Thickness and temperature dependence of the magnetodynamic damping of pulsed laser deposited La0.7Sr0.3MnO3 on (111)-oriented SrTiO3
We have investigated the magnetodynamic properties of La0.7Sr0.3MnO3 (LSMO) films of thickness 10, 15 and 30 nm grown on (111)-oriented SrTiO3 (STO) substrates by pulsed laser deposition. Ferromagnetic resonance (FMR) experiments were performed in the temperature range 100–300 K, and the magnetodynamic damping parameter α was extracted as a function of both film thickness and temperature. We found that the damping is lowest for the intermediate film thickness of 15 nm with α≈2·10−3, where α is relatively constant as a function of temperature well below the Curie temperature of the respective films., This work was supported by the Norwegian Research
Council (NFR), project number 216700. V.F acknowledge
partial funding obtained from the Norwegian PhD
Network on Nanotechnology for Microsystems, which is
sponsored by the Research Council of Norway, Division
for Science, under contract no. 221860/F40. F.M. acknowledges
financial support from RYC-2014-16515 and
from the MINECO through the Severo Ochoa Program
(SEV- 2015-0496). J.M and F.M aslo acknowledge funding
from MINECO through MAT2015-69144., Peer reviewed