Pasar al contenido principal

Resultados relacionados

Resultados totales (Incluyendo duplicados): 3
Encontrada(s) 1 página(s)

DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Effect of the heat treatment on the microstructure and hardness evolution of a AlSi10MgCu alloy designed for laser powder bed fusion

  • Martin, Arturo
  • San Sebastián, María
  • Gil, E.
  • Wang, C.Y.
  • Milenkovic, Srdjan
  • Pérez Prado, María Teresa
  • Cepeda-Jiménez, C.M.
The aim of this work is to investigate the influence of the addition of Cu on the microstructure and on the microhardness of a laser powder bed fusion (L-PBF)-fabricated AlSi10MgCu alloy. With this goal, AlSi10Mg+4 wt%Cu pre-alloyed powder was produced by gas atomization. Following a parameter optimization study, dense as-built specimens with a high relative density of 99.8% were fabricated. An outstanding microhardness value, exceeding 180 HV, was obtained after aging at 160 °C for 16 h. This value is similar to that of the high strength Al 7075 in the T6 condition. With the aid of analytical transmission electron microscopy, it was concluded that the origin of the observed excellent mechanical behavior could be attributed to the beneficial effect of Cu in reducing the Al-matrix cell size, and in increasing the density and decreasing the size of the Si-based nanoprecipitates at cell interiors. More specifically, it is proposed that the maximum hardness is associated to the development of Cu-rich GP-I zones, which act as precursors of Si nanoprecipitates. Overaging leads to a reduction in microhardness due to transformation of these GP-I zones into coarser θ’’ precipitates and thus to a smaller volume fraction of larger Si-based nanoparticles., This work was funded by the European Union's Horizon 2020 Clean Sky 2 research and innovation program under grant agreement No 755610, project AlForAMA. The authors acknowledge the support from the topic manager, Leonardo Aircraft. CYW acknowledges the financial support from the Fundamental Research Funds for the Central Universities in China (grant number 3102019QD0415). MTPP would like to acknowledge funding from the Madrid region under the program S2018/NMT-4381-MAT4.0-CM.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion

  • Pérez Prado, María Teresa
  • Martín Jiménez, Ángela
  • Shi, D.F.
  • Milenkovic, Srdjan
  • Cepeda-Jiménez, C.M.
This research aims to study the laser powder bed fusion (L-PBF) processability, the microstructure and the tensile mechanical properties of an AlFeCr alloy at a wide range of temperatures. With this goal, Al-5Fe-6Cr (wt%) pre-alloyed powder was produced by casting and gas atomization. The microstructure of the as-atomized powders and the as-built specimens was characterized via scanning electron microscopy, x-ray diffraction, and transmission electron microscopy. Following a parameter optimization study, dense as-built specimens with a high relative density of 99.8% and a Vickers hardness at room temperature of 192 HV were fabricated. In addition, the newly developed AlFeCr alloy exhibits yield strength values of 273 ± 5 MPa and 179 ± 3 MPa at 300ºC and 400ºC, respectively. The exceptional strength of this alloy at high temperature is attributed to the homogeneous precipitation during processing of large density of nanoscale icosahedral (i-phase) and intermetallic phases, which are endowed with high thermal stability. These values are significantly higher than those corresponding to the conventional wrought Al7075 aluminum alloy in the T6 condition and to all Al alloys manufactured by L-PBF to date. The current research sheds guidelines for the design of high strength aluminum alloys containing transition alloying elements that are suitable to be processed by L-PBF for high temperature structural applications in a cost effective way., The authors wish to acknowledge financial support from the European Union’s Horizon 2020 Clean Sky 2 program (contract No 755610, project AlForAMA). DFS acknowledges the financial support from the China Scholarship Council (Grant no 201706050154). Funding from projects PID2019-111285RB-I00 and PID2020-118626RB-I00 awarded by MCIN/AEI/10.13039/501100011033 is also acknowledged.
DIGITAL.CSIC. Repositorio Institucional del CSIC
Publicación Artículo científico (JournalArticle)

Influence of the Zr content on the processability of a high strength Al-Zn-Mg-Cu-Zr alloy by laser powder bed fusion

  • Martín Jiménez, Ángela
  • Vilanova, M.
  • San Sebastián, María
  • Wang, C.Y.
  • Milenkovic, Srdjan
  • Pérez Prado, María Teresa
  • Cepeda-Jiménez, C.M.
The objective of this research is to study the effect of the Zr on the L-PBF processability, microstructure, and microhardness of an AlZnMgCu-Zr alloy. Two AlZnMgCu-0.5 and 1.5 wt% Zr pre-alloyed powders were produced by casting followed by gas atomization. In addition, an excess of Mg and Zn was added to the target compositions to compensate for vaporization during L-PBF. The as-atomized powders and the as-built and heat treated specimens were characterized via scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. Crack-free samples with a relative density of 99.0 ± 0.1% were obtained in the alloy containing 1.5 wt%Zr. The as-built microstructure of this alloy consisted of small equiaxed grains without preferred grain orientation near the melt pool boundary and slightly columnar grains between adjacent melt pools. After a solution and aging heat treatment (T6), the newly developed AlZnMgCu-1.5Zr alloy has an outstanding Vickers micro-hardness of 223 ± 3 HV, which is significantly higher than that of the wrought Al7075-T6 aluminum alloy. This excellent mechanical behavior is attributed to the presence of large AlZr nucleant particles of up to 500 nm in size that inhibit grain growth during solidification and the subsequent heat treatment, and of a high density of nanoscale second phases (MgZn and AlZr) located within the aged α-Al grains., The authors wish to acknowledge financial support from the European Union's Horizon 2020 Clean Sky 2 program (contract No 755610, project AlForAMA). Leonardo Aircraft is also thanked for its support as topic manager. CYW acknowledges funding from the Fundamental Research Funds for the Central Universities in China (grant number 3102019QD0415). Funding from projects PID2019-111285RB-I00 and PID2020-118626RB-I00 awarded by MCIN/AEI/10.13039/501100011033 is also acknowledged.