Pasar al contenido principal

Sustainable Development of Cement and Concrete Technology with Low Environmental Impact

RYC2021-032620-I

•
Nombre agencia financiadora Agencia Estatal de Investigación
Acrónimo agencia financiadora AEI
Programa Programa Estatal para Desarrollar, Atraer y Retener Talento
Subprograma Subprograma Estatal de Incorporación
Convocatoria Ramón y Cajal
Año convocatoria 2021
Plan Estatal 2021-2023 Plan Estatal de Investigación Científica y Técnica y de Innovación
Centro beneficiario AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 4
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Durability of Magnesium Potassium Phosphate Cements (MKPCs) under Chemical Attack

  • Chhaiba, Salma
  • Martínez-Sánchez, Sergio
  • Husillos Rodríguez, N.
  • Palomo, Ángel
  • Kinoshita, Hajime
  • García-Lodeiro, Inés
Magnesium phosphate cements (MPCs), also known as chemically bonded ceramics, represent a class of inorganic cements that have garnered considerable interest in recent years for their exceptional properties and diverse applications in the construction and engineering sectors. However, the development of these cements is relatively recent (they emerged at the beginning of the 20th century), so there are still certain aspects relating to their durability that need to be evaluated. The present work analyses the chemical durability of magnesium potassium phosphate cements (MKPCs) during 1 year of immersion in three leaching media: seawater, a Na2SO4 solution (4% by mass) and deionized water. For this, pastes of prismatic specimens of MKPC, prepared with different M/P ratio (2 and 3), were submitted to the different chemical attacks. At different ages, the changes on the mechanical strengths, microstructure (BSEM, MIP) and mineralogy (XRD, FTIR, TG/DTG) were evaluated. The results obtained indicate that, in general terms, MKPC systems show good behavior in the three media, with the more resistant system being the one prepared with a M/P molar ratio of 3., The JIN project (PID2020-116738RJ-I0 AEI/10.13039/501100011033) and the RYC excellence contract (RYC2021-032620-I), funded by the Spanish Ministry of Science and Innovation (MCIN/AEI/10.13039/50110001033) and the European Union “Next generation EU/PRTR”. Institutional Review Board Statement, Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Acid resistance of alkali-activated binders based on clays from phosphate mining by-products

  • Mabroum, Safaa
  • García-Lodeiro, Inés
  • El Machi, Aiman
  • Chhaiba, Salma
  • Taha, Yassine
  • Benzaazoua, Mostafa
  • Blanco-Varela, María Teresa
  • Hakkou, Rachid
This paper outlines the results of studying the resistance of alkali-activated materials (AAM), based on calcined yellow clay from phosphate mine by-products as a precursor, to an acid attack (with sulfuric and phosphoric acids, 5 %, pH ≈ 0,8–2). Calcined yellow clay (YC850) is used as the source of aluminosilicates, containing montmorillonite, dolomite, and quartz. The alkali-activation of such materials allows the determination of an adequate valorization way and evaluating their durability leads to defining the range of application. The residual compressive strengths were measured after 1, 2, and 4 weeks of immersion in those acids. The deterioration suffered by the paste specimens was examined using different techniques., The degree of deterioration differs from one acid to another; in sulfuric acid, the strengths decrease from 47 MPa to 10.6 MPa presenting 77.4 %. While in phosphoric acid, the decrease was about 36.2 % (30 MPa) after 28 days of attack. This detriment in the strengths is associated with changes not only in the microstructure but also with the alteration of the reaction products, mainly the binding gels C-A-S-H and (C,N)-A-S-H, which undergoes dealumination and decalcification. What is more, the chemical attack involves several reactions; calcium coming from the precursor reacts with the sulfates (in the H2SO4 attack) inducing the precipitation of gypsum, which is responsible for the significant strength loss. In addition, the dissolution of crystalline minerals, such as periclase and gehlenite (present in the precursor) generates higher porosity explaining the obtained results., The authors are acknowledged the concession of the project ICOOP +2020 (ref COOPA20454 funded by the CSIC) and to the Spanish Agency: AGENCIA ESTATAL DE INVESTIGACIÓN (JIN Projects 2021 PID2020-116738RJ-I00/AEI/10.13039/501100011033) and the RYC Excellence Contract (RYC2021-032620-I, MCIN/AEI/10.13039/50110001033). This work was supported by OCP-SA, Morocco, under the specific agreement OCP/UM6P #AS03., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

Durability of Magnesium Potassium Phosphate Cements (MKPCs) under Chemical Attack

  • Chhaiba, Salma
  • Martínez-Sánchez, Sergio
  • Husillos Rodríguez, N.
  • Palomo, Ángel
  • Kinoshita, Hajime
  • García-Lodeiro, Inés
Six replicates per series were used to determine the compressive strengths. Testing was conducted using an Ibertest Autest 200/10-SW (Madrid, Spain) test frame, the average and standard deviation of the results were then calculated and reported. Prior to microstructural characterization (Mercury Intrusion Porosimetry (MIP) and Scanning Electron Microscopy with Energy Dispersive X-ray Analysis (BSEM/EDX), one of the specimens, left unbroken, is submitted to immersion in isopropanol for 2 days to stop further hydration reactions. Subsequently, they were dried in a desiccator for a minimum of 48 h to eliminate any residual isopropanol. To prepare the powder samples (for the mineralogical analysis), specimen fragments were ground to pass through a 63 μm sieve as per previous recommendations to stop the reaction processes. Subsequently, they were mixed with isopropanol for 3 min, filtered and placed in a vacuum desiccator until a constant weight was attained. Changes in the pore structure were evaluated by mercury intrusion porosimetry (MIP) on a Micromeritics Poresize 9320 IV.09 mercury intrusion porosimeter (Micromeritics Instrument Corporation, Norcross, GA, USA), assuming a sample–mercury contact angle of 140◦. The microstructure of the samples was studied by Backscattering Electron Microscopy (BSEM) on a JEOL JSM6400 scanning electron microscope (Tokyo, Japan). Additionally, a semi-quantitative analysis of the chemical composition of the reaction products was conducted via Energy Dispersive X-ray spectroscopy (EDX) on a Links ISIS EDX analyzer, collecting at least 40 points from the cementitious matrix per sample; the data were processed using the Bruker ESPRIT 1.9 software, whereas the mineralogical and chemical composition of samples were studied via X-ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR) and Thermogravimetric analysis (TG/DTG). XRD measurements were carried out on a Bruker D8 Advance diffractometer (Karlsruhe, Germany) in a 2θ range of 5–60◦ with a step size of 0.02◦ every 0.5 s using CuKα radiation at 40 kV and 30 mA. The existing phases were identified and quantified using the DiffracPlus EVA 4 2.1 and TOPAS 5.0 software, in conjunction with a chemical reconciliation. A Nicolet 6700 spectrometer (Thermo Fisher Scientific, Waltham, MA, USA, 02451) was employed for FTIR analysis, covering a range of 400 cm−1 to 4000 cm−1 with a resolution of 4 cm−1, using powdered samples embedded in KBr pellets (0.001 g sample/ 0.099 g KBr). Thermogravimetric analysis (TGA) was conducted using a Perkin-Elmer TG analyzer (PerkinElmer, Shelton, USA). Powdered samples underwent heating from room temperature to 800 ◦C at a rate of 10 ◦C min−1 under a N2 flow of 200 cm3/min., [EN] This is the experimental dataset used in the paper Materials 17, 4252 (2024) (https://doi.org/10.3390/ma17174252) Durability of magnesium potassium phosphate cements (MKPCs) pastes during 1 year of inmersión under chemical attack, focusing on the effects of deionized water, sodium sulfate and seawater, have been determined with different analytical tecnhiques. Prismatic specimens (1 × 1 × 6 cm3) of MKPC were prepared with different MgO/H2PO4 ratio (2 and 3), at different ages, cured under two curing conditions (CC and LAB), where were maintained up to 28 days: - CC: In a climatic chamber at 21 ± 3 ◦C and 99 ± 5% relative humidity (RH). - LAB: In the laboratory at 21 ± 3 ◦C and 52 ± 5% of relative humidity (RH). After these 28 days, three set of samples, for each curing regime, were prepared. One additional set was used as a reference (only cured for 28 days). Changes in the mechanical strengths, mineralogy (XRD, FTIR, TG/DTG), and microstructure (BSEM, MIP) of all 4 sets were determined., We acknowledge financial support from the JIN project (PID2020-116738RJ-I0 AEI/10.13039/501100011033) and the RYC excellence contract (RYC2021-032620-I), funded by the Spanish Ministry of Science and Innovation (MCIN/AEI/10.13039/50110001033) and the European Union “Next generation EU/PRTR”., COMPRESSIVE STRENGHTS folder: C S M-P-(2-3) H2O; C S M-P-(2-3) SO4 ; C S M-P-(2-3) SW. MIP folder: porosimetry_readme; M-P 3 CC 28d (Ref 0); M-P 3 LAB 28d (Ref 0); M-P 3 CC 28d H2O; M-P 3 CC 28d SO4; M-P 3 CC 28d SW; M-P 3 CC 90d H2O; M-P 3 CC 90d SO4; M-P 3 CC 90d SW; M-P 3 CC 180d H2O; M-P 3 CC 180d SO4; M-P 3 CC 180d SW; M-P 3 CC 1y H2O; M-P 3 CC 1y SO4; M-P 3 CC 1y SW; ); M-P 3 LAB 28d H2O; M-P 3 LAB 28d SO4; M-P 3 LAB 28d SW; M-P 3 LAB 90d H2O; M-P 3 LAB 90d SO4; M-P 3 LAB 90d SW; M-P 3 LAB 180d H2O; M-P 3 LAB 180d SO4; M-P 3 LAB 180d SW; M-P 3 LAB 1y H2O; M-P 3 LAB 1y SO4; M-P 3 LAB 1y SW. TG-DTG folder: TG-DTG_readme; loss of water; TG-DTG M-P 3 CC 28d, 1 year. XRD folder: XRD_readme; M-P 3 CC 28d H2O; M-P 3 CC 28d SO4; M-P 3 CC 28d SW; M-P 3 CC 90d H2O; M-P 3 CC 90d SO4; M-P 3 CC 90d SW; M-P 3 CC 180d H2O; M-P 3 CC 180d SO4; M-P 3 CC 180d SW; M-P 3 CC 1year H2O; M-P 3 CC 1year SO4; M-P 3 CC 1year SW. FTIR folder: FTIR_readme; FTIR M-P 3 CC Ref, 28d, 1y. SEM-EDX folder: BSEM-EDX_readme; mapping M-P 3 CC-REF; mapping M-P 3 CC-H2O; mapping M-P 3 CC-SO4; mapping M-P 3 CC-SW; SEM M-P 3 CC H2O a; SEM M-P 3 CC H2O b; SEM M-P 3 CC SO4 a; SEM M-P 3 CC SO4 b; SEM M-P 3 CC SW a; SEM M-P 3 CC SW b; EDX M-P-3 28d; EDX M-P-3 1y. WATER COMPOSITION folder, Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Datos de investigación Set de datos (Dataset)

Encapsulation of polucite in magnesium phosphate cement (MKPC)

  • Husillos Rodríguez, N.
  • Chhaiba, Salma
  • Kinoshita, Hajime
  • Palomo, Ángel
  • García-Lodeiro, Inés
Pollucite, (Cs(Si2Al)O6·nH2O), has long been considered one of the most stable and suitable mineral forms for the immobilization of radioactive cesium over time, due to its good thermal stability, its low leaching rate (high resistance to leaching) and the fact that it has a dense and stable structure through its strong covalent bonds. But even if Cs is fixed in a chemically stable form (pollucite), this form is still classified as intermediate level waste (ILW) and must therefore be safely encapsulated in a cementitious matrix. For this purpose, magnesium phosphate cement pastes (MKPC) have been designed with the incorporation of pollucite, in a proportion of 0 and 10 %. The effect of the incorporation of the pollucite on the mineralogy and microstructure of the MKPC systems was analysed from the mechanical and mineralogical point of view. Mechanical compressive strengths (1, 7, 28 and 90 days), as well as mineralogical and microstructural changes in presence of pollucite (XRD, ATD/TG, Hg porosimetry and BSEM) were analysed. Finally, the confining capacity of this matrix has been determined after 90d of leaching (ANSI/ANS-16.1-2003)., Peer reviewed