RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publication Artículo científico (JournalArticle)

Understanding the thermal and dielectric response of organosolv and modified kraft lignin as a carbon fibre precursor

  • Culebras, Mario
  • Beaucamp, Anne
  • Kandola, Baljinder K.
  • Horrocks, A. Richard
  • Panzetti, Gianmarco
  • Birkinshaw, Colin
  • Collins, Maurice N.
  • Sanchis Sánchez, María Jesús|||0000-0002-3528-3966
  • Carsí Rosique, Marta|||0000-0003-2315-3344
[EN] Understanding the thermal behaviour of lignin is crucial in order to realise its valorisation as an engineering polymer. Two hardwood lignins, organosolv (OSL) and chemically modified kraft lignin (ML) have been chosen to represent important classes of renewable and abundant raw materials. The relationship between ionic mobility and viscosity in OSL and ML has been studied. The rheological results have been interpreted in terms of the competitive processes of thermal plasticisation and stiffening through crosslinking. Results show that with OSL, crosslinking proceeds relatively rapidly, and this is consistent with its more reactive structure. Higher molecular weight (M-w) influenced the melt stability as cross-linking kinetics was reduced and this was attributed to the reduction of chain ends available for cross-linking reactions. Scanning calorimetry has shown that both materials are glassy and pass through the glass transition between 100 degrees C and 115 degrees C, with the higher molecular weight modified material having a slightly higher T-g. Both lignins show pronounced maxima in the Gram-Schmidt plots for methane or methanol around 400 degrees C. However, a significant difference between the materials is observed with the detection of a strong carbonyl peak in the evolution products of the ML, which is attributed to the scission of the hydroxypropyl substituent present in the ML structure. The differences in the degradation processes are further reflected in the dielectric properties of the partially degraded materials where loss maxima occur at different temperatures and show different degrees of frequency dependence. An important observation is the difference in conductivity, where higher values for OSL are attributed to the cross-linking between adjacent benzene rings, whereas with the ML, a lower conductivity is associated with intrinsically less conductive intermolecular linkages. These results demonstrate that the thermal decomposition of the two lignins follows significantly different paths at the molecular level. With the more reactive OSL, it appears to be the case that there is a greater tendency to form direct ring to ring crosslinks and this is very significant for the properties of the intended end product., Mario Culebras, Anne Beaucamp, Baljinder K. Kandola, A. Richard Horrocks, Gianmarco Panzetti and Maurice N Collins acknowledge the funding received from the BioBased Industries Joint Undertaking under the European Union's Horizon 2020 research and innovation programme grant agreement no. 720707. MC and MJS are thankful to the Spanish Ministerio de Economia y Competitividad (MAT2015-63955-R) for the partial financial help.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publication Artículo científico (JournalArticle)

Exploring the role of lignin structure inmolecular dynamics of lignin/bioderived thermoplastic elastomer polyurethane blends

  • Ortiz Serna, Mª Pilar
  • Carsí Rosique, Marta|||0000-0003-2315-3344
  • Sanchis Sánchez, María Jesús|||0000-0002-3528-3966
  • Culebras, M.
  • Collins, M. N.
[EN] The relaxation behavior of two lignins (Alcell organosolv, OSL, and hydroxypropyl modified Kraft, ML) and biobased thermoplastic polyurethane (TPU) blends have been studied by Differential scanning calorimetry (DSC), Dynamic-mechanical analysis (DMA) and Dielectric relaxation spectroscopy (DRS). The effect of blending on the glass and local relaxation processes as a function of composition, frequency, and temperature has been assessed. The dielectric spectra were resolved into dipolar relaxations as well as conductive processes for differing blend compositions. Characteristic relaxation times, activation energies and dielectric relaxation strengths of lignin/xTPU blends were also investigated. It was found that blending suppresses the alpha-relaxation process of the blends compared to virgin TPU. On the other hand, while the position of the beta-relaxation was not influenced by blending, a reduction of the activation energies, E-a, of this process was observed in the lignin/xTPU blends. Finally, changes are observed in the conductivity behavior of both blends, with conductivity processes more favorable for the OSL/xTPU blends., M. Carsi and M.J. Sanchis thank the Spanish Ministerio de Economia y Competitividad (RTI2018-093711-B-I00) for partial financial help. M. Culebras and M. N Collins acknowledge received funding from the BioBased Industries Joint Undertaking under the European Union's Horizon 2020 research and innovation programme under grant agreement no. 720707.