Skip to main content

Resultados relacionados

Resultados totales (Incluyendo duplicados): 4
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Sustainable production of hydrogen via steam reforming of furfural (SRF) with Co-catalyst supported on sepiolite

  • Sayas, S.
  • Da Costa-Serra, J. F.
  • Chica Lara, Antonio
Natural sepiolite is a mineral very abundant in Spain, being the main producer worldwide. This material is presented by the first time as promised support to prepare cobalt catalysts with high activity and hydrogen selectivity in the steam reforming of furfural (SRF). Two methods for cobalt incorporation on natural sepiolite, precipitation (PP) and incipient wetness impregnation (IWI), are explored and their influence in the preparation of catalysts highly active and selective in the SRF is studied. PP method makes possible to synthesize a catalytic material with high catalytic performance (high conversion of furfural, > 95%, and high hydrogen selectivity, 70%). Furthermore the production of non-desired byproducts such as CO, CH and acetone, decrease significantly in the catalyst prepared by PP (CoSep). Characterization by N adsorption-desorption to determine surface area, XRD, TPR and TEM shows that PP method favors the formation of smaller metallic particles of Co with a high dispersion. These differential physicochemical properties seem to explain the better catalytic performance exhibited by the sepiolitic catalyst prepared by the PP method (CoSep). In addition, this catalyst exhibits also a higher resistance to deactivation after 24 h of reaction time. This fact seems to be related to the lower coke deposition on the catalyst prepared by precipitation and particularly, with the lower sinterization of the metallic Co particles during the steam reforming of furfural., Thank you to the Spanish Government (Project RTI2018-102161-I00) and Generalitat Valenciana (PROMETEO/2018/006 grant) for the fanatical supporting. The support of the microscopy service at Universitat Politècnica de València (UPV) for the SEM and TEM analysis is also recognized.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Biogas dry reforming over Ni–Ce catalyst supported on nanofibered alumina

  • González, Juan José
  • Da Costa-Serra, J. F.
  • Chica Lara, Antonio
Four catalysts based on Ni and Ni–Ce supported on two γ-aluminas with different morphology (nanofibers and nanograins) have been prepared and studied in the dry reforming of simulated biogas. Catalysts were characterized by N physisorption, X-ray diffraction (XRD), temperature-programmed reduction (TPR), transmission electron microscopy (TEM), scanning electron microscopy (SEM), inductively coupled plasma with optical emission spectrometer (ICP-OES), chemisorption of H and elemental analysis (EA) to determine their most relevant physicochemical properties. Characterization results show that metallic Ni particles supported on nanofibered alumina (NFA) presents a higher dispersion and smaller size than that supported on the nanograiny alumina (NGA) probably due to the higher mesoporosity presented by the NFA support. On the other hand, the incorporation of Ce has a similar effect than the fibrous morphology, decreasing also the size of the Ni metallic particles and increasing their dispersion. In the dry reforming of synthetic biogas (CH/CO = 1.5) the nanofibered alumina containing 5 wt% Ni and 1.5 wt% Ce (NiCe/NFA) showed the highest catalytic activity at 750 °C (98% CO conversion) and stability (7.7% nickel sinterization level and 2.9 wt% carbon deposition). The stability of this catalyst was also demonstrated at 750 °C during 55 h of reaction time with a loss of activity at the steady state under 2%. In addition, the catalyst was regenerated at 600 °C in oxygen flow, recovering completely its initial catalytic performance. The excellent catalytic behavior of NiCe/NFA material has been related to the fibrous morphology of the alumina support, which promotes a better dispersion of the supported Ni metal particles, decreasing their size and increasing the number of actives sites where dry reforming reaction can take place. In addition, the incorporation of Ce seems to have also an important role by increasing the Ni-support interactions, decreasing sinterization of the metallic Ni particles and coke deposition. The contribution of both effects (morphology and Ce), separately and in combination, have been proved to enhance significantly the catalytic activity and stability of the synthesized catalysts in the dry reforming of simulated biogas., Thank you to the Spanish Government, Spain (Project RTI2018-102161-I00) and Generalitat Valenciana, Spain (PROMETEO/2018/006 grant) for the financial support. The support of the microscopy service at Universitat Politècnica de València (UPV) for the SEM and TEM analysis is also recognized.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Zeolite-supported Ni catalysts for CO2 methanation: Effect of zeolite structure and Si/Al ratio

  • Da Costa-Serra, J. F.
  • Cerdá Moreno, Cristina
  • Chica Lara, Antonio
The urgent need to reduce CO emissions requires the development of efficient catalysts for the conversion of CO into chemicals and fuels. In this study, a series of nickel catalysts supported on ITQ-2 and ZSM-5 zeolites have been prepared, characterized and tested in the hydrogenation reaction of CO towards methane. Specifically, two ITQ-2 and two ZSM 5 zeolites with different aluminum content have been studied. For both types, the higher Si/Al ratio of the material, the more active the catalyst due probably to its higher hydrophobicity. The largest difference was found for the ITQ-2 samples, being the CO conversion for the sample with a greater Si/Al ratio 50 points higher at 350 °C. Comparing both zeolite structures, while similar catalytic results were obtained with the samples with lower Si/Al ratio, a distinctly higher activity was found for the ITQ-2 zeolite without aluminum, pure silica. Therefore, this result suggests that the presence of aluminum is of particular relevance. Among the studied materials, the catalyst supported on the delaminated ITQ-2 zeolite without Al was the most active catalyst. Its higher activity was mainly attributed to the smaller crystallite size of nickel supported on the large external surface area presented by this zeolite., This research was funded by the Spanish Ministry of Science, Innovation and Universities, grant numbers SVP-2014-068713 and RTI2018-102161-B-I00.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Sustainable production of hydrogen by steam reforming of ethanol using cobalt supported on nanoporous zeolitic material

  • Da Costa-Serra, J. F.
  • Navarro, María Teresa
  • Rey García, Fernando
  • Chica Lara, Antonio
Cobalt catalysts supported on Y zeolite and mesoporized Y zeolite (Y-mod) have been studied in steam reforming of ethanol (SRE). Specifically, the eect of the mesoporosity and the acidity of the y zeolite as a support has been explored. Mesoporous were generated on Y zeolite by treatment with NH4F and the acidity was neutralized by Na incorporation. Four cobalt catalysts supported on Y zeolite have been prepared, two using Y zeolite without mesoporous (Co/Y, Co/Y-Na), and two using Y zeolite with mesoporous (Co/Y-mod and Co/Y-mod-Na). All catalysts showed a high activity, with ethanol conversion values close to 100%. The main dierences were found in the distribution of the reaction products. Co/Y and Co/Y-mod catalysts showed high selectivity to ethylene and low hydrogen production, which was explained by their high acidity. On the contrary, neutralization of the acid sites could explain the higher hydrogen selectivity and the lower ethylene yields exhibited by the Co/Y-Na and Co/Y-mod-Na. In addition, the physicochemical characterization of these catalysts by XRD, BET surface area, temperature-programmed reduction (TPR), and TEM allowed to connect the presence of mesoporous with the formation of metallic cobalt particles with small size, high dispersion, and with high interaction with the zeolitic support, explaining the high reforming activity exhibited by the co/y-mod-Na sample as well as its higher hydrogen selectivity. It has been also observed that the formation of coke is aected by the presence of mesoporous and acidity. Both properties seem to have an opposite eect on the reforming catalyst, decreasing and increasing the coke deposition, respectively., “This research was funded by Generalitat Valenciana, grant number PROMETEO/2018/006”, Spanish Government (Project RTI2018-102161-I00) and RED DE EXCELENCIA EN BIORREFINERIAS SOSTENIBLES (RED2018-102623-T).