Skip to main content

FLEXIBILIDAD NANO-ESTRUCTURAL Y PROPIEDADES MAGNETICAS, OPTICAS Y CATALITICAS EN OXIDOS METALICOS MULTIFUNCIONALES

MAT2014-57547-R

•
Funding agency name Ministerio de Economía y Competitividad
Funding agency acronym MINECO
Program Programa Estatal de I+D+i Orientado a los Retos de la Sociedad
Call Proyectos I+D+i Retos de Investigación
Call year 2014
State Plan 2013-2016 Plan Estatal de Investigación Científica y Técnica y de Innovación
Management unit Secretaría de Estado de Educación, Formación Profesional y Universidades
Beneficiary centre AGENCIA ESTATAL CONSEJO SUPERIOR DE INVESTIGACIONES CIENTIFICAS (CSIC)

Resultados relacionados

Resultados totales (Incluyendo duplicados): 6
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Lattice damage in 9-MeV-carbon irradiated diamond and its recovery after annealing

  • Agulló Rueda, F.
  • Gordillo, N.
  • Ynsa, M. D.
  • Maira-Vidal, Aránzazu
  • Cañas, J.
  • Ramos, M. A.
We have studied the radiation damage in diamond as a function of layer depth upon self-ion implantation with 9-MeV carbon ions and its recovery after annealing at 1000◦C. Raman and photoluminescence spectra show substantial damage of the lattice, namely, amorphization, neutral vacancies, and interstitial defects. Damage is maximum in the stopping layer at a depth of 4 μm. After annealing there is some recovery of the lattice, but the residual damage increases with fluence, up to about 2×10^16 ions/cm2. At this fluence the stopping layer becomes highly disordered and does not heal with annealing. Surprisingly, for higher fluence values, of about 5×10^16 ions/cm2, there is almost no residual damage. After full amorphization is reached, the layers appear to recrystallize by solid phase epitaxy (SPE), using the pristine diamond layers underneath as a template. These results prove that graphitization of diamond after annealing can be avoided in deeply buried layers, implanted at fluences much higher than expected. High fluences, in fact, can lead to high quality diamond layers. If SPE can be confirmed, it would have a great interest for diamond device applications, as it allows for higher doping levels., We thank the technical staff of CMAM for operating the tandem ion-beam accelerator. Funding: This work was supported by the Ministerio de Economía y Competitividad (MINECO), Spain [MAT2014-57547-R, MAT2014-54826-C2-1-R, FIS2014-54498-R, and CTQ-2014-53334-C2-2-R], the María de Maeztu Program for Units of Excellence in R&D [MDM-2014-0377], and the Comunidad Autónoma de Madrid [NANOFRONTMAG-CM (S2013/MIT-2850)]., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Micro-Raman spectroscopy of near-surface damage in diamond irradiated with 9-MeV boron ions

  • Agulló Rueda, F.
  • Ynsa, M. D.
  • Gordillo, N.
  • Maira-Vidal, Aránzazu
  • Moreno-Cerrada, D.
  • Ramos, M. A.
We have studied the near-surface damage in a diamond crystal caused by irradiation with swift boron ions and its healing after high-temperature annealing. A diamond crystal was irradiated with 9-MeV 11B3+ ions with fluence values between 1×10^15 and 4.42×10^16 ions/cm2 to generate various levels of lattice damage. The ions loose energy to the lattice and, according to simulations, stop at a depth of about 5 μm, where they form a thin buried implantation layer. For the near-surface layers damage is produced by the ions at high kinetic energy before they slow down. Only intrinsic defects can be produced, with no boron atoms. The lattice damage of the near-surface layers and its recovery after annealing for 1 h at 1000°C were studied by Raman and photoluminescence spectroscopies. Back-scattered light from a 514.5-nm laser beam was collected from the sample surface, probing a depth of a few micrometers. We observe some disordering of the lattice plus the formation of neutral vacancies, interstitial and other lattice defects. After annealing the Raman spectrum shows a significant recovery of the lattice order and the disappearance of isolated neutral vacancies. Residual damage is confirmed by the luminescence spectrum, that shows the appearance of new spectral features., This work was supported by the Ministerio de Economía y Competitividad (MINECO), Spain [ MAT2014-57547-R,MAT2014-54826-C2-1-R, andFIS2014-54498-R], the María de Maeztu Program for Units of Excellence in R&D [ MDM-2014-0377], and the Comunidad Autónoma de Madrid [ NANOFRONTMAG-CM (S2013/MIT-2850)]. Research by N. G. is supported by MINECO [JCI-2012-12652]., Peer-reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Tribocorrosion response in biological environments of multilayer TaN films deposited by HPPMS

  • Mendizabal, Lucia
  • Lopez, Ainara
  • Bayón, Raquel
  • Herrero, Pilar
  • Barriga, Javier
  • Gonzalez, Javier J.
Biomedical implant failure arises mainly from the degradation caused by tribological processes occurring in the corrosive environment the human body represents, known as tribocorrosion. The material loss and metal ion release resulting from tribocorrosion processes compromise the biocompatibility of metallic implants. The deposition of protective coatings on metallic substrates is a promising solution to overcome this problem. Pure titanium (Ti-cp) is widely used as an implant material due to its excellent corrosion resistance and high biocompatibility. However, its mechanical properties must be improved in order to ensure a longer durability. For this purpose, TaN monolayer and multilayer coatings were deposited on medical grade Ti-cp to enhance its tribocorrosion performance in simulated body fluids. TaN coatings were deposited by recently developed High Power Pulsed Magnetron Sputtering (HPPMS) technique. HPPMS enables the deposition of extremely dense coatings with superior properties compared to the ones grown by conventional sputtering. Columnar-free TaN monolayer and multilayer films were developed exhibiting corrosion resistances in the MΩ range, one order of magnitude higher than for Ti-cp. Friction coefficient of Ti-cp was reduced from 0.58 to 0.25 while wear rate was considerably decreased. The determined material loss after tribocorrosion tests for Ti-cp was 0.4 mm. It was reduced up to 1.55 × 10 mm by the application of best-performing TaN multilayer film., Financial support of this research program from the Basque Government (EMAITEK program) and Spanish National Department of the Education and Science in the projects: CSD2008-00323 FUNCOAT and MAT2014-57547-R is gratefully acknowledged.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Laser heating induced phase changes of VO2 crystals in air monitored by Raman spectroscopy

  • Vilanova-Martínez, Paloma
  • Hernández-Velasco, Jorge
  • Landa Cánovas, Ángel
  • Agulló Rueda, F.
We have studied the effect of intense visible light on vanadium dioxide crystals in air by measuring micro-Raman spectra for increasing laser powers. A laser wavelength of 632.8 nm was used. For power densities above 500 MW/m2 laser heating triggers the phase transition, which is known to occur at around 68° C, from the room temperature insulating VO2(M) monoclinic phase to the high temperature semiconductor VO2(R) tetragonal rutile phase. The changes are fully reversible and the crystal goes back to the monoclinic phase when the laser power is lowered to the initial value. This transition is also observed in electron diffraction experiments under vacuum, heating in this case produced by the electron beam. For laser power densities above 1300 MW/m2 the change is irreversible and laser heating provokes a reaction with the oxygen in air and an oxidation into V2O5. For comparison we have also done thermogravimetric and differential scanning calorimetry experiments from 20° C to 600° C., We thank the technical help of M. C. García-González and C. Chaparro-Ronda from the Thermal Analysis Lab (ICMM-CSIC). Funding for this work was provided under MAT2011-27192 and MAT2014-57547-R projects from the Spanish Government (Ministerio de Economía y Competitividad)., Peer reviewed
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publication Artículo científico (JournalArticle)

Characterization of the interface between highly conductive Ga:ZnO films and the silicon substrate

  • Gabàs, Mercedes
  • Ochoa-Martínez, E.
  • Navarrete-Astorga, E.
  • Landa Cánovas, Ángel
  • Herrero, Pilar
  • Agulló Rueda, F.
  • Palanco, S.
  • Martínez-Serrano, J. J.
  • Ramos-Barrado, J. R.
Gallium-doped zinc oxide films are an interesting alternative for transparent conductive materials. To improve their performance, the interface between the grown layer and the substrate must be fully understood. Accordingly, ZnO and Ga:ZnO films have been deposited onto p-type doped Si (111) substrates by magnetron sputtering for 1, 2, 3 and 20 min and their interfaces characterized by transmission electron microscopy, photoelectron spectroscopy, spectroscopic ellipsometry and impedance spectroscopy. The combination of transmission electron microscopy techniques suggested a more complex interface chemistry in the Ga:ZnO/Si case, a point confirmed by x-ray photoelectron spectroscopy measurements on very thin films. While the ZnO/Si interface consists mostly of silicon oxides, zinc silicates and some Zn0, the Ga:ZnO/Si interface, besides these constituents, has a noticeable amount of Ga:ZnO and small quantities of Ga0. The band alignment deduced from the photoelectron spectroscopy measurements, together with the layers and Si band gap values, evidences a higher work function for the doped film and a smaller conduction band barrier for the Ga:ZnO/Si interface. Concerning the optical and electrical characteristics, spectroscopic ellipsometry revealed no significant differences between the two interfaces, while impedance spectroscopy measurements demonstrated that the Ga:ZnO/Si interface is less resistive than the ZnO/Si one., Authors gratefully acknowledge financial support from the Spanish Ministerio de Economía & Competitividad (MINECO) and E.U. FEDER funds through the projects FUNCOAT-CSD2008-00023-CONSOLIDER INGENIO, TEC2014-53906-R, TEC2014-54260-C3-3-P, RYC-2010-06711 and MAT2014-57547-R, and from the Junta de Andalucía (FQM-192).
Dipòsit Digital de Documents de la UAB
Publication Artículo científico (JournalArticle)

Nanostructural changes upon substitutional Al doping in ZnO sputtered films

  • Landa Cánovas, Ángel R.
  • Santiso, José|||0000-0003-4274-2101
  • Agulló Rueda, Fernando|||0000-0001-9211-1987
  • Herrero, Pilar
  • Navarrete Astorga, Elena
  • Ochoa Martínez, E.
  • Ramos Barrado, José R.
  • Gabás, M.
Al:ZnO layers, with low and high Al content, 0.2% and 2.1% cat. respectively, have been prepared using the RF magnetron sputtering technique. Noticeable differences in the optical and electrical properties have been detected in these films. With doping, the resistivity decreases and the band-gap increases. The alterations in the films crystalline structure are explained in terms of the nanostructural changes induced by Al substitutional doping, such as a higher concentration of edge dislocation defects and a higher rotation of crystalline nanodomains in the plane of the films (normal to the preferential orientation c-axis) for the high content Al:ZnO layer. A complete description of such effects has been accomplished using several characterization techniques, such as X-ray diffraction, Raman spectroscopy and transmission electron microscopy. The combination of these techniques provides an exhaustive understanding of the films nanostructure.