DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Hydrogenation of Furfural to Cyclopentanone in Tert–Butanol-Water Medium: A Study of the Reaction Intermediates Reactivity Using Cu/ZnO/Al2O3 as Catalyst

  • Orozco-Saumell, Ana
  • Mariscal López, Rafael
  • Vila, Francisco
  • López Granados, Manuel
  • Martín Alonso, David
The catalytic transformation of furfural to cyclopentanone has been investigated using two different liquid phases as solvent: water and 30 wt.% tert–butanol in water. When using neat water at 160 °C, 40 bar of H2, and after 2 h of reaction time, furfural polymerizes, and the yield of cyclopentanone is just 42% with a low carbon balance, indicating that furfural is transformed to non-detected by-products, likely heavy resins. When using 30 wt.% tert–butanol in water, the yield of cyclopentanone is ca. 20%, and the major product is furfuryl alcohol with a 47% yield. We have studied the catalytic transformation of the most relevant reaction intermediates in the overall conversion of furfural to cyclopentanone. In the presence of tert–butanol, two steps are inhibited in the overall pathway: (i) the Piancatelli rearrangement of furfuryl alcohol and (ii) the transformation of cyclopentenone. This inhibition is attributed to the neutralization of protons from water dissociation by surface sites on the catalyst, preventing their participation in the overall reaction. To counteract these inhibitions when tert–butanol is present, higher H2 pressure (60 bar) and temperatures (200 °C) are required. We have been able to obtain productivities per gram of catalyst and mols of Cu basis of 411 gprod·h−1·gcat−1 and 14 gprod·s−1·molCu−1, respectively, which is substantially above that found for other copper-based catalysts., This research was funded by the Spanish Ministry of Science, Innovation, and Universities (projects RTI2018-094918-B-C41, -C42 and -C44). AOS also acknowledges financial support for a contract financed by the Biobased Industries Joint Undertaking (JU) under the European Union’s Horizon 2020 research and innovation program under grant agreement No. 101023202. The JU receives support from the European Union’s Horizon 2020 research and innovation program and the Bio-based Industries Consortium., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Aqueous phase hydrogenation of maleic acid to succinic acid mediated by formic acid: the robustness of the Pd/C catalytic system

  • Orozco-Saumell, Ana
  • Mariscal López, Rafael
  • Iglesias, J.
  • Maireles-Torres, P.
  • López Granados, Manuel
Long-term liquid phase studies of the activity in the formic acid-mediated hydrogenation of MAc to SAc were conducted in a fixed bed continuous reactor for two relevant situations: neutralising maleic and formic acids with NaOH and at the pH determined by both acids. Deactivation could only be observed when the catalyst was subjected to a WHSV of MAc above 13 gMAc gcat−1 h−1. Despite this deactivation, the reaction conditions can be adjusted (lowering the reaction temperature and/or decreasing the WHSV) to compensate for the loss of activity. Thus, for the neutralisation case, the catalyst could present a yield of SAc close to 100% for at least 400 h at a WHSV-MAc of 13 gMAc gcat−1 h−1 by setting the temperature at 180 °C, corresponding to an overall productivity above 5300 g of SAc per gcat, equivalent to more than 107 kg of SAc per gPd. An in-depth study of the catalyst used under these severe conditions was also conducted using a number of physico-chemical techniques. The sintering of Pd particles, Pd leaching, reduction-carbidization of Pd2+ and/or Pd into Pd carbides (PdCx) and deposition of organic compounds were identified in the spent catalysts for both the neutralised and acid runs. The presence of Na+ and of CO chemisorbed at the surface of the catalyst were also detected in the neutralised and acid cases, respectively. The rinsing of the catalyst with aqueous H2SO4 or treating the catalyst at 200 °C with streams containing O2 or H2 did not reactivate the catalyst. We concluded that the relevant causes of deactivation are Pd leaching and deposits of organic compounds; CO poisoning is also likely in the acid case. This is in agreement with the fact that deactivation is detected under high MAc-WHSV: the rate of leaching, CO chemisorption and deposition accelerates upon increasing it. © 2022 The Royal Society of Chemistry., This research was funded by the Spanish Ministry of Science, Innovation, and Universities (projects RTI2018-094918-B-C41, -C42 and -C44) and the Regional Government of Madrid (Project BIOTRES-CM S2018/EMT-4344). This project has also received funding from the Biobased Industries Joint Undertaking (JU) under the European Union's Horizon 2020 research and innovation programme under grant agreement no. 101023202. The JU receives support from the European Union's Horizon 2020 research and innovation programme and the Biobased Industries Consortium. AOS, due to the CSIC-UAM framework agreement, thanks to the PhD Program in Applied Chemistry of Doctoral School of Autonomous University of Madrid., Supplementary material, Peer reviewed