Skip to main content

SONDAS NANOMETRICAS MULTIFUNCIONALES PARA LA FORMACION DE IMAGENES BIOMEDICAS

MAT2012-34919

•
Funding agency name Ministerio de Economía y Competitividad
Funding agency acronym MINECO
Program Programa Nacional de Proyectos de Investigación Fundamental
Subprogram Subprograma de Proyectos de Investigación Fundamental no Orientada
Call Proyectos I+D
Call year 2012
State Plan 2008-2011 Plan Nacional de Investigación Científica, Desarrollo e Innovación Tecnológica
Management unit Secretaría de Estado de Investigación, Desarrollo e Innovación
Beneficiary centre UNIVERSIDAD AUTONOMA DE MADRID

Resultados relacionados

Resultados totales (Incluyendo duplicados): 1
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Crystal structure and luminescent properties of Eu3+-doped A-La2Si2O7 tetragonal phase stabilized by spray pyrolysis synthesis

  • Fernández-Carrión, Alberto J.
  • Ocaña, Manuel
  • Florian, Pierre
  • García-Sevillano, J.
  • Cantelar, Eugenio
  • Fitch, Andrew N.
  • Suchomel, Matthew R.
  • Becerro, Ana Isabel
Pure A-La2Si2O7 powder has been synthesized through a spray pyrolysis method followed by calcination at 1100 ºC for 15 h. The crystallographic structure, refined from the synchrotron powder diffraction pattern of the sample, showed tetragonal symmetry with space group P41, a= 6.83568(1) Å and c = 24.84160(3) Å. The 29Si and 139La NMR spectra have been described here for the first time in the literature and could be simulated with four Si and four La resonances, respectively, in good agreement with the presence of 4 Si and 4 La crystallographic sites in the unit cell. The same synthesis method was successful for the synthesis of Eu3+-doped A-La2Si2O7 (% Eu= 3 to 40). The analysis of the unit cell volumes indicated that Eu3+ replaces La3+ in the unit cell for all Eu3+ substitution levels investigated. However, anomalous diffraction data indicated that the La/Eu substitution mechanism was not homogeneous but Eu much prefers to occupy the RE3 sites. The Eu-doped A-La2Si2O7 phosphors thus synthesized exhibited a strong orange-red luminescence after excitation at 393 nm. Life time measurements indicated that the optimum phosphor was that with an Eu3+ content of 20%, which showed a life time of 2.3 ms. The quantum yield (QY) of the latter was found to be 12 % at 393 nm excitation. These experimental observations together with the high purity of the phase obtained by the proposed spray pyrolysis method make this material an excellent phosphor for optoelectronic applications., A.J.F.-C. gratefully acknowledges an F.P.D.I. grant from Junta de Andalucía and J.G.-S. an F.P.I. grant from MICINN. Supported by DGICYT (Project No. CTQ2010-14874/BQU), MEC (Project. MAT2012-34919), and Junta de Andalucía (JA FQM 06090). Use of the Advanced Photon Source at Argonne National Laboratory was supported by the U.S. Department of Energy, Office of Science, Office of Basic Energy Sciences, under Contract No. DE-AC02-06CH11357., Peer reviewed