assisted leaching of a spent NMC622 cathode in either 0.5 M HCl in 25 % (v/v) Gly in water or 0.5 M HCl in EG for 3 h at 40 °C with a constant potential of 1 V or 2 V. Figure S8. Separation of the spent NMC622 cathode into two layers during the electrochemically-assisted leaching process in 0.5 M HCl in 25 % (v/v) Gly in water for 3 h at 40 °C.Figure S9. Leaching efficiency of Al (%) from electrochemically-assisted leaching of NMC622 spent cathode after applying 1.0 V, 2.0 V or 2.5 V vs Ag/AgNO3 for 3 hours at 40°C, with aliquots collected at 15 min., 30 min., 1 h, 2 h and 3 h. Table S3. Parameters of the kinetics model based on the shrinking core model, logarithmic rate and mixed kinetics equation fittings,2-4 for Co, Ni and Mn after electrochemically-assisted leaching of a spent NMC622 cathode in 0.5 M HCl in 25 % (v/v) Gly in water for 3 h at 40 °C with a constant potential of 1.0 V, 2.0 V or 2.5 V. Figure S10. X-ray diffractograms of the NMC622 cathode material measured before assembly into the pouch cell (pristine electrode), after disassembly of the pouch cell (spent electrode) and after EL for 3 hours at 40 °C at either 1.0 V, 2.0 V or 2.5 V, focusing on the displacement of the a) (003); b) (101), (006) and (102); and c) (108) and (110) peaks. DISCUSSION: Coordination of Co ions by EG based on the Raman spectra from Figure S5., This work was partly developed within the scope of the project CICECO-Aveiro Institute of Materials, UIDB/50011/2020, UIDP/50011/2020, and LA/P/0006/2020, financed by national funds through the FCT/MCTES. H. Bastos acknowledges the financial support from Deakin University (DUPR Scholarship 0000038986). The authors acknowledge the Australian Research Council (ARC) Training Centre for Future Energy Storage Technologies (storEnergy) (IC180100049) for funding. Financial support from EU (IONBIKE 2.0 MSCA-SE grant agreement No 101129945) is also acknowledged., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Research data Set de datos (Dataset)

Supplementary files for Understanding the impact of additives on cobalt leaching efficiency using a citric acid-based deep eutectic solvent [Dataset]

  • Perera, Isuri N.
  • Pringle, Jennifer M.
  • O'Dell, Luke A.
  • Siriwardana, Amal
  • Pozo Gonzalo, Cristina
Under a Creative Commons BY-NC 3.0 license., Figure S1: FTIR spectra of neat CA:ChCl:EG (1:1:1.1), neat CA:ChCl:EG (1:1:4), leachate from Co3O4 using CA:ChCl:EG (1:1:1.1) and leachate from Co3O4 using CA:ChCl:EG (1:1:4).; FTIR analysis: Table S1: Molar ratio of the components present in the solution relative to Co, Figure S2: Variation of Co leaching efficiency from Co3O4 using CA:ChCl:EG (1:1:1.1) with time (72 h), 700 rpm stirring rate and 1:5 S:L ratio. Figure S3: Cyclic voltammograms corresponding to Co2+ in the leachates from (a) Co3O4 and (b) LiCoO2 and the neat CA:ChCl:EG (1:1:1.1) using GC working electrode. Scan rate: 50 mVs-1 and temperature: 60 °C. Insets: magnification of the cyclic voltammogram starting in the positive direction; H NMR analysis: Figure S4: EDX map spectra of electrodeposit resulting from the Co3O4 leachate using CA:ChCl:EG (1:1:1.1) (a) site 1 and (b) site 2. EDX map spectra of (c) Ni foil., This research was supported by the Australian Research Council Training Centre for Future Energy Storage Technologies (grant agreement No IC180100049) and funded by the Australian Government. I. N. Perera acknowledges the financial support from Deakin University (DUPR Scholarship). C.P.G. gratefully acknowledges the financial support from EU (IONBIKE 2.0 MSCA-SE, grant agreement No 101129945)., Peer reviewed