Effect of the maturity of recycled aggregates on the mechanical properties and autogenous and drying shrinkage of high-performance concrete

  • Revilla Cuesta, Víctor
  • Evangelista, Luís
  • Brito, Jorge de
  • Ortega López, Vanesa
  • Manso Villalaín, Juan Manuel
The high cement content of high-performance concrete (HPC) results in improved strength, but also in large shrinkage. The substitution of natural aggregates (NA) with recycled aggregates (RA) notably affects these properties in conventional concrete. This study intends to analyse the effect of the content of RA and their maturity (time elapsed between casting and crushing of the parent concrete from which RA are obtained) on these properties of HPC. To this end, five mixes were manufactured with 0%, 25%, and 100% of coarse and fine RA of different maturities, 7 days (early-age RA) and 6 months (matured RA). The mechanical properties and the autogenous, drying, and total shrinkage of all mixes were determined. Both the increase of RA content and the lower stiffness and strength of early-age RA relative to matured RA worsened the mechanical behaviour of HPC. Regarding shrinkage, the lower stiffness and higher water absorption of matured RA compared to NA decreased autogenous shrinkage by 20%, but increased drying and total shrinkage. The lower stiffness of early-age RA and their shrinkage amplified all types of shrinkage of HPC around 10–20%. Nevertheless, the hydration of their unhydrated cement particles during the mixing process reduced those increases from what was expected. Total shrinkage of early-age recycled aggregate HPC could be estimated from the shrinkage of both a HPC mix of identical composition but with matured RA and the parent concrete. Overall, it can be concluded that RA’s maturity affects the mechanical performance and, especially, the shrinkage of HPC, so it should be considered when using this type of aggregate., Spanish Ministry MCIU, AEI and ERDF [grant numbers FPU17/03374; EST19/00263]. The authors also acknowledge the support of the Foundation for Science and Technology, CERIS Research Centre and Instituto Superior Técnico, the Junta de Castilla y León [grant number UIC231], and the University of Burgos [grant number Y135.GI].
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publicación Artículo científico (JournalArticle)

Mechanical performance and autogenous and drying shrinkage of MgO-based recycled aggregate high-performance concrete

  • Revilla Cuesta, Víctor
  • Evangelista, Luís
  • Brito, Jorge de
  • Skaf Revenga, Marta
  • Ortega López, Vanesa
The high strength and durability of high-performance concrete (HPC) may be significantly reduced by shrinkage cracking. The use of reactive magnesium oxide (MgO) can reduce shrinkage of cement-based materials due to its expansive properties. This study intends to analyse the validity of MgO as shrinkage-reducing agent in recycled aggregate HPC. To do so, ten HPC mixes with 0%, 25%, and 100% of both early-age (7-days air curing) and matured (6-month air curing) RA were produced. In half of the mixes, 10% ordinary Portland cement was replaced with MgO. The use of MgO slightly worsened the mechanical behaviour of HPC, especially when combined with large amounts of RA. On the other hand, the expansion of MgO fully offset the autogenous shrinkage of HPC and reduced total shrinkage by around 20–40%. Water storage of RA, and its deferred release over time, produced a more efficient hydration of MgO, which in turn led to a further reduction of autogenous shrinkage. However, the increase of drying shrinkage caused by RA was greater than this decrease of autogenous shrinkage due to MgO, so the higher the RA content of HPC the lower the total shrinkage reduction when adding MgO. Thus, the decrease of total shrinkage caused by MgO was compensated by the shrinkage increase because of RA when adding amounts above 35% early-age RA and 42% matured RA. Therefore, despite the suitability of MgO as shrinkage-reducing agent in recycled aggregate HPC, its effectiveness was reduced with increasing amounts of RA., Spanish Ministry of Universities, MICINN, AEI and ERDF [grant numbers FPU17/03374; EST19/00263; PID2020-113837RB-I00; 10.13039/501100011033]. The authors also acknowledge the support of the Foundation for Science and Technology, CERIS Research Centre and Instituto Superior Técnico, the Junta de Castilla y León [grant number UIC231], and the University of Burgos [grant number Y135.GI].
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publicación Artículo científico (JournalArticle)

Shrinkage prediction of recycled aggregate structural concrete with alternative binders through partial correction coefficients

  • Revilla Cuesta, Víctor
  • Evangelista, Luís
  • Brito, Jorge de
  • Skaf Revenga, Marta
  • Manso Villalaín, Juan Manuel
Estimating the shrinkage of structural concrete is essential to calculate, at the design stage, the stresses that a structure may experience due to this phenomenon. Nevertheless, changes in composition, as well as the use of wastes as raw materials, alter the shrinkage behaviour of concrete and render invalid shrinkage-prediction models from the standards. This paper shows a procedure to estimate the shrinkage of recycled aggregate concrete made with alternative binders. This procedure is based on modifying the shrinkage estimated through the Eurocode 2 or ACI 209.2R models by multiplying it by a partial correction coefficient for every change in concrete composition. The application of this procedure to high-performance and self-compacting concretes made with various contents of recycled aggregate of different maturity, reactive magnesium oxide and ground granulated blast furnace slag showed that it is suitable for estimating long-term shrinkage with maximum deviations of ±10%. However, to obtain an adequate accuracy, it is necessary to bear in mind some tips, such as the need to consider the prediction interactions between the factors, the usefulness of the natural logarithm of the concrete age to improve the estimation accuracy or the convenience of introducing a concrete-age-dependent coefficient to reach accurate shrinkage estimations at early ages. Finally, the partial correction coefficients are found to be of a simpler nature for the ACI 209.2R model, so this model is recommended for predicting the shrinkage of recycled aggregate concrete., This work was supported by the Spanish Ministry of Universities, MICINN, AEI, EU and ERDF [grant numbers PID2020-113837RB-I00; 10.13039/501100011033; FPU17/03374; EST19/00263]. Moreover, the authors acknowledge the support of the Junta de Castilla y León [grant number UIC231]; the University of Burgos [grant number Y135. GI]; and the Foundation for Science and Technology, CERIS Research Centre and Instituto Superior Técnico.
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publicación Tesis doctoral (DoctoralThesis)

Performance of self-compacting concrete manufactured with coarse and fine recycled concrete aggregate and slag-based binder

  • Revilla Cuesta, Víctor
El hormigón autocompactante es un tipo de hormigón caracterizada por su elevada fluidez, lo que permite que pueda ponerse en obra sin ningún tipo de vibrado y con un menor consumo de energía. La sostenibilidad de este material de construcción puede aumentarse mediante el empleo de materiales alternativos en su composición. La presente Tesis Doctoral estudia el efecto del empleo de árido de hormigón reciclado y escoria siderúrgica granulada molida para la fabricación del hormigón autocompactante. Mediante un compendio de siete artículos científicos, se demuestra que este tipo de hormigón conserva la autocompactabilidad hasta 60 minutos después del proceso de mezcla, que la estimación indirecta de su resistencia a compresión es posible, y que el comportamiento plástico longitudinal y transversal, así como su deformabilidad térmica, es adecuado para su uso. Globalmente, se demuestra que el empleo de estos subproductos en el hormigón autocompactante puede realizarse de forma exitosa., This work was supported by [MICINN, AEI and ERDF] under grant [PID2020–113837RB-I00; 10.13039/501100011033]. Ministerio de Ciencia e Innovación (MICINN), a la Agencia Estatal de Investigación (AEI) y a los Fondos Europeos de Desarrollo Regional (FEDER) la financiación de la presente Tesis Doctoral a través de la convocatoria de 2017 de las Ayudas para la Formación de Profesorado Universitario, FPU17/03374. Sin esta beca, mi Tesis Doctoral jamás habría existido. A estas mismas instituciones les agradezco también la financiación a través de la convocatoria de 2020 de las Ayudas a la movilidad para estancias breves y traslados temporales para beneficiarios del programa de Formación del Profesorado Universitario, EST19/00263, gracias a la cual pude realizar la estancia en el Instituto Superior Técnico (IST) de la Universidad de Lisboa.