Skip to main content

GREENER PERMANENT MAGNETS WITHOUT OR WITH LESS CRITICAL RAW MATERIALS

PCI2024-153493

•
Funding agency name Agencia Estatal de Investigación
Funding agency acronym AEI
Program Programa Estatal para Afrontar las Prioridades de Nuestro Entorno
Subprogram Subprograma Estatal de Internacionalización
Call Proyectos Programación Conjunta Internacional
Call year 2024
State Plan 2021-2023 Plan Estatal de Investigación Científica y Técnica y de Innovación
Beneficiary centre AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 2
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Recovery of Rare Earths from End-of-Life NdFeB Permanent Magnets from Wind Turbines

  • Alcaraz, Lorena
  • Rodríguez-Largo, Olga
  • Barquero-Carmona, Gorka
  • Berja, Alba
  • Quesada, Adrián
  • López, Félix A.
This work aims to recover rare earths from wind turbines NdFeB magnets through pyrometallurgical and hydrometallurgical techniques. First, a NdFeB hydride powder is obtained by decrepitation with hydrogen. Subsequently, this powder was subjected to a chlorination roasting process and successive leaching with water to bring the metals into solution. This was followed by a liquid-liquid extraction to remove the iron and purify the rare earth solution. For this purpose, Aliquat 336 diluted in Solvesso was selected as the iron selective extraction agent. As a single extraction was not enough for complete iron removal, a second Fe extraction step was carried out. This second extraction step was performed using the restored organic phase. This restoration was achieved by treating the organic phase with Na<inf>2</inf>SO<inf>3</inf> and then washing it with a 3 M HCl solution. In this way, the process was achieved more sustainably. Finally, the rare earths contained in the final solution were precipitated using oxalic acid to obtain mixed rare earth oxalates. © 2025 Elsevier B.V., All rights reserved., We acknowledge funding from the EIT Raw Materials, co-funded by the European Commission, through Project INSPIRES (20090), from the European Commission through Horizon Europe project BEETHOVEN (101129912) and from the Spanish Ministerio de Ciencia, Innovación y Universidades through projects PID2021-124585NB−C33, PCI2024-153493, TED2021-130957B−C51, CNS2022-135876 and by “ERDF A way of making Europe”. Funded by the European Union. Views and opinions expressed are however those of the author(s) only and do not necessarily reflect those of the European Union or HADEA. Neither the European Union nor the HADEA can be held responsible for them., this journal provides supporting information supplied by the authors. Such materials are peer reviewed and may be re-organized for online delivery, but are not copy-edited or typeset. Technical support issues arising from supporting information (other than missing files) should be addressed to the authors at DOI: 10.1002/cssc.202402237, Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Efficient recycling of End-of-Life ceramic ferrite hard magnets into new permanent ceramic magnets

  • Berja, Alba
  • Granados-Miralles, Cecilia
  • Casaleiz, Daniel
  • Guzmán-Mínguez, J. C.
  • Frangez, Tina
  • Fernández Lozano, José Francisco
  • Quesada, Adrián
Within current sustainable and circular economy approaches, recycling hexaferrite magnets has emerged as a strategic alternative to rare-earth-based magnets. This study proposes an efficient recycling and fabrication protocol for sintered ferrite magnets by merging annealing and sintering into a single step, reducing energy consumption and emissions. Rietveld analysis revealed temperature-dependent variations in ferrite and hematite fractions, with reduced hematite content at a sintering temperature of 1250°C. Magnetic characterization indicated decreasing coercive field, H <inf> c </inf>, and remanent magnetization, M <inf> r </inf>, with increasing sintering temperature, while a density of 93 % was achieved at 1250°C for 30 min. X-ray diffraction, FE-SEM, and particle size analysis confirmed that the reduced magnetic properties of recycled magnets, compared to commercial counterparts, are due to hematite formation and sintering-induced grain growth. These findings highlight the importance of thermal optimization to balance densification and magnetic performance. This work demonstrates the first successful fabrication of fully recycled strontium ferrite magnets from End-of-Life materials. © 2025 The Authors., This work has been supported through the INSPIRES project funded by the EIT RawMaterials under grant number 20090, the BEETHOVEN project funded by the European Commission under grant agreement 101129912, and the GENIUS project funded by the Ministerio de Ciencia, Innovación y Universidades / Agencia Estatal de Investigación (MCIN/AEI/10.13039/501100011033) through Grant PCI2024–153493. Also, this work has been supported by grants TED2021–130957B-C51, CNS2022–135876, and RYC2021–031181-I funded by MICIU/AEI/10.13039/501100011033 and by the European Union NextGenerationEU/PRTR, grants PID2023–151036OA-I00 and PID2021–124585NB-C33 funded by MICIU/AEI/10.13039/501100011033 and by ERDF, EU, and by the JECS Trust, through Fund Contract no. 2022319., Peer reviewed