Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

Chemical solution synthesis and ferromagnetic resonance of epitaxial thin films of yttrium iron garnet

  • Lucas, I.
  • Jimenez-Cavero, P.
  • Vila-Fungueirino, J.M.
  • Magen, C.
  • Sangiao, S.
  • de Teresa, J.M.
  • Morellon, L.
  • Rivadulla, F.
We report the fabrication of epitaxial Y3Fe5O12 (YIG) thin films on Gd3Ga5O12 (111) using a chemical solution method. Cubic YIG is a ferrimagnetic material at room temperature, with excellent magneto-optical properties, high electrical resistivity, and a very narrow ferromagnetic resonance, which makes it particularly suitable for applications in filters and resonators at microwave frequencies. But these properties depend on the precise stoichiometry and distribution of Fe3+ ions among the octahedral/tetrahedral sites of a complex structure, which hampered the production of high-quality YIG thin films by affordable chemical methods. Here we report the chemical solution synthesis of YIG thin films, with excellent chemical, crystalline, and magnetic homogeneity. The films show a very narrow ferromagnetic resonance (long spin relaxation time), comparable to that obtained from high-vacuum physical deposition methods. These results demonstrate that chemical methods can compete to develop nanometer-thick YIG films with the quality required for spintronic devices and other high-frequency applications.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

Quantification of the interfacial and bulk contributions to the longitudinal spin Seebeck effect

  • Jiménez-Cavero, P.
  • Lucas, I.
  • Bugallo, D.
  • López-Bueno, C.
  • Ramos, R.
  • Algarabel, P.A.
  • Ibarra, M.R.
  • Rivadulla, F.
  • Morellón, L.
We report the disentanglement of bulk and interfacial contributions to the thermally excited magnon spin current in the spin Seebeck effect under static heating. For this purpose, we have studied the dependence of the inverse spin Hall voltage and the thermal conductivity on the magnetic layer thickness. Knowledge of these quantities allows us to take into account the influence of both sources of thermal spin current in the analysis of the voltage dependence. The magnetic layer thickness modulates the relative magnitude of the involved thermal drops for a fixed total thermal difference throughout the sample. In the end, we attain the separate contributions of both sources of thermal spin current - bulk and interfacial - and obtain the value of the thermal magnon accumulation length scale in maghemite, which we find to be 29(1) nm. According to our results, bulk magnon accumulation dominates the spin Seebeck effect in our studied range of thicknesses, but the interfacial component is by no means negligible.
Zaguán. Repositorio Digital de la Universidad de Zaragoza
Publicación Artículo científico (JournalArticle)

Optimization of YIG/Bi stacks for spin-to-charge conversion and influence of aging

  • Sangiao Barral, Soraya
  • Morales Aragonés, José Ignacio
  • Lucas del Pozo, Irene
  • Jiménez Cavero, Pilar
  • Morellón Alquézar, Luis
  • Sánchez Azqueta, Carlos
  • De Teresa Nogueras, José María
We show that an optimized growth of magnetic layer/non-magnetic layer stacks allows for the improvement of the spin-to-charge conversion efficiency. From the analysis of the voltage signal generated in spin pumping experiments due to the inverse spin Hall effect (ISHE) on Y3Fe5O12 (YIG)/Bi stacks, we have determined values for the spin Hall angle and the spin-diffusion length in Bi of 0.0068(8) and 17.8(9) nm, respectively. Based on these results, we have also studied the influence of aging on the spin-to-charge conversion efficiency by performing spin pumping experiments on YIG/Bi stacks after exposing the samples to ambient conditions for several days and up to 150 days. We have found that in YIG/Bi samples with Bi thicknesses around or below the spin-diffusion length, the ISHE voltage signal is still above 80% of its initial value after 100 days.