Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 3
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Role of the activated carbon surface on catalytic wet peroxide oxidation

  • Rey Barroso, Ana
  • Faraldos, Marisol
  • Bahamonde, A.
  • Casas, J. A.
  • Zazo, J. A.
  • Rodríguez, J. J.
[EN] Three activated carbons with fairly different characteristics have been checked in catalytic wet peroxide oxidation (CWPO) using phenol as a model compound for the purpose of learning the role of these materials which can be used as supports for the preparation of Fe or other metallic catalysts. A complex contribution of mixed effects is involved making difficult to predict the behavior of a given activated carbon. The surface of these materials promotes the undesirable decomposition of H2O2 to unreactive O2 instead of OH radicals in an extent depending on the nature and accessibility of the oxygen groups. A frankly basic surface including groups such as pyrone with an egg-shell type distribution on the carbon particle seems to be beneficial for a more effective decomposition of H 2O2 leading to a higher oxidation activity. The presence of iron in the activated carbon ashes is also an important factor which may hide in part other effects derived from the structure and surface composition of the carbon. However, that factor cannot explain by itself the differences found in the behavior of the activated carbons since two of them with a similar Fe content showed markedly different activities in CWPO of phenol. © 2008 American Chemical Society., Spanish Ministry of Education and Science by the financial support of the CTQ2007-61748/PPQ, CTQ2005-02284/PPQ, and CTM2007-60577/TECNO. Ana Rey acknowledges an FPU Grant from the Spanish Ministry of Education and Science.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Catalytic wet peroxide oxidation of phenol over Fe/AC catalysts: Influence of iron precursor and activated carbon surface

  • Rey Barroso, Ana
  • Faraldos, Marisol
  • Casas, J. A.
  • Zazo, J. A.
  • Bahamonde, A.
  • Rodríguez, J. J.
[EN] Different activated carbon-supported Fe catalysts have been prepared and tested in CWPO of phenol. Three well characterized activated carbons and two iron precursors (iron nitrate and iron pentacarbonyl) have been used. The behavior of these catalysts in CWPO has been related with their porous structure, surface composition, in terms of oxygen groups and Fe distribution onto the catalyst particles. The catalysts with a more uniform distribution of Fe showed a higher oxidation activity than the ones with an internal (egg-yolk type) or external (egg-shell type) distribution. These last provoke a faster decomposition of H2O2 mainly to O2, non-reactive at the mild reaction temperature used (50º C). No significant differences were observed from the iron precursors. Complete conversion of phenol and almost 80 % mineralization were obtained in less than 2 hours with the best catalyst. The residual by-products consisted in short-chain organic acids without significance in terms of toxicity. Fe leaching was observed in all the cases which can be mainly attributed to the presence of oxalic acid as oxidation by-product, refractory to the CWPO process investigated. The intensity of Fe leaching was related with the concentration of oxalic acid, This work has been supported by the Spanish Plan Nacional de I+D+i through the projects CTM2007-60577/TECNO, CTQ2007-1661748/PPQ and CTQ2005-02284/PPQ. Ana Rey thanks to the Ministerio de Educación y Ciencia (MEC) for a FPU Grant., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Optimizing calcination temperature of Fe/activated carbon catalysts for CWPO

  • Zazo, J. A.
  • Fraile, A. F.
  • Rey Barroso, Ana
  • Bahamonde, A.
  • Casas, J. A.
  • Rodriguez, J. J.
[EN] The influence of the calcination temperature (within the temperature range 150-300 °C) on the chemical nature of the surface as well as on the activity of an own-made Fe/AC catalyst for catalytic wet peroxide oxidation (CWPO) has been studied. The catalyst surface was characterized by means of TG, TPD and N2 adsorption/desorption analysis. The presence of iron promotes the oxidation of the activated carbon surface, increasing the amount of oxygen surface groups, mainly carboxylic acid, anhydride and lactone groups. On the other hand, the calcination step modifies the distribution of these groups, increasing the amount of lactone groups and reducing the pHslurry. Within the temperature range studied, the calcination temperature does not affect to the porous structure. The changes observed in the catalyst surface led to an increase of the catalytic activity as a consequence of a higher H2O2 decomposition into OH{radical dot} radicals, probably due to a better dispersion of the active phase. Neither oxygen surface groups by themselves nor pHslurry seemed to have influence on the catalytic activity. © 2009 Elsevier B.V. All rights reserved., Financial support from the Spanish Plan Nacional I+D+I through the projects CTQ2005-02284/PPQ, CTQ2007-61748/PPQ and CTM2007-60577/TECNO and from the CAM through the project S-0505/AMB/0395.