Dielectric spectroscopy of novel thiol-ene/epoxy thermosets obtained from allyl-modified hyperbranched poly(ethyleneimine) and diglycidylether of bisphenol A

  • Badia, J.D.
  • Acebo, C.
  • Gil-Castell, O.
  • Serra, A.
  • Teruel-Juanes, Roberto|||0000-0002-0190-4445
  • Ribes-Greus, A.|||0000-0003-2460-8291
[EN] Dielectric Thermal Analysis (DETA) of a series of new thermoset obtained by click chemistry was performed. The new thermosets were obtained by a dual-curing process consisting in a first photochemical thiol-ene, followed by a thermal thiol-epoxy starting from an allyl-terminated hyperbranched poly(ethyleneimine) (HBPEI) and different proportions of diglycidylether of bisphenol A (DGEBA) and the corresponding stoichiometric proportions of pentaerythritol tetrakis (3-mercaptopropionate, PETMP). The dielectric behaviour was obtained experimentally supressing the conductive effects. Two sub-Tg intramolecular non-cooperative gamma and beta relaxations and an intermolecular cooperative alpha-relaxation were detected. The gamma-relaxation was ascribed to the dipole orientation of the terminal thiol groups. Two gamma relaxations gamma(epo) and gamma(ene) were observed, according to the influence of the surroundings. Only thermosets with a content of flexible HBPEI/PETMP domains higher than a 50% w/w showed the gamma(ene) relaxation at lower temperatures and higher frequencies. The beta-relaxation was a non-Johari-Goldstein relaxation, ascribed to the dipole transfer of the linear -CH2-O-(C=O)-CH2-CH2- groups of the thiol constrained in the glassy state. The alpha-relaxation was ascribed to the long-term segmental movements of the thermosets, occurring during the transition from the glassy to the rubbery stage. A synergic effect of reducing the rigidity and compactness of the thermosets by the reduction of aromatic moieties of the DGEBA/PETMP units, and the increase of the flexibility induced by the addition of HBPEI/PETMP units affected the macromolecular movement of the thermosets., European Regional Development Funds and the Spanish Ministry of Science, Innovation and Universities for ENE2017-86711-C3-1-R, MAT2017-82849-C2-1-R, ENE2014-53734-C2-1-R, UPOV13-3E-1947 and projects. Ministry of Education for the FPU13/01916) for O. Gil-Castell. Generalitat de Catalunya for the 2017-SGR-77 project. Generalitat Valenciana for the APOSTD14/041 for JD Badia and GRISOLIA/2012/003 for R. Teruel-Juanes.
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Publicación Artículo científico (JournalArticle)

Analysis of Poly(thiourethane) Covalent Adaptable Network through Broadband Dielectric Spectroscopy

  • B. Pascual-Jose|||0000-0001-7562-916X
  • Ribes-Greus, A.|||0000-0003-2460-8291
  • De la Flor, S.
  • Serra, A.
[EN] The dielectric spectra of the poly(thiourethane) network, HDI-S3, have been analyzed to know the nature and the cooperativity of each of the six dielectric processes observed. At low temperatures, ¿1, ¿2, and ß dielectric relaxations were attributed to noncooperative local motions in the glassy state, in which apparent activation energies are 30, 36, and 60 kJ·mol¿1, respectively. At higher temperatures, three dielectric relaxations are observed (¿Tg, ¿*, ¿). The ¿Tg relaxation is attributed to the glass transition, and it is overlapped with the ¿* relaxation. The molecular origin of ¿* relaxation is associated with the bond exchange reaction. Finally, the ¿ relaxation is ascribed to the heterogeneity of the sample although its origin is uncertain. The DC conductivity (¿DC) is found to be an appropriate variable to analyze the bond exchange reaction. Accordingly, the HDI-S3 has a molecular exchange mechanism of dissociative nature., The authors would like to thank the support of the European Union through the European Regional Development Funds (ERDF) and the Spanish Ministry of Science and Innovation for the research projects POLYELMETH (PID2020-116322RB-C31) and MCIN/AEI/10.13039/201100011033, which financed the PID2020/115102RB-C21 project, and the Generalitat de Catalunya for the 2017-SGR-77. This study forms part of the Advanced Materials programme and was supported by MCIN with funding from European Union NextGenerationEU (PRTR-C17.11) and by Generalitat Valenciana.