RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Dielectric relaxation, ac conductivity and electric modulus in poly(vinylidene fluoride)/NaY zeolite composites

  • Lopes, A.C.
  • Costa, C.M.
  • Neves, I.C.
  • Lanceros-Mendez, S.
  • Sabater i Serra, Roser|||0000-0002-5550-7066
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] Poly(vinylidene fluoride)/zeolite composites prepared by solvent casting at 190 °C have been investigated by scanning electronic microscopy, Fourier transformed infrared spectroscopy and broadband dielectric relaxation spectroscopy. The inclusion of the NaY zeolite filler in the polymer matrix induces the crystallization of poly(vinylidene fluoride), PVDF, in the electroactive γ phase. The dielectric function, ac conductivity and electric modulus of the composites were investigated as a function of zeolite content in the frequency range from 0.1 Hz to 1×107 Hz at temperatures from −120 to 150 °C. The main relaxation process (β-relaxation) of the amorphous phase of the polymer matrix is not affected by the presence of the zeolite, as verified by the similar relaxation parameters obtained for the pure polymer and for the PVDF/NaY4% composite. In a similar way, the zeolite low temperature relaxation is not significantly affected by the polymer phase. On the other hand, the electric modulus formalismreveals significant contributions of the fillers to the electrical permittivity and conductivity of the composites. The presence of the zeolite particles increases ac conductivity and theMaxwell Wagner Sillars contribution that is predominant at low frequencies with respect to ohmic contribution to permittivity., This work is partially funded by the Centre of Physics and Centre of Chemistry (University of Minho, Portugal) and by FEDER funds through the Programa Operacional Factores de Competitividade-COMPETE and by national funds by FCT-Fundação para a Ciência e a Tecnologia, project references, NANO/NMed-SD/0156/2007, PTDC/CTM/69316/2006, PEst-C/QUI/UI0686/2011 and PTDC/CTM-NAN/112574/2009. A.C.L. and C.M.C. also thank the FCT for the grant SFRH/BD/62507/2009 and SFRH/BD/68499/2010, respectively. The authors also thank support from the COST Action MP1003, the European Scientific Network for Artificial Muscles (ESNAM)
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Effect of neutralization and cross-linking on the thermal degradation of chitosan electrospun membranes

  • Correia, D. M.
  • Gamiz Gonzalez, Mª Amparo
  • Botelho, G.
  • Lanceros-Mendez, S.
  • Sencadas, V.
  • Vidaurre, Ana|||0000-0003-3394-1176
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] Thermal degradation of as-electrospun chitosan membranes and samples subsequently treated with ethanol and cross-linked with glutaraldehyde has been studied by thermogravimetry (TG) coupled with an infrared spectrometer. The influence of the electrospinning process and cross-linking in the electrospun chitosan thermal stability was evaluated. Up to three degradation steps were observed in the TG data, corresponding to water dehydration reaction at temperatures below 100 C, loss of side groups formed between the amine groups of chitosan and trifluoroacetic acid between 150 and 270 C and chitosan thermal degradation that starts around 250 C and goes up to 400 C. The Kissinger model was employed to evaluate the activation energies of the electrospun membranes during isothermal experiments and revealed that thermal degradation activation energy increases for the samples processed by electrospinning and subsequent neutralization and cross-linking treatments with respect to the neat chitosan powder., This work was supported by FEDER through the COMPETE Program and by the Portuguese Foundation for Science and Technology (FCT) in the framework of the Strategic Project PEST-C/FIS/UI607/2011 and PEST-C/QUI/UIO686/2011. The authors also thank funding from "Matepro-Optimizing Materials and Processes", ref. "NORTE-07-0124-FEDER-000037", co-funded by the "Programa Operacional Regional do Norte" (ON.2 - O Novo Norte), under the "Quadro de Referencia Estrategico Nacional" (QREN), through the "Fundo Europeu de Desenvolvimento Regional" (FEDER). The authors also thank support from the COST Action MP1003 - "European Scientific Network for Artificial Muscles", MP1206 "Electrospun Nano-fibres for bio inspired composite materials and innovative industrial applications" and MP1301 "New Generation Biomimetic and Customized Implants for Bone Engineering". DMC and VS thank the FCT for the SFRH/BD/82411/2011 and SFRH/BPD/63148/2009 grants, respectively. JLGR and MAGG acknowledge the support of the Spanish Ministry of Science and Innovation through project no. MAT2010-21611-C03-01 and MAGG the BES-2011-044740 grant. CIBER-BBN is an initiative funded by the VI National R&D&i Plan 2008-2011, Iniciativa Ingenio 2010, Consolider Program, CIBER Actions and financed by the Instituto de Salud Carlos III with assistance from the European Regional Development Fund.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Influence of oxygen plasma treatment parameters on poly(vinylidene fluoride) electrospun fiber mats wettability

  • Correia, Daniela M.
  • Ribeiro, Clarisse
  • Sencadas, Vitor Joao Gomes Da Silva
  • Botelho, G.
  • Carabineiro, S.A.C.
  • Lanceros-Mendez, Senentxu
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] Electrospun poly(vinylidene fluoride) (PVDF) fiber mats find applications in an increasing number of areas, such as battery separators, filtration and detection membranes, due to their excellent properties. However, there are limitations due to the hydrophobic nature and low surface energy of PVDF. In this work, oxygen plasma treatment has been applied in order to modify the surface wettability of PVDF fiber mats and superhydrophilic PVDF electrospun membranes have been obtained. Further, plasma treatment does not significantly influences fiber average size (similar to 400 +/- 200 nm), morphology, electroacfive beta-phase content (similar to 80-85%) or the degree of crystallinity (X-c of 42 +/- 2%), allowing to maintain the excellent physical-chemical characteristics of PVDF. Plasma treatment mainly induces surface chemistry modifications, such as the introduction of oxygen and release of fluorine atoms that significantly changes polymer membrane wettability by a reduction of the contact angle of the polymer fibers and an overall decrease of the surface tension of the membranes., This work is funded by FEDER funds through the "Programa Operacional Fatores de Competitividade - COMPETE" and by national funds arranged by FCT - Fundacao para a Ciencia e a Tecnologia, project references NANO/NMed-SD/0156/2007, PTDC/CTM-NAN/112574/2009, PEST-C/FIS/UI607/2011 and PEST-C/QUI/UIO686/2013. The authors also thank funding from Matepro - Optimizing Materials and Processes", ref. NORTE-07-0124-FEDER-000037", co-funded by the "Programa Operacional Regional do Norte" (ON.2-O Novo Norte), under the "Quadro de Referencia Estrategico Nacional" (QREN), through the "Fundo Europeu de Desenvolvimento Regional" (FEDER). The authors also thank support from the COST Action MP1003, 2010 'European Scientific Network for Artificial Muscles', MP1206 "Electrospun Nano-fibres for bio inspired composite materials and innovative industrial applications" and MP1301 "New Generation Biomimetic and Customized Implants for Bone Engineering". DMC, CR, VS and SACC thank the FCT for the SFRH/BD/82411/2011, SFRH/BPD/90870/2012, SFRH/BPD/64958/2009 and Investigator FCT IF/1381/2013 grants, respectively. JLGR acknowledges the support of Ministerio de Economia y Competitividad, MINECO, through the MAT2013-46467-C4-1-R project. CIBER-BBN is an initiative funded by the VI National R&D&i Plan 2008-2011, Iniciativa Ingenio 2010, Consolider Program, CIBER Actions and financed by the Instituto de Salud Carlos III with assistance from the European Regional Development Fund. Dr. Carlos M. Sa (CEMUP) is acknowledged for assistance with XPS analyses.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Influence of electrospinning parameters on Poly(hydroxybutyrate) electrospun membranes fiber size and distribution

  • Correia, Daniela M.
  • Ribeiro, Clarisse
  • Ferreira, Jose C. C.
  • Botelho, Gabriela
  • Lanceros Mendez, Senen
  • Sencadas, Vitor
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
Poly(hydroxybutyrate) (PHB) obtained from sugar cane waste was dissolved in a blend of chloroform and dimethylformamide (DMF) and electrospun at 40 degrees C. By adding DMF to the solution, the electrospinning process for the PHB polymer becomes more stable, allowing complete polymer crystallization during the jet travelling between the tip and the grounded collector. The influence of processing parameters on fiber size and distribution was systematically studied. It was observed that an increase of tip inner diameter promotes a decrease of the fiber average size and a broader distribution. Conversely, an increase of the electric field and flow rate produces an increase of fiber diameter until a maximum of similar to 2.0 mu m but for electric fields higher than 1.5 kV cm(-1), a decrease of the fiber diameter was observed. Polymer crystalline phase seems to be independent of the processing conditions and a crystallinity degree of 53% was found. Moreover, thermal degradation of the as-spun membrane occurs in single step degradation with activation energy of 91 kJ mol(-1). Furthermore, MC-3T3-E1 cell adhesion was not inhibited by the fiber mats preparation, indicating their potential use for biomedical applications., Contract grant sponsor: FEDER; contract grant sponsor: Programa Operacional Factores de Competitividade-COMPETE; contract grant sponsor: FCT-Fundacao para a Ciencia e a Tecnologia; contract grant numbers: NANO/NMed-SD/0156/2007, PTDC/CTM/73030/2006, and PTDC/CTM/69316/2006; contract grant sponsor: COST Action MP1003, 2010 'European Scientific Network for Artificial Muscles'; contract grant sponsor: FCT; contract grant numbers: SFRH/BPD/63148/2009 and SFRH/BD/82411/2011; contract grant sponsor: IINL; contract grant sponsor: Spanish Ministry of Science and Innovation (including the FEDER financial support); contract grant number: MAT2010-21611-C03-01; contract grant sponsors: VI National R&D&i Plan 2008-2011, Iniciativa Ingenio 2010, Consolider Program, and Instituto de Salud Carlos III (with assistance from the European Regional Development Fund).
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Influence of crystallinity and fiber orientation on hydrophobicity and biological response of poly(L-lactide) electrospun mats

  • Areias, A.C.
  • Ribeiro, Clarisse
  • Sencadas, Victor
  • Garcia Giralt, Natalia
  • Diez Perez, A.
  • Lanceros Mendez, Senen
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] Poly(L-lactide) electrospun mats have been produced with random and aligned fiber orientation and degrees of crystallinity from 0 up to nearly 50%. These two factors, fiber alignment and degree of crystallinity, strongly affect the hydrophobicity of the samples, this being larger for the aligned fiber mats and for the fibers with a higher degree of crystallinity. Whereas, the first effect can be associated with a decrease in the degree of porosity, the second should be related to an increase in fiber stiffness as the observed fiber roughness variations do not show strong differences between the samples. Proliferation of human chondrocytes cultured in a monolayer on these substrates is similar in both aligned and non-aligned amorphous mats. Crystallization of the aligned mats, on the other hand, nearly suppresses proliferation and the cells produce higher amounts of aggrecan, characteristic of the extracellular matrix of hyaline cartilage., This work is funded by FEDER funds through the "Programa Operacional Factores de Competitividade - COMPETE'' and by national funds by FCT (Fundacao para a Ciencia e a Tecnologia, project references PTDC/CTM/69316/2006, PTDC/CTM-NAN/112574/2009, and NANO/NMed-SD/0156/2007). V.S. thanks the FCT for the SFRH/BPD/63148/2009 grant. C. R. thanks the IINL for the financial support via a PhD grant. NG thanks Red Tematica de Investigacion Cooperativa en Envejecimiento y Fragilidad (RETICEF), which is an initiative of the ISCIII and the Catalan Government (2009SGR00848). JLGR acknowledges the support of the Spanish Ministry of Education through project No. MAT2010-21611-C03-01 (including the FEDER financial support). The authors thank the support from the COST Action MP1003, 2010, 'European Scientific Network for Artificial Muscles' (ESNAM).
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Relaxation dynamics of poly(vinylidene fluoride) studied by dynamical mechanical measurements and dielectric spectroscopy

  • Sencadas, V.
  • Lanceros-Mendez, S.
  • Andrio Balado, A.
  • Sabater i Serra, Roser|||0000-0002-5550-7066
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] The aim of this study is to analyze the mobility of polymer chains in semicrystalline poly(vinylidene fluoride) (PVDF). PVDF crystallizes from the melt in the crystalline phase. The transformation from the phase to the electroactive phase can be induced by stretching at temperatures in the range between 80 and 140 ◦C. The spherulitic structure of the crystalline phase is deformed during stretching to form fibrils oriented in the direction of the strain. The amorphous phase confined among the crystalline lamellae is distorted as well and some degree of orientation of the polymer chains is expected. Dynamicmechanical and dielectric spectroscopy measurements were performed in PVDF films stretched to strain ratios up to 5 at temperatures between 80 and 140 ◦C. Dynamic-mechanical measurements were conducted between −60 ◦C and melting and in this temperature range the relaxation spectra show the main relaxation of the amorphous phase (called -relaxation) and at higher temperatures a relaxation related to crystallites motions (c-relaxation). Although the mean relaxation times of the -relaxation are nearly equal in PVDF before and after crystal phase transformation, a significant change of shape of the relaxation spectrum proves the effect of chain distortion due to crystal reorganization. In stretched PVDF the elastic modulus of the polymer in the direction of deformation is significantly higher than in the transversal one, as expected by chain and crystals fibril orientation. The recovery of the deformation when the sample is heated is related with the appearance of the c-relaxation. Dielectric spectroscopy spectrum shows the main relaxation of the amorphous phase and a secondary process (-relaxation) at lower temperatures. Stretching produces significant changes in the relaxation processes, mainly in the strength and shape of the main relaxation. The Havriliak-Negami function has been applied to analyze the dielectric response., This work is funded by FEDER funds through the "Programa Operacional Factores de Competitividade-COMPETE" and by national funds by FCT-Fundacao para a Ciencia e Tecnologia, project references NANO/NMed-SD/0156/2007, PTDC/CTM/69316/2006 and PTDC/CTM-NAN/112574/2009. V. S. thanks the FCT for the SFRH/BPD/63148/2009 grant. JLGR acknowledges the support of the Spanish Ministry of Science and Innovation through MAT2010-21611-C03-01 (including the FEDER financial support), and EUI2008-00126 projects and funding in the Centro de Investigacion Principe Felipe in the field of Regenerative Medicine through the collaboration agreement from the Conselleria de Sanidad (Generalitat Valenciana), and the Instituto de Salud Carlos III (Ministry of Science and Innovation). The authors also acknowledge support from the COST Action MP1003, 2010 "European Scientific Network for Artificial Muscles".
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Electrical and thermal behavior of gamma-phase poly(vinylidene fluoride)/NaY zeolite composites

  • Lopes, A. C.
  • Caparros, C.
  • Neves, I. C.
  • Lanceros-Mendez, Senentxu
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
Poly(vinylidene fluoride), PVDF, based composites with increasing NaY zeolite content up to 32 wt.% have been processed by solvent casting and melt crystallization. Depending on the melting temperature of the polymer, the composite crystallizes in the electroactive gamma or non electroactive a-phase of the polymer. The dielectric constant at room temperature reaches values larger that 1000 for the 32 wt.% composite at 1 kHz and it is mainly attributed to restricted ion mobility and interfacial polarization effects due to the zeolite inclusion, leading also to high dielectric losses. For the higher zeolite concentrations the composite d.c. electrical conductivity is characterized by two conducting regimes separated by a concentration independent breaking voltage of 4 V, which is associated to an intrazeolite charge transport., This work is funded by FEDER funds through the "Programa Operacional Factores de Competitividade - COMPETE" and by National funds by FCT- Fundacao para a Ciencia e a Tecnologia, Project references NANO/NMed-SD/0156/2007, PTDC/CTM/69316/2006, PEst-C/QUI/L110686/2011 and PTDC/CTM-NAN/112574/2009. ACL thanks the FCT for the Grant SFRH/BD/62507/2009. The authors also thank support from the COST Action MP1003, the 'European Scientific Network for Artificial Muscles' (ESNAM).
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Composition-dependent physical properties of poly[(vinylidene fluoride)-co-trifluoroethylene] poly(ethylene oxide) blends

  • Costa, Carlos M.
  • Tamano Machiavello, M.N.
  • Lanceros Mendez, Senen
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
Polymer blends based on poly(vinylidene fluoride-co-trifluoroethylene) copolymers, P(VDF-TrFE), and poly(ethylene oxide), PEO, with varying compositions have been prepared by solvent casting. In this way, P(VDF-TrFE) crystallizes from the solution while solvent evaporates, while PEO crystallizes from the melt during cooling to room temperature. The surface morphology of the polymer blends indicates the transition from the fibrillar microstructure typical of PVDF-TrFE to the spherulite structure characteristic of PEO. The vibration mode characteristics of P(VDF-TrFE) are not influenced by the presence of PEO in the polymer blend. Confinement of PEO in the P(VDF-TrFE) phase change the conformation of PEO from trans to helix, increasing this transformation for increasing P(VDF-TrFE) content in the polymer blends. Sequential crystallization of the two polymers produce separated amorphous phases whose independent cooperative conformational motions are revealed by two main dynamic-mechanical relaxations. No chemical interaction seems to exist between the polymers within the blend., This study is funded by FEDER funds through the "Programa Operacional Factores de Competitividade - COMPETE'' and by national funds by FCT-Fundacao para a Ciencia e a Tecnologia, Project References NANO/NMed-SD/0156/2007 and PTDC/CTM/69316/2006. C. M. C. also thanks the FCT for the Grant SFRH/BD/68499/2010. The authors also thank support from the COST Action MP1003, the "European Scientific Network for Artificial Muscles'' (ESNAM). JLGR acknowledges the support of the Spanish Ministry of Education through Project No. MAT2010-21611-C03-01 (including the FEDER financial support). CIBER-BBN is an initiative funded by the VI National R&D&D&i Plan 2008-2011, Iniciativa Ingenio 2010, Consolider Program, CIBER Actions and financed by the Instituto de Salud Carlos III with assistance from the European Regional Development Fund.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Influence of fiber diameter and crystallinity on the stability of electrospun poly(L-lactic acid) membranes to hydrolytic degradation

  • Dias, Juliana C.
  • Ribeiro, Clarisse
  • Sencadas, V.
  • Botelho, G.
  • Lanceros Mendez, Senentxu
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
Hydrolytic degradation of electrospun mats of poly(l-lactic acid), PLLA, as a function of crystallinity and fiber diameter has been studied. The degradation in a saline phosphate buffer solution (PBS) up to 20 weeks produced a slight decrease in the sample mass but a clear decrease of the polymer average molecular weight in the amorphous fibers. This effect decreases as crystallinity increases. It is important for applications that morphological characteristics of the membranes such as average fiber diameter and membrane porosity are also affected by the degradation process. Fiber diameter increases while membrane porosity decreases, resulting in closer packed fibers due to the release of internal tensions related to the electrospinning and/or thermal treatment processes., This work is funded by FEDER funds through the "Programa Operacional Factores de Competitividade - COMPETE" and by national funds arranged by FCT - Fundacao para a Ciencia e a Tecnologia, project references NANO/NMed-SD/0156/2007, PTDC/CTM/73030/2006 and PTDC/CTM/69316/2006. The authors also thank support from the COST Action MP1003, 2010 'European Scientific Network for Artificial Muscles'. V.S. thanks the FCT for the SFRH/BPD/63148/2009 grant. C. R. thanks the Iberian Institute of Nanotechnology Laboratory (IINL) for a PhD grant. JLGR acknowledge the support of the Spanish Ministry of Education through project No. MAT2010-21611-C03-01 (including the FEDER financial support).
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Processing and characterization of alpha-elastin electrospun membranes

  • Araujo, J.
  • Padrao, J.
  • Silva, J. P.
  • Dourado, F.
  • Correia, D. M.
  • Botelho, G.
  • Lanceros-Mendez, S.
  • Sencadas, V.
  • Gómez Ribelles, José Luís|||0000-0001-9099-0885
[EN] Elastin isolated from fresh bovine ligaments was dissolved in a mixture of 1,1,1,3,3,3-Hexafluoro-2-propanol and water were electrospun into fiber membranes under different processing conditions. Fiber mats of randomly and aligned fibers were obtained with fixed and rotating ground collectors and fibrils were composed by thin ribbons whose width depends on electrospinning conditions; fibrils with 721 nm up to 2.12 ¿m width were achieved. After cross-linking with glutaraldehyde, ¿-elastin can uptake as much as 1700 % of PBS solution and a slight increase on fiber thickness was observed. The glass transition temperature of electrospun fiber mats was found to occur at ~80 °C. Moreover, ¿-Elastin showed to be a perfect elastomeric material, and no mechanical hysteresis was found in cycle mechanical measurements. The elastic modulus obtained for random and aligned fibers mats in a PBS solution was 330±10 kPa and 732±165 kPa, respectively. Finally, the electrospinning and cross-linking process does not inhibit MC-3T3-E1 cell adhesion. Cell culture results showed good cell adhesion and proliferation in the cross-linked elastin fiber mats., This work is funded by FEDER funds through the "Programa Operacional Factores de Competitividade-COMPETE" and by national funds arranged by FCT-Fundacao para a Ciencia e a Tecnologia, project references NANO/NMed-SD/0156/2007, PTDC/CTM-NAN/112574/2009, and PEST-C/FIS/UI607/2011. The authors also thank funding from "Matepro-Optimizing Materials and Processes", ref. "NORTE-07-0124-FEDER-000037", cofunded by the "Programa Operacional Regional do Norte" (ON.2-O Novo Norte), under the "Quadro de Referencia Estrategico Nacional" (QREN), through the "Fundo Europeu de Desenvolvimento Regional" (FEDER). The authors also thank support from the COST Action MP1003, 2010 'European Scientific Network for Artificial Muscles'. VS, JP, JS, and DMC thank the FCT for the SFRH/BD/48708/2008, SFRH/BD/64901/2009, SFRH/BPD/64958/2009 and SFRH/BPD/63148/2009, and SFRH/BD/82411/2011 grants, respectively. JLGR acknowledges the support of the Spanish Ministry of Science and Innovation through project No. MAT2010-21611-C03-01 (including the FEDER financial support). CIBER-BBN is an initiative funded by the VI National R&D&i Plan 2008-2011, Iniciativa Ingenio 2010, Consolider Program, CIBER Actions and financed by the Instituto de Salud Carlos III with assistance from the European Regional Development Fund.