Skip to main content

Sustainable thermal tnergy storage with phase change materials for a decarbonized society

RYC2023-044207-I

•
Funding agency name Agencia Estatal de Investigación
Funding agency acronym AEI
Program Programa Estatal para Desarrollar, Atraer y Retener Talento
Subprogram Subprograma Estatal de Incorporación
Call Ramón y Cajal
Call year 2023
State Plan 2021-2023 Plan Estatal de Investigación Científica y Técnica y de Innovación
Beneficiary centre UNIVERSIDAD DE ZARAGOZA

Resultados relacionados

Resultados totales (Incluyendo duplicados): 4
Encontrada(s) 1 página(s)

Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publication Artículo científico (JournalArticle)

Rheological study on xylitol crystallization for its use as phase change material: analytical and statistical analysis

  • Navarro, Miguel
  • Gracia, Zeus
  • Asín, Jesús
  • Lázaro, Ana
  • Martí, Marta
  • Delgado, Mónica
In a global context in which decarbonization of society is wanted through the use of renewable sources, energy storage plays a fundamental role. Among the different forms of energy storage that exists, this work focuses on latent heat energy storage (LHTES) for medium-low temperatures, between 70 °C and 120 °C. Xylitol, a sugar-alcohol, is a promising phase change material (PCM) due to its low cost, low corrosivity, high latent heat (240 J/g) and a melting temperature of 92 °C. However, its use as PCM is hindered by a high degree of supercooling and a low crystallization rate. To address these challenges, this work used a seeding and shearing technique to trigger crystallization. Rheological experiments were performed to monitor viscosity changes during crystallization, in order to study the crystallization induction time. The systematic analysis included the effects of temperature (70–90 °C), shear rate(1-100s−1), and seed crystal size (300–400 μm and 600–700 μm). Key results show that temperature is the most dominant factor. The shortest induction time at 70 °C was found at 10s, increasing to 1500s at 90 °C. Increasing seed size and reducing the rheometer gap also shortened induction times, while shear rate had minimal influence, likely due to non-uniform shear during the test. For practical applications, operating at 80 °C is recommended to balance induction time and energy loss due to supercooling. Optimizing shear-triggered mechanism, such as stirred tanks designs, can improve crystallization controllability.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publication Artículo científico (JournalArticle)

Polysaccharide–protein complex-stabilized Pickering phase change material emulsions for low-temperature thermal energy storage

  • Yu, Tingting
  • Qiu, Xiaolin
  • Delgado, Mónica
  • Lázaro, Ana
  • Hu, Yang
Low-temperature phase change material emulsions (PCMEs) are excellent thermal storage media but have environmental and toxicity issues due to poorly degradable synthetic surfactants; single-component biopolymer systems lack stability, low-temperature Pickering emulsion research is scarce, protein-polysaccharide composite stabilizers in PCMEs are unreported, and Boron Nitride (BN) -biopolymer synergistic effects on supercooling remain unexplored. This study aims to develop an environmentally friendly, high-performance, low-temperature Pickering phase change material emulsion to simultaneously optimize stability, environmental compatibility, and thermal performance. This study proposes substituting traditional emulsifiers with self-assembled sodium caseinate (SC)-xanthan gum (XG) nanocomposites. Phase change emulsions were prepared by high-speed homogenization, and boron nitride was added to synergistically reduce supercooling and improve heat transfer. The SC–XG complexes adsorb at n-tetradecane/water interfaces, forming a viscoelastic interfacial network that enhances droplet stability and restricts coalescence. Thermal analysis revealed that, at 0.5% (w/v) XG, the 50 vol% n-tetradecane PCME droplets are uniform and kinetically stable, delivering a latent heat of 89.5 J g− 1. Adding only 0.75 wt% BN induces heterogeneous nucleation, cuts supercooling from 7.8 ◦C to 0.24 ◦C, and boosts thermal conductivity. This study proposes a novel protein-polysaccharide-based technical pathway for constructing green and sustainable low-temperature thermal storage materials, while also synergistically regulating the crystallization behavior and heat transfer performance of the emulsion through BN. This study provides both a theoretical foundation and a green technical solution for designing stable and efficient phase change material emulsions for thermal energy storage.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publication Artículo científico (JournalArticle)

Evaluation of thermal energy storage for medium-low temperature applications: Comparison of commercial solutions with a xylitol-based prototype

  • Navarro, Miguel
  • Lázaro, Ana
  • Delgado, Mónica
In recent years, thermal energy storage (TES) has become a promising and popular technology for energy storage. Among the different technologies, this work focuses on latent heat thermal energy storage (LHTES) system, specifically it assesses the potential of xylitol as phase change material (PCM) in TES systems for low-medium temperature applications. Xylitol, a sugar alcohol with stable supercooling, has a high latent heat (240 J/g), high energy storage density (1.45 kg/l), and a melting temperature of 92 °C. However, stable supercooling and low crystallization rate limits its practical application. Therefore, a laboratory-scale prototype working in the 70-100 °C range has been proposed and experimentally characterised that uses a seeding and shearing technique to mitigate this supercooling and accelerate crystallization, thereby increasing the thermal energy discharge power. The study compares this lab-scale prototype with four leading commercial solutions in terms of both materials and systems. Moreover, the methodology developed in the framework of IEA SHC Task 58 for TES system comparison in terms of energy density and power is applied. The results show the xylitol prototype has higher normalized power values than other experimental systems analysed in the framework of IEA SHC Task 58, reaching energy densities of up to 40.8 kWh/m3 system-wise in an optimized configuration. The study concludes that stirred TES prototype with xylitol is a competitive alternative to current commercial solutions.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publication Artículo científico (JournalArticle)

Sustainable Peg‐Based Shape‐Stabilized Phase Change Materials Using Raw Pine Cone as a Low‐Cost Filler and Graphite for Enhanced Thermal Conductivity

  • Akrouti, Amira
  • Trigui, Abdelwaheb
  • Delgado, Mónica
  • Navarro, Miguel
  • Lazaro, Ana
  • Hassani, Rym
This study investigates the development of a novel shape‐stabilized phase change material (ssPCM). Pinecone (PC) powder, a low‐cost and sustainable lignocellulosic support, was combined with polyethylene glycol (PEG 6000) as the phase change material (PCM). Graphite was incorporated to enhance thermal conductivity, minimize leakage, and improve shape stability. Thermophysical properties were evaluated to assess the potential of these ssPCM as thermal energy storage (TES) materials. The Fourier transform infrared spectroscopy (FTIR) was used to verify the chemical compatibility among components, and thermogravimetric analysis (TGA/DTG) to evaluate thermal stability and decomposition behavior. Brunauer–Emmett–Teller (BET) surface area, mercury intrusion porosimetry (MIP), and field emission scanning electron microscopy (FESEM) were conducted to investigate the structure of the PC support and its influence on ssPCMs. Density was measured using a thermomechanical analyzer (TMA), while thermal diffusivity was determined with a laser flash apparatus (LFA). Among the prepared composites, 80% PEG, 10% G, 10% PC showed the most promising thermal storage performance, with a latent heat of 153.7 kJ/kg by differential scanning calorimetry (DSC) and 207.3 kJ/kg by the T‐history method. Preliminary results suggest that these ssPCM offer a cost‐effective and reliable solution for TES applications, combining eco‐friendly materials with enhanced thermal, structural, and thermophysical performance.