Skip to main content

CARATERIZACION AVANZADA DE ECOCEMENTOS SOSTENIBLES: ENTENDER MEJOR LA HIDRATACION PARA MEJORAR SUS PROPIEDADES.

BIA2017-82391-R

•
Funding agency name Agencia Estatal de Investigación
Funding agency acronym AEI
Program Programa Estatal de I+D+i Orientado a los Retos de la Sociedad
Call Proyectos I+D+i Retos de Investigación
Call year 2017
State Plan 2017-2020 Plan Estatal de Investigación Científica y Técnica y de Innovación
Beneficiary centre UNIVERSIDAD DE MALAGA

Resultados relacionados

Resultados totales (Incluyendo duplicados): 2
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Belite cements and their activation

  • Cuesta, Ana
  • Ayuela, Andrés
  • Aranda, Miguel A.
Belite cements, BCs, containing mainly belite, alite and calcium aluminates, are currently used as low heat cements. These binders produce high amounts of C–S–H gel and have very good durability properties which are reviewed. Additional advantages include: (i) lower limestone demand, with lower associated CO2 emissions; (ii) lower energy demand; (iii) lower kiln operating temperature, which means lowering CO2 and NOx emissions from fuel burning; and (iv) lower temperature increase at early hydration age. However, early-age strength developments are not competitive with those of Portland cements. Hence, to improve their early-age strength developments is a research priority known as activation. This enhancement can be attained by three compatible approaches: (i) chemical, (ii) physical; and (iii) admixture activations. The current research status for BCs activation is reviewed including: cost-effective element substitutions to stabilize high-temperature forms; fast cooling, milling and mild temperature hydration as physical activation; and the use of C–S–H seeds as admixture activation. After discussion of the resulting microstructures, a research outlook is exercised., The work in Malaga has been supported by BIA2017-82391-R research grant, which is co-funded by FEDER. The work in San Sebastián was supported by PID2019-105488GB-I00 research grant, the Gobierno Vasco UPV/EHU (Project No. IT-1246-19), and the EIG CONCERT-Japan 5th Joint Call on Functional Porous Materials (Project No. PCI2019-103657-POROPCM)., Peer reviewed
Dipòsit Digital de Documents de la UAB
Publication Artículo científico (JournalArticle)

Rietveld quantitative phase analysis of oil well cement, in situ hydration study at 150 bars and 150 °C

  • Fraga, Edmundo|||0000-0003-4335-4995
  • Cuesta, Ana|||0000-0002-8634-2241
  • Zea-Garcia, Jesus D.|||0000-0001-9469-7117
  • Gómez De la Torre, Angeles|||0000-0001-5481-7268
  • Yáñez Casal, Armando|||0000-0003-4626-7993
  • Aranda, Miguel A. G.|||0000-0001-7708-3578
Oil and gas well cements are multimineral materials that hydrate under high pressure and temperature. Their overall reactivity at early ages is studied by a number of techniques including through the use of the consistometer. However, for a proper understanding of the performance of these cements in the field, the reactivity of every component, in real-world conditions, must be analysed. To date, in situ high energy synchrotron powder diffraction studies of hydrating oil well cement pastes have been carried out, but the quality of the data was not appropriated for Rietveld quantitative phase analyses. Therefore, the phase reactivities were followed by the inspection of the evolution of non-overlapped diffraction peaks. Very recently, we have developed a new cell specially designed to rotate under high pressure and temperature. Here, this spinning capillary cell is used for in situ studies of the hydration of a commercial oil well a cement paste at 150 bars and 150 °C. The powder diffraction data were analysed by the Rietveld method to quantitatively determine the reactivities of each component phase. The reaction degree of alite was 90% after 7 hours, and that of belite was 42% at 14 hours. These analyses are accurate, as the in situ measured crystalline portlandite content at the end of the experiment, 12.9 wt%, compares relatively well with the value determined ex situ by thermal analysis, i.e., 14.0 wt%. The crystalline calcium silicates forming at 150 bars and 150 °C are also discussed.