DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación
Artículo científico (JournalArticle)
Novel silicon oxycarbide/spodumene glass-ceramic composites with tailored thermal expansion coefficient
[EN] Highly densified silicon oxycarbide (SiOC)/spodumene composites with low coefficient of thermal expansion (CTE) were obtained just selecting the spark plasma sintering temperature employed. For the first time we proposed the use of spodumene a cheap and natural available lithium aluminium silicate mineral as meltable/active filler for SiOC-derived composites, due to its powerful fluxing properties and also its very low CTE. SiOC/spodumene composites sintered at 1200 ⁰C display a very low CTE (0.128±0.004–1.902±0.002 × 10−6 K−1) due to the α,β-transformation of spodumene. At higher sintering temperatures the CTE increases to 3.288±0.004 × 10−6 and 4.516±0.006 × 10−6 K−1 (1300 and 1400 ⁰C) due to the β-SiC formation. In this range of temperature, spodumene promotes the phase separation of SiOC and subsequent crystallization of cristobalite and β-SiC. The maximum values of hardness (11.5 ± 0.5 GPa) and elastic modulus (91±4 MPa) are reached at 1300 ⁰C, where the SiOC/composite displays a neat densification and the lowest roughness (1.61±0.01 nm)., This work was supported by project MAT2016–78700-R financed by the Spanish Research Agency and the European Regional Development Fund (AEI/FEDER, EU) and project ENE2012-39385-CO3-01 funded by Ministry of Economy, Industry and Competitiveness of Spain. We acknowledge support of the publication fee by the Spanish National Research Council (CSIC) Open Access Publication Support Initiative through its Unit of Information Resources for Research (URICI). The authors acknowledge C. Díaz-Dorado for her help in the preparation of AFM figures., Peer reviewed