Skip to main content

Procesamiento Coloidal y Caracterización de Semiconductores Cerámicos

IJCI-2016-28538

•
Funding agency name Agencia Estatal de Investigación
Funding agency acronym AEI
Program Programa Estatal de Promoción del Talento y su Empleabilidad en I+D+i
Subprogram Subprograma Estatal de Incorporación
Call Juan de la Cierva Incorporación
Call year 2016
State Plan 2013-2016 Plan Estatal de Investigación Científica y Técnica y de Innovación
Beneficiary centre AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 4
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Effect of SrR delivery in the biomarkers of bone regeneration during the in vitro degradation of HNT/GN coatings prepared by EPD

  • Abdollahi Boraei, S. B.
  • Nourmohammadi, J.
  • Sadat Mahdavi, F.
  • Yus, Joaquín
  • Ferrández-Montero, Ana
  • Sánchez-Herencia, A. Javier
  • González Granados, Zoilo
  • Ferrari, Begoña
[EN] Among strontium-based drugs, the Strontium ranelate (SrR) is a divalent strontium salt of ranelic acid which has an overall effect over the bone microarchitecture improvement. However, some findings reveal that the SrR affects in an opposite manner to the cell proliferation and osteoblastic differentiation, based on its concentration. Consequently, its release should be controlled. The incorporation of Halloysite nanotubes (HNT) as nanocarriers of SrR, into gelatine (GN) coatings, tailors the release of this anabolic bone-forming and anti-catabolic agent to stimulate bone growth. In fact, as-prepared GN/HNT-SrR coatings release 100 % SrR in phosphate buffered saline (PBS) within 21 days, and cellular studies of the nanocomposite coatings (MTT, Alkaline Phosphatase activity (ALP) and Calcium deposition assay) confirm the valuable bio-performance of these composite coatings to enhanced bone regeneration. In the present manuscript, suspensions with HNT/GN weight ratio of 0.5 are formulated to coat AISI 316 L stainless steel foils by Electrophoretic Deposition (EPD). Zeta potential determination is used to stablish the drug loading (HNT-SrR) by electrostatic interaction, as well as to optimize the dispersion of bare HNT and HNT SrR-loaded in a GN aqueous solution. Polyethilenimnine (PEI) is used as stabilizer to buffer the suspension media, assure cargo-drug dispersion and sequential release, while the thermal gelling of the suspension controls and step up the coating formation during EPD., The authors would like to thank the University of Tehran, Tehran, Iran for support and technical assistance, and the financial support of Comunidad de Madrid: ADITIMAT: S2018/NMT-4411, and M-ERA.NETPCIN-2017-036 and IJCI-2016-28538 (MICINN, Spain).
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Heteroacoagulation of lignocellulose fibers-based biotemplates and functionalized TiO2 nanoparticles to tailor film microstructures

  • González Granados, Zoilo
  • Yus, Joaquín
  • Bravo, Yessica
  • Sánchez-Herencia, A. Javier
  • Rodríguez, Alejandro
  • Dewalque, Jennifer
  • Manceriu, Laura
  • Henrist, Catherine
  • Ferrari, Begoña
[EN] The heterocoagulation of lignocellulose nanofibers (LCNFs) with functionalized TiO nanoparticles (NPs) is presented as an innovative revalorization strategy for the exploitation of lignocellulose wastes. Their use as bio-templates could be considered a promising alternative in a current biorefinery scheme, since the massive production of porous materials in numerous nanotechnological applications, could offer new alternatives of exploitation. The surface modification of TiO NPs by adsorption of polyetilenimine (PEI) favors its anchorage with LCNFs through a peptide bond during heterocoagulation in aqueous suspension. The functionalization of LCNFs with TiO NPs results in organic–inorganic core–shell nanostructures, used to shape coatings by dipping, and sinter them at low temperature (450 °C). In this process, the LCNFs were used as endo-templates for shaping stable porous coatings, when they burn during the consolidation of the inorganic structure. In this work, the successful inclusion and homogeneous distribution of biomaterials (LCNF templates) in the semiconductor inorganic microstructure is discussed in terms of dye loading (by UV–Visible Spectroscopy), photovoltaic efficiency and charge transfer (by Electrochemical Impedance Spectroscopy, EIS) in a Dye Sensitized Solar Cell (DSSC). Results confirm that the TiO/template network yielded better photoefficiency and electron transport properties than mesoporous films assembled only from TiO NPs. The preparation of TiO-based photoanodes with enhanced performance (with an efficiency value around 6%, for a thickness of 8.7 µm) allows validating the successful colloidal procedure herein employed., The authors thank the support to the projects S2018/NMT-4411 (Comunidad de Madrid) and MAT2015-70780-C4-1 (MINECO/FEDER). Z. Gonzalez acknowledges to the European Ceramic Society for the funds of the ‘‘Frontiers of Research’’ program and also to the Spanish Ministry of Economy and Competitiveness for the Postdoctoral Fellowship: IJCI-2016-28538
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Understanding the effects of different microstructural contributions in the electrochemical response of Nickel-based semiconductor electrodes with 3D hierarchical networks shapes

  • Yus, Joaquín
  • Ferrari, Begoña
  • Sánchez-Herencia, A. Javier
  • González Granados, Zoilo
[EN] It is well known that exposed surface area, nanoparticles connectivity and its consolidation level in a nanostructure are key points in the enhancement of the electrochemical performance in energy storage devices. The design and optimization of different electrodes with specific microarchitectures (based on the arrangement manipulation of NiO nanoplatelets, used as building blocks), has allowed distinguishing the effects of each microstructural contribution in their final electrochemical responses, overpassing thermal and mechanical mismatches between the semiconductor ceramic structure and the metallic collector. In all cases, the same electroactive material and the same coating technique were used, preventing the interference of secondary phenomena in the EIS studies, and allowing argue over the contribution of the microstructural features incorporated to the electrode (nature and shape of the collector, degree of sintering and consolidation of the ceramic microstructure, incorporation of non-noble metallic nanoparticles and the macro/meso/microposity effect) in the effective profiting of the Faradaic phenomena observed during their cycling. The modification of the Ni-based electrodes allows understanding how microstructural features infer the electron transport and the ion diffusion through the consolidated structure. The EIS analysis proves that the design of the porous hierarchical network of our semiconductors electrodes resulted in a good rate capability (with capacitance values of 1000 F g¿1 or 500 C g¿1), exhibiting a relaxation time constant (¿0 = 18 ms), while a slight increase of the charge-transfer resistance (Rct = 3.65¿) is negligible if the exposed surface is high enough to maintain a high ion transport. The inclusion of non-noble nanoparticles, such as Ni NPs, in the NiO semiconductor microstructure and the optimum deposited mass and sintering treatment create a metal-ceramic electrode that enhances both the charge transfer resistance (1.55 ¿) showing relaxation time in the range (¿0 = 11 ms) and maintaining an excellent capacitive behavior (750 F g¿1 or 375C g¿1) at quick charge/discharge rate., 2018/NMT-4411(Comunidad de Madrid, Spain) and MAT2015-70780-C4-1(MINECO/FEDER, Spain). J. Yus acknowledges the Comunidad de Madrid for the support from the Youth Employment Initiative,CAMPD17_ICV_002. Z. Gonzalez acknowledges the Postdoctoral Fellowship: IJCI-2016-28538 (MINECO, Spain)
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Tesis doctoral (DoctoralThesis)

Aqueous colloidal processing of W and WC-based composites, sintering and mechanical properties at high temperature

  • García Ayala, Esperanza Macarena
E. M. Garcia-Ayala, Z. Gonzalez, B. Ferrari, J. Y. Pastor, A. J. Sanchez-Herencia, Colloidal Approach to the Additive Manufacturing of W-based Materials, in: EuroPM 2018 Proceedings (2020) ISBN: 978-1-899072-50-7. E.M. Garcia-Ayala, S. Tarancon, B. Ferrari, J.Y. Pastor, A.J. Sanchez-Herencia, "Thermomechanical behaviour of WC-W2C composites at first wall in fusion conditions", Int. J. Refract Metal. Hard Mater., 98 105565 (2021). DOI: 10.1016/j.ijrmhm.2021.105565 E.M.Garcia-Ayala, L.Silvestroni, J.Yus, B.Ferrari, J.Y.Pastor and A.J.Sanchez-Herencia"Colloidal processing and sintering of WC-based ceramics with low Ni content as sintering aid", J. Eur. Ceram. Soc, 41 (3) 1848, -1858 (2021).DOI: 10.1016/j.jeurceramsoc.2020.10.038 M.E. Garcia-Ayala, S. Tarancon, Z. Gonzalez, B. Ferrari, J.Y. Pastor, A.J. Sanchez-Herencia, "Processing of WC/W composites for extreme environments by colloidal dispersion of powders and SPS sintering",Int. J. Refract. Met. Hard Mater., 84,105026 ( 2019,)DOI:10.1016/j.ijrmhm.2019.105026, [EN] There have been many advanced technologies that operates at high temperature under severe conditions, such as those over the inner walls of the future fusion nuclear reactor (ITER, DEMO, etc.). Refractory metals such as tungsten are proposed as optimum materials to face these conditions. Pure ceramics, such as WC and metal ceramics are proposed also as alternative materials for the components that require operate at high temperature under high wear conditions or neutronic damage. For that reason, the design of complex compositions and microstructures is necessary to achieve reliable materials under these conditions. That makes this work investigate on colloidal processing W and WC materials, as well as their composites with nickel for softening of the sintering conditions. Aqueous colloidal processing is proposed as an alternative to the solvent-less techniques. By the study of zeta potential and chemical analysis of powders suspended in water the optimal conditions for high solid content suspension preparation were determined at different pH conditions and considering the use a cationic dispersant (polyethyleneimine, PEI). The rheological studies have determined the maximum solid content through the Krieger-Dougherty model adjustment, so the time spent removing water after powder preparation can be diminished. Three different types of composite powders were prepared: WC-W, WC-Ni and W-Ni. For WC-W composites, the amount of metallic phase was fixed in 10, 20 and 50 vol.%, while for WC-Ni and W-Ni mixtures, the amount of metallic nickel phase was 5 vol.% (3 wt.%). Three different sintering methods are used: Spark Plasma Sintering (SPS), Hot-Press Sintering (HPS) and Vacuum Sintering (VS). WC-W materials were sintered by SPS at 1700 and 1800 oC for 10 min and 60 MPa. The crystalline and chemical studies determined the high reactivity between W and WC during the thermal cycle, which gives place to the presence of a third species: tungsten semicarbide (W2C), which provoked all the W consumption. Mechanical tests at high temperatures for the W2C/WC composites demonstrated their excellent properties and performance at conditions similar to the ITER divertor walls. A self-reinforcement behaviour due to the appearing of metallic tungsten in the microstructure as the temperature approach to 1200 ºC is described. On the other hand, mixture of WC with Ni and W with Ni, obtained by aqueous colloidal processing were sintered by the three mentioned sintering techniques and the differences between them studied. Two types of Ni powders were used: a commercial nickel (cNi) and a nanometric nickel synthesized in the lab (nNi). WC-Ni sintered by HPS achieved a density higher than 98%, which was not the case of SPS and VS sintered samples. SEM/EDX observations demonstrated that sintering was by a solution-precipitation mechanism that leaved the nickel located in the grain junctions, while there were slight carbon precipitations favoured by the thermodynamical conditions during the thermal cycle. For W-Ni alloys, successful results were obtained from VS process, achieving 96% density and a fully dense microstructure. In this case, W and Ni reacts while thermal treatment, giving an intermetallic species: NiW. For both WC-Ni and W-Ni materials, the presence of small amounts of Ni showed a clear softening of sintering conditions, which make the sintering of W and WC an affordable method for wide productions in terms of both technology and economic cost. Mechanical tests of these composites exhibited a ductilisation of the materials due to the presence of the nickel phase, which matches to the data found in the literature for this type of composites and alloys., [ES] Existen multitudes de tecnologías avanzadas capaces de operar a alta temperatura bajo condiciones severas, como aquellos que conforman las paredes interiores de futuros reactores de fusión nuclear (ITER, DEMO, etc.). Los metales refractarios como el wolframio se proponen como los materiales óptimos para trabajar bajo estas condiciones. Los cerámicos puros, como el WC, y los composites cerámica-metal (cermets) también se presentan como claras alternativas para aquellos materiales requeridos para operaciones a alta temperatura, bajo alto desgaste o radiación neutrónica. Por este motivo, el diseño de composiciones complejas y microestructuras es necesario para lograr la preparación de materiales que trabajen en dichas condiciones. Todo ello hace que se profundice en la Investigación de materiales de W y WC formulados por procesamiento coloidal, así como sus materiales compuestos con níquel metálico para suavizar sus condiciones de sinterización. El procesamiento coloidal en base acuosa se propone como una fuerte alternativa a las tradicionales técnicas sin disolvente (en seco). Mediante el estudio del potencial zeta y el análisis químico de los polvos suspendidos en agua, las condiciones óptimas para la preparación de suspensiones con alto contenido en sólidos se determinaron a diferentes valores de pH, y considerando el uso de un dispersante catiónico (polietilenimina o PEI). Los estudios reológicos determinaron el máximo contenido en sólidos mediante el ajuste de Krieger-Dougherty, de tal forma que se lograba disminuir el tiempo de eliminación de disolvente. Se prepararon tres tipos diferentes de polvos compuestos: WC-W, WC-Ni y W-Ni. Para los composites WC-W, la cantidad de fase metálica se fijó en 10, 20 y 50 vol.%, mientras que para las mezclas WC-Ni y W-Ni, la cantidad de níquel metálico fue de un 5 vol.% (3% en peso). Se emplearon tres métodos distintos de sinterización: Sinterización asistida por Corriente Pulsada (SPS), Sinterización por presión asistida en caliente (HPS) y Sinterización a vacío (VS). Los materiales de WC-W se sinterizaron por SPS a 1700 y 1800 oC durante 10 minutos, a 60 MPa de presión. Los estudios químicos y de cristalinidad determinaron la alta reactividad entre W y WC durante el ciclo térmico, el cual dio lugar a la aparición de una tercera especie: el semicarburo de wolframio (W2C), lo que provocó el agotamiento total del wolframio metálico. Los ensayos mecánicos a alta temperatura para los compuestos W2C/WC demostraron sus excelentes propiedades a condiciones similares a las del divertor del ITER. Se describe un comportamiento de refuerzo mecánico debido a la aparición de wolframio metálico en la microestructura, a medida que se describe un ascenso de la temperatura hasta los 1200 oC. Por otra parte, las mezclas de WC con Ni, y W con Ni, obtenidas mediante procesamiento coloidal en agua, se sinterizaron a través de las tres técnicas ya mencionadas, por lo que se estudiaron los diferentes resultados. Se usaron dos tipos de polvo de Ni: un níquel comercial (cNi), y un níquel nanométrico sintetizado en el laboratorio (nNi). WC-Ni se sinterizó por HPS, logrando una densidad mayor al 98%, lo que no ocurrió en el caso de las muestras sinterizadas por SPS y VS. Los análisis por SEM/EDX demostraron que la sinterización seguía un mecanismo de disolución-precipitación, lo que provocó la localización del níquel metálico en los límites de grano, mientras que aparecieron algunas precipitaciones de grafito favorecidas por las condiciones termodinámicas durante el ciclo térmico. Para las aleaciones W-Ni, se obtuvieron resultados bastante exitosos para el proceso de sinterización a vacío (VS), alcanzando densidades superiores al 96%, así como una microestructura consolidada y totalmente densificada. En este caso, W y Ni reaccionan durante el tratamiento térmico, dando lugar a una nueva especie: el intermetálico NiW. Para ambos composites WC-Ni y W-Ni, la presencia de pequeñas cantidades de Ni mostró un claro suavizamiento de las condiciones de sinterización, lo que hace que la sinterización de W y WC se conciba como un método asequible para grandes producciones a escala industrial en términos tanto tecnológicos como económicos. Los ensayos mecánicos de estos materiales exhibieron una clara ductilización debido a la presencia de fase níquel, lo que coincide con los datos encontrados en la literatura para este tipo de composites y aleaciones., Esta tesis se enmarca en el proyecto MAT2015-70780-C4-1-P del plan nacional, titulada “Procesamiento coloidal en medio acuoso de composites en base W y WC, sinterización y propiedades mecánicas a alta temperatura”. Este trabajo se ha desarrollado combinando las principales líneas de investigación de los dos grupos en los cuales se ha llevado a cabo el trabajo experimental: la Química Coloidal desarrollada por el grupo Tailoring through Colloidal Processing (ICV-CSIC), y el conocimiento sobre propiedades mecánicas del grupo CIME (UPM).