Pasar al contenido principal

DISEÑO DE LAS PROPIEDADES DE LAMINAS DE OXIDOS METALICOS (DOPADOS) CRECIDOS POR SPUTTERING MEDIANTE TRATAMIENTOS TERMICOS ULTRARRAPIDOS

RTI2018-095137-B-I00

•
Nombre agencia financiadora Agencia Estatal de Investigación
Acrónimo agencia financiadora AEI
Programa Programa Estatal de I+D+i Orientado a los Retos de la Sociedad
Convocatoria Proyectos I+D+i Retos de Investigación
Año convocatoria 2018
Plan Estatal 2017-2020 Plan Estatal de Investigación Científica y Técnica y de Innovación
Centro beneficiario AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 2
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Phase selectivity in Cr and N Co-Doped TiO2 films by modulated sputter growth and post-deposition flash-lamp-annealing

  • Gago, Raúl
  • Prucnal, Slawomir
  • Hübner, René
  • Munnik, Frans
  • Esteban-Mendoza, David
  • Jiménez, Ignacio
  • Palomares, F. Javier
In this paper, we report on the phase selectivity in Cr and N co-doped TiO2 (TiO2:Cr,N) sputtered films by means of interface engineering. In particular, monolithic TiO2:Cr,N films produced by continuous growth conditions result in the formation of a mixed-phase oxide with dominant rutile character. On the contrary, modulated growth by starting with a single-phase anatase TiO2:N buffer layer, can be used to imprint the anatase structure to a subsequent TiO2:Cr,N layer. The robustness of the process with respect to the growth conditions has also been investigated, especially regarding the maximum Cr content (<5 at.%) for single-phase anatase formation. Furthermore, post-deposition flash-lamp-annealing (FLA) in modulated coatings was used to improve the as-grown anatase TiO2:Cr,N phase, as well as to induce dopant activation (N substitutional sites) and diffusion. In this way, Cr can be distributed through the whole film thickness from an initial modulated architecture while preserving the structural phase. Hence, the combination of interface engineering and millisecond-range-FLA opens new opportunities for tailoring the structure of TiO2-based functional materials., The research leading to these results has received funding from projects RTI2018-095137-B-I00 and MAT2016-80394-R from Ministerio de Ciencia, Innovación y Universidades (Spain) and grant agreement n° 226716 from the European Community’s Seventh Framework Programme (FP7/2007-2013). Funding of TEM Talos F200X by the German Federal Ministry of Education of Research (BMBF) through Grant No. 03SF0451 in the framework of HEMCP is gratefully acknowledged., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

ZnOTe Compounds Grown by DC-Magnetron Co-Sputtering

  • Sánchez Garrido, Olga
  • Hernández-Vélez, M.
ZnOTe compounds were grown by DC magnetron cosputtering from pure Tellurium (Te) and Zinc (Zn) cathodes in O2/Ar atmosphere. The applied power on the Zn target was constant equal to 100 W, while the one applied on the Te target took two values, i.e., 5 W and 10 W. Thus, two sample series were obtained in which the variable parameter was the distance from the Te targets to the substrate. Sample compositions were determined by Rutherford Backscattering Spectroscopy (RBS) experiments. Structural analysis was done using X-Ray diffraction (XRD) spectrometry and the growth of the hexagonal w-ZnO phase was identified in the XRD spectra. RBS results showed high bulk homogeneity of the samples forming ZnOTe alloys, with variable Te molar fraction (MF) ranging from 0.48–0.6% and from 1.9–3.1% for the sample series obtained at 5 W and 10 W, respectively. The results reflect great differences between the two sample series, particularly from the structural and optical point of view. These experiments point to the possibility of Te doping ZnO with the permanence of intrinsic defects, as well as the possibility of the formation of other Te solid phases when its content increases. The results and appreciable variations in the band gap transitions were detected from Photoluminescence (PL) measurements., This work was supported by the Ministerio de Ciencia, Innovación y Universidades of Spain through the Project RTI2018-095137-B-I00., Peer reviewed