Publication Artículo científico (JournalArticle)

Hydraulic fracture behavior in the presence of hydrogen in notched miniature cylindrical specimens of a 42CrMo4 steel

  • Peral, Luis Borja
  • Díaz Portugal, Andrés
  • Arniella, V.
  • Belzunce, J.
  • Alegre Calderón, Jesús Manuel
  • Cuesta Segura, Isidoro Iván
The influence of internal hydrogen on the mechanical behavior of the 42CrMo4 steel grade has been evaluated by means of internal pressure fracture tests performed on hydrogen precharged notched cylindrical specimens. The notched cylindrical specimens were precharged in a 1 M H2SO4 solution + 0.25 g/l As2O3 for 3 h and 1.2 mA/cm2. Thereupon, hydraulic fracture tests were done under different ramps of pressure: 208, 100, 52, 35 and 25 MPa/h, respectively. Hydrogen content introduced into the notched cylindrical specimens (∼1 ppm) was determined by thermal desorption analysis (TDA), using a LECO DH 603 hydrogen analyser. Hydrogen damage was observed as testing time increased until 2 h. The burst pressure is reduced around 28 % while the Notch Mouth Opening Displacement decreased around 50 %. Hydrogen embrittlement susceptibility is discussed through the hydrogen embrittlement micromechanisms., The authors would like to thank the Spanish Government for the financial support received to perform the research projects RTI2018-096070-B-C33 and PID2021-124768OB-C21. L.B. Peral is grateful for his Margarita Salas Postdoctoral contract (Ref.: MU-21-UP2021-030) funded by the University of Oviedo through the Next Generation European Union.
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publication Artículo científico (JournalArticle)

Parameter Optimisation in Selective Laser Melting on C300 Steel

  • Cuesta Segura, Isidoro Iván
  • Díaz Portugal, Andrés
  • Rojo, M. A.
  • Peral, Luis Borja
  • Martínez, J.
  • Alegre Calderón, Jesús Manuel
Additive manufacturing (AM) of metallic materials is increasingly being adopted in numerous sectors, such as biomedicine, aerospace or automotive industries, due to its versatility in the creation of complex geometries and the minimisation of material waste when compared to traditional subtractive methods. In order to ensure a reliable operation of these parts, however, an in-depth study of the effect of additive manufacturing on mechanical properties, including tensile, fatigue and fracture resistance, is necessary. Among the vast number of methods and materials, this project is focused in one of the most promising techniques for the industry: Selective Laser Melting (SLM) for the production of a tools steel, in particular C300 steel components for the automotive sector. The main objective of this paper is to optimise some of the key parameters in the printing process, such as laser power, laser speed and hatch spacing. These variables are essential to obtain parts with good resistance. To that purpose, tensile tests were performed in 3D printed specimens, and then elastoplastic properties were extracted, organised and analysed through a design of experiments for the subsequent output fitting using the response surface methodology., This research was funded by: INVESTUN/22/BU/0003 // BU-002-P20 // MU-21-UP2021-030.
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publication Artículo científico (JournalArticle)

Hydrogen uptake and diffusion kinetics in a quenched and tempered low carbon steel: experimental and numerical study

  • Peral, Luis Borja
  • Díaz Portugal, Andrés
  • Alegre Calderón, Jesús Manuel
  • Cuesta Segura, Isidoro Iván
To better understand hydrogen uptake kinetics, electrochemical permeation tests have been performed in a quenched and tempered low-alloy steel. Hydrogen uptake and transport has been studied with three different surface roughness, in four different solutions (1 M H2SO4, 1 M H2SO4+As2O3, 0.1 M NaOH and 3.5% NaCl) and two different hydrogen charging current densities (1 and 5 mA/cm2). A strong effect of the charging solution, current density and surface roughness has been demonstrated. In 1 M H2SO4 + As2O3 solution and 5 mA/cm2, hydrogen recombination on the surface of the samples is strongly reduced and interstitial diffusion prevails due to the trap saturation ( ). However, in 1 M H2SO4, 0.1 M NaOH and 3.5% NaCl, hydrogen transport is dominated by trapping and detrapping processes ( ). Permeation transients are numerically reproduced through Finite Element simulations and compared to the experimental results. The relationship between hydrogen diffusion kinetics at the microstructural level and surface effects is clearly established by a mapping strategy obtained from the wide range of experimental results, combined with a numerical approach., The authors would like to thank the Spanish Government for the financial support received to perform the research projects RTI2018-096070-B-C33 and PID2021-124768OB-C21. This work was supported by the Regional Government of Castilla y León (Junta de Castilla y León) and by the Ministry of Science and Innovation MICIN and the European Union Next Generation EU/PRTR (MR4W.P2 and MR5W.P3). L.B. Peral is also grateful for his Margarita Salas Postdoctoral contract (Ref.: MU-21-UP2021-030) funded by the University of Oviedo through the Next Generation European Union.
Repositorio Institucional de la Universidad de Burgos (RIUBU)
Publication Artículo científico (JournalArticle)

Influence of hydrogen on the hydraulic fracture behavior of a 42CrMo4 steel welds: Effect of the prior austenite grain size

  • Peral, Luis Borja
  • Díaz Portugal, Andrés
  • Arniella, V.
  • Belzunce, J.
  • Alegre Calderón, Jesús Manuel
  • Cuesta Segura, Isidoro Iván
The influence of hydrogen on the mechanical behavior of a quenched and tempered 42CrMo4 steel has been evaluated by means of high internal pressure fracture tests carried out on hydrogen precharged notched cylindrical specimens. The notched cylindrical specimens were precharged in a 1 M H2SO4 + 0.25 g/l As2O3 solution for 3 h with 1.2 mA/cm2. Hydraulic fracture tests were performed at different loading rates. Hydrogen embrittlement resistance increased with grain size refinement although the fine grained specimen had a higher hydrogen content than the coarse grained one. Fractographic analysis showed hydrogen enhanced decohesion fracture was less pronounced with decreasing grain size. Hydrogen embrittlement susceptibility is discussed in terms of the prior austenite grain size (PAGS) and the operative fracture mechanisms., The authors would like to thank the Spanish Government for the financial support received to perform the research projects TED2021-130413B-I00 and PID2021-124768OB-C21. This work was supported by the Regional Government of Castilla y León (Junta de Castilla y León) and by the Ministry of Science and Innovation MICIN and the European Union Next Generation EU/PRTR (MR5W.P3) and PRTR (MR4W.P2). L.B. Peral is grateful for his Margarita Salas Postdoctoral contract (Ref.: MU-21-UP2021-030) funded by the University of Oviedo through the Next Generation European Union.